Effect of microstructure and printed pores on the adiabatic shearing behavior of Ti6Al4V titanium alloy manufactured by selective electron beam melting
Source abstract
Abstract
Ti6Al4V alloy sample manufactured by selective electron beam melting technology as well as its heat-treated sample, and hot-rolled Ti6Al4V alloy sample were the research objects in the present work. The effects of microstructure and printed pores on the localized adiabatic shearing behavior of the printed, heat-treated and hot-rolled Ti6Al4V alloy were firstly investigated with the split Hopkinson compression bar, metallurgical microscopy and X-ray computed tomography technology. The hot-rolled sample had fine equiaxed grains, no printed pores and the highest density, so its adiabatic shearing susceptibility was the lowest. The printed sample had the highest porosity, the lowest density, and the orientation of the c-axis of hcp-α phase parallel to the loading direction led to the higher critical resolved shear stress and flow stress during compression deformation, thus the corresponding thermal softening effect was stronger, and its adiabatic shearing susceptibility was the highest. While the porosity of the heat-treated sample was smaller and the density was larger, the columnar grains were transformed into equiaxed grains after heat treatment, so the adiabatic shearing susceptibility of the heat-treated sample was lower than that of the printed sample. The existence of printed pores was equivalent to omitting the void nucleation stage of microcrack formation during dynamic deformation, and the printed pores located in the 45 o shearing direction would grow and converge directly along the shearing direction to form microcracks, and also accelerate the propagation of microcracks and more easily cause adiabatic shearing fracture. The porosity of the sample decreased after heat treatment, but the average volume and average equivalent diameter of the pores decreased, and the number of pores increased instead. The greater the number of pores inside the material, the greater the chance of pores in the shearing direction, so the heat-treated sample was more likely to initiate microcracks in the adiabatic shearing band, and the crack propagation rate would be faster and more likely to cause adiabatic shearing fracture than the printed sample.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High-Velocity Impact and Material Behavior · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Energy and emissions saving potential of additive manufacturing: the case of lightweight aircraft components10.1016/j.jclepro.2015.04.109 ↗
2. Machinability of steels and titanium alloys under lubrication10.1016/0043-1648(93)90481-Z ↗
3. Additive manufacturing technologies: 3D printing, rapid prototyping, and direct digital manufacturing
4. Additive manufacturing of Ti6Al4V alloy: a review10.1016/j.matdes.2018.107552 ↗
5. Dodd · 2012
6. Impact of the initial microstructure and the loading conditions on the deformation behavior of the Ti17 titanium alloy10.1007/s10853-019-04014-5 ↗
7. Effects of microstructure on the adiabatic shearing behaviors of titanium alloy10.1016/j.msea.2010.12.068 ↗
8. Effect of phase composition on self-organization of shearing bands in Ti-1300 titanium alloy10.1016/j.msea.2011.06.068 ↗
9. Effect of high strain rate on adiabatic shearing of α+β dual-phase Ti alloy
10. Influence of shock pre-strain on the dynamic mechanical behavior and adiabatic shearing failure of the Ti-6Al-4V alloy with lamellar microstructure10.1016/j.engfailanal.2020.104500 ↗
11. Microstructural characterization and evolution mechanism of adiabatic shearing band in a near beta-Ti alloy10.1016/j.msea.2010.12.053 ↗
12. Micro-mechanisms of shearing deformation localization of Ti6Al4V alloy under shearing-compressive loading conditions10.3390/ma13245646 ↗
13. Formation of adiabatic shearing band within Ti-6Al-4V: an in-situ study with high-speed photography and temperature measurement
14. Adiabatic shearing bands on the titanium side in the titanium/mild steel explosive cladding interface: experiments, numerical simulation, and microstructure evolution10.1007/s11661-006-0193-9 ↗
15. Adiabatic shearing band on the titanium side in the Ti/mild steel explosive cladding interface10.1016/1359-6454(95)00200-6 ↗
16. Microstructure evolution in adiabatic shearing band in α-titanium10.1007/s10853-006-0811-3 ↗
17. Dynamic recrystallization in adiabatic shearing band in α-titanium10.1016/j.matlet.2005.12.097 ↗
18. Compression testing of a sintered Ti6Al4V powder compact for biomedical applications10.1016/j.matchar.2005.01.006 ↗
19. Deformation and fracture behavior of laser processed dense and porous Ti6Al4V alloy under static and dynamic loading10.1016/j.msea.2012.04.036 ↗
20. Moskowitz · 1977
21. Porous and foamed amorphous metals10.1557/mrs2007.126 ↗
22. The rate-dependent deformation and localization of fully dense and porous Ti-6Al-4V10.1016/S0921-5093(97)00076-2 ↗
23. Numerical study of the deformation and fracture behavior of porous Ti6Al4V alloy under static and dynamic loading10.1016/j.ijimpeng.2014.08.011 ↗
24. Void coalescence in a porous solid under dynamic loading conditions10.1007/s10704-012-9683-5 ↗
25. Ramesh · 2008
26. In situ observation of ductile fracture using X-ray tomography technique10.1016/j.actamat.2010.11.065 ↗
27. Porosity measurements and analysis for metal additive manufacturing process control10.6028/jres.119.019 ↗
28. Comparison of density measurement techniques for additive manufactured metallic parts10.1108/13552541111156504 ↗
29. Hall-Petch relationship and deformation mechanism of pure Mg at room temperature10.1016/j.jallcom.2022.165924 ↗
30. The electrical resistivity log as an aid in determining some reservoir characteristics10.2118/942054-G ↗
31. Extended mean-field method for predicting yield behaviors of porous materials10.1016/j.mechmat.2006.02.008 ↗
32. Anisotropic yield behavior of Lotus-type porous Iron: measurements and micromechanical mean-Field analysis10.1557/JMR.2005.0009 ↗
33. Microstructure, anisotropic mechanical properties and very high cycle fatigue behavior of Ti6Al4V produced by selective Electron beam melting10.1007/s12540-020-00664-2 ↗
34. On the process of transition of the cubic-body-centered modification into the hexagonal-close-packed modification of zirconium10.1016/S0031-8914(34)80244-3 ↗
35. Post-processing to modify the α phase Micro-texture and β phase grain morphology in Ti-6Al-4V fabricated by powder bed Electron beam melting10.1007/s11661-019-05247-4 ↗
36. Deformation mechanisms of a commercial titanium alloy Ti6Al4V as a function of strain rate and initial texture
37. Mechanical properties and adiabatic shearing sensitivity of Ti-6Al-4V alloy with different microstructures
38. Microstructural evolution associated with shearing location of AISI 52100 under high strain rate loading10.1016/j.msea.2016.03.050 ↗
39. Gerhard · 1994
40. Wang · 1992
41. Effects of pre-notches on the self-organization behaviors of shearing bands in aluminum alloy10.1016/j.msea.2010.04.079 ↗