Abstract
This paper aims to investigate the effects of In and aging treatment on the microstructure, mechanical properties and electrochemical corrosion behavior of Sn 2Cu solder alloy. It is found that In could refine the β-Sn grains, resulting in an improved microstructure and enhanced microhardness and tensile properties. Moreover, adding In lowered the undercooling of the Sn 2Cu solder alloy, with a maximum reduction of 5.97 °C. The corrosion resistance of the alloy was also dramatically improved by In addition, as evidenced by: (1) a lower corrosion current density compared to the matrix alloy; (2) a smaller surface roughness and pit depth after corrosion; (3) an increased ratio of SnO 2 in the corrosion product layer. On the other hand, aging treatment had an adverse impact on the mechanical properties, but a beneficial influence on corrosion resistance of solder alloy.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Advanced Welding Techniques Analysis · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (51)
Show source-provided references
1. Quasi-in-situ observation on diffusion anisotropy dominated asymmetrical growth of Cu-Sn IMCs under temperature gradient[J]
2. Effect of small additions of alloying elements on the properties of Sn-Zn eutectic alloy[J]10.1007/s11664-006-0227-5 ↗
3. Microstructural and mechanical characterization of melt spun process Sn-3.5Ag and Sn-3.5Ag-xCu lead-free solders for low cost electronic assembly[J]10.1016/j.msea.2017.03.022 ↗
4. Effects of Ni modified MWCNTs on the microstructural evolution and shear strength of Sn-3.0Ag-0.5Cu composite solder joints[J]10.1016/j.matchar.2020.110287 ↗
5. Interfacial embrittlement by bismuth segregation in copper/tin-bismuth Pb-free solder interconnect[J]10.1557/JMR.2001.0229 ↗
6. High temperature lead-free solder for microelectronics[J]10.1007/s11837-001-0097-5 ↗
7. C3F8 plasma fluorination of lead free solders for fluxless soldering[J]10.1016/j.apsusc.2003.11.061 ↗
8. Interfacial reaction between Sn-0.7 Cu (-Ni) solder and Cu substrate[J]10.1007/BF02692576 ↗
9. Effect of co addition into Ni film on shear strength of solder/Ni/cu system: experimental and theoretical investigations[J]10.1016/j.msea.2020.139589 ↗
10. Effect of ag addition on the microstructural and mechanical properties of Sn-cu eutectic solder[J]10.2320/matertrans.42.739 ↗
11. Influence of indium addition on characteristics of Sn–0.3Ag–0.7Cu solder alloy[J]10.1016/j.jallcom.2009.06.020 ↗
12. Structural and elastic properties of eutectic Sn–cu lead-free solder alloy containing small amount of ag and in[J]10.1016/j.jallcom.2011.01.062 ↗
13. Effect of indium on microstructure, mechanical properties, phase stability and atomic diffusion of Sn-0.7 Cu solder: experiments and first-principles calculations[J]10.1016/j.msea.2022.143938 ↗
14. Influence of CrFeCoNiCu high-entropy alloy and ultrasonic stirring on the thermal, electrochemical and mechanical properties of Zn-30Sn high-temperature solder alloy[J]10.1016/j.matchar.2023.112977 ↗
15. Influence of Fe and ho additions on Sn-3.0 Ag-0.5 Cu solder alloy: microstructure, electrochemical and mechanical properties[J]10.1016/j.matchar.2023.113307 ↗
16. Research on Bi contents addition into Sn–Cu-based lead-free solder alloy[J]10.1007/s10854-022-08464-7 ↗
17. Effect of Nd addition on the corrosion behavior of SAC305 solder alloy[J]10.1016/j.corsci.2023.111264 ↗
18. Corrosion resistance of ternary Sn-9Zn-xIn solder joint in alkaline solution[J]10.1016/j.jallcom.2015.11.184 ↗
19. Electrochemical migration and electrochemical corrosion behaviors in 3wt.% NaCl solution of 64Sn-35Bi-1Ag solder with in do** for micro-nanoelectronic packagings[C]//2012
20. Aging induced structural and electrochemical corrosion behaviour of Sn-1.0 Ag-0.5 Cu and Sn-3.8 Ag-0.7 Cu solder alloys[J]10.1016/j.jallcom.2018.01.292 ↗
21. Corrosion characteristics of Sn-20Bi-xCu-yIn solder in 3.5% NaCl solution[J]10.1016/S1003-6326(23)66225-9 ↗
22. Microstructure evolution and shear fracture behavior of aged Sn3Ag0. 5Cu/Cu solder joints[J]10.1016/j.msea.2016.07.071 ↗
23. Effect of Zn and in to microstructure of aged SAC305/Cu joint[J]
24. Controlling Ag3Sn plate formation and its effect on the creep resistance of Sn–3.0 Ag–0.7 Cu lead-free solder by adding minor alloying elements Fe, Co, Te and Bi[J]10.1007/s12540-020-00856-w ↗
25. Effect of Sb and in additives on thermal and electrical properties of Sn–9Zn–4Bi alternative lead-free solder alloy[J]
26. Effects of indium addition on properties and wettability of Sn-0.7Cu-0.2Ni lead-free solders[J]10.1016/j.matdes.2014.07.035 ↗
27. Thermodynamic characteristics, microstructure and mechanical properties of Sn-0.7Cu-xIn lead-free solder alloy[J]10.1016/j.jallcom.2018.01.386 ↗
28. Effects of indium on the intermetallic layer between low-Ag SAC0307-xIn lead-free solders and Cu substrate[J]10.1016/j.jallcom.2016.01.231 ↗
29. Atomic radii in crystals[J]10.1063/1.1725697 ↗
30. Comparison of corrosion behaviour of zinc in NaCl and in NaOH solutions; Part II: Electrochemical analyses[J]10.1016/j.corsci.2010.08.018 ↗
31. Corrosion behavior assessment of tin-lead and lead free solders exposed to fire smoke generated by burning polyvinyl chloride[J]10.1016/j.matchemphys.2018.03.057 ↗
32. Corrosion resistance of Pb-free and novel nano-composite solders in electronic packaging[M]
33. Corrosion characterization of tin–lead and lead free solders in 3.5wt.% NaCl solution[J]10.1016/j.corsci.2007.11.025 ↗
34. Electrochemical behavior of Sn-xZn lead-free solders in aerated NaCl solution
35. Electrochemical behaviour of lead-free Sn–0.7 Cu–xIn solders alloys in 3.5 wt% NaCl solution[J]10.1007/s10854-021-06824-3 ↗
36. Electrochemical migration and electrochemical corrosion behaviors in 3wt.% NaCl solution of 64Sn-35Bi-1Ag solder with In doping for micro-nanoelectronic packagings[C]
37. Interfacial reactions and growth kinetics for intermetallic compound layer between in–48Sn solder and bare Cu substrate[J]10.1016/j.jallcom.2004.05.055 ↗
38. Reliability of in-48Sn solder/Au/Ni/Cu BGA packages during reflow process[J]10.1007/s11664-005-0166-6 ↗
39. Solderability of Sn–9Zn–0.5Ag–1In lead-free solder on cu substrate: part 1. Thermal properties, microstructure, corrosion and oxidation resistance - ScienceDirect[J]10.1016/j.jallcom.2005.09.094 ↗
40. Corrosion characterization of tin–lead and lead free solders in 3.5 wt.% NaCl solution[J]10.1016/j.corsci.2007.11.025 ↗
41. Electrochemical corrosion behaviour of Pb-free SAC 105 and SAC 305 solder alloys: a comparative study[J]10.17576/jsm-2017-4602-14 ↗
42. Electrochemical corrosion behaviour of Sn-Zn-xBi alloys used for miniature detonating cords[J]10.1016/j.jmst.2019.03.026 ↗
43. Localized corrosion (pitting): a model of passivity breakdown including the role of the oxide layer nanostructure[J]10.1016/j.corsci.2008.06.047 ↗
44. In-situ EIS study on the initial corrosion evolution behavior of SAC305 solder alloy covered with NaCl solution[J]10.1016/j.jallcom.2020.156953 ↗
45. Effect of Ag3Sn intermetallic compounds on corrosion of Sn-3.0 ag-0.5 cu solder under high-temperature and high-humidity condition[J]10.1016/j.corsci.2012.05.006 ↗
46. XPS study on the surface films of a newly designed Ni-free Ti-based bulk metallic glass[J]10.1016/j.actamat.2006.10.054 ↗
47. Effects of microstructure and temperature on corrosion behavior of Sn–3.0 Ag–0.5 Cu lead-free solder[J]10.1007/s10854-011-0552-1 ↗
48. Electrochemical corrosion behaviour of Pb-free Sn–8.5 Zn–0.05 Al–XGa and Sn–3Ag–0.5 Cu alloys in chloride containing aqueous solution[J]10.1016/j.corsci.2008.06.042 ↗
49. Electrochemical behaviour of lead-free Sn–0.7Cu–xIn solders alloys in 3.5 wt% NaCl solution[J]10.1007/s10854-021-06824-3 ↗
50. Study of the effect of heat treatment on corrosion property of the AlxCoCrFeNi high-entropy alloys (x= 0.3, 0.7, and 1) prepared by spark plasma sintering[J]10.1016/j.jallcom.2023.172194 ↗
51. Electrochemical corrosion behavior of Sn-0.7 Cu solder alloy with the addition of bismuth and iron[J]10.1016/j.jallcom.2019.151925 ↗