The effect of normal force on fretting corrosion behavior of Inconel 690 in 3.5% sodium chloride
Source abstract
Abstract
Abstract The effect of normal force on fretting corrosion behaviors of Inconel 690 in 3.5% sodium chloride was investigated. The results indicated that fretting corrosion behaviors strongly depended on fretting regime and normal force. In gross slip regime, the wear volume increased but coefficient of friction (COF) decreased with increasing normal force. The damage mechanism was nanostructures and delamination cracks, and the tribologically transformed structure was separated into Ni-rich/Cr-rich oxide zones. The wear mechanism was delamination/oxidation wear. In partial slip regime, wear volume and COF decreased with increasing normal force. The main damage mechanism was fatigue cracks and asperity corrosion. The fatigue cracks propagated along the direction of 40–50° to the surface. The wear mechanism was oxidation/abrasive wear.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Mechanical stress and fatigue analysis · Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Materials challenges in nuclear energy10.1016/j.actamat.2012.11.004 ↗
2. Tribological behavior and tool wear analyses in rough turning of large-scale parts of nuclear power plants using grooved coated insert10.1016/j.triboint.2014.06.017 ↗
3. Flow-induced vibration and fretting-wear predictions of steam generator helical tubes10.1016/j.nucengdes.2006.12.001 ↗
4. On fretting maps10.1016/0043-1648(88)90134-2 ↗
5. A study on the interaction between fretting wear and cyclic plasticity for Ti–6Al–4V10.1016/j.wear.2008.12.039 ↗
6. Effect of grain size and hardness on fretting wear behavior of Inconel 600 alloys10.1016/j.triboint.2014.08.005 ↗
7. Effect of precipitated carbides on the fretting wear behavior of Inconel 600 alloy10.1016/j.wear.2014.03.012 ↗
8. Effects of displacement amplitude on fretting wear behaviors and mechanism of Inconel 600 alloy10.1016/j.wear.2013.04.027 ↗
9. Effect of pH value on the fretting wear behavior of Inconel 690 alloy10.1016/j.triboint.2015.10.025 ↗
10. Evolution of wear damage in Inconel 600 alloy due to fretting against Type 304 stainless steel
11. Microstructural characterization of subsurface caused by fretting wear of Inconel 690TT alloy10.1016/j.matchar.2016.03.010 ↗
12. The effect of subsurface deformation on the wear behavior of steam generator tube materials10.1016/S0043-1648(02)00157-6 ↗
13. A comparative study on the fretting wear of steam generator tubes in Korean power plants10.1016/S0043-1648(03)00147-9 ↗
14. Third body effects on friction and wear during fretting of steel contacts10.1016/j.triboint.2011.02.013 ↗
15. Tribocorrosion behaviours of AISI 310 and AISI 316 austenitic stainless steels in 3.5% NaCl solution10.1016/j.matchemphys.2016.01.013 ↗
16. Electrochemical investigation of corrosion and wear interactions under fretting conditions10.1016/j.wear.2012.02.001 ↗
17. Synergistic effect of cavitation erosion and corrosion of various engineering alloys in 3.5% NaCl solution10.1016/S0921-5093(00)00899-6 ↗
18. An experimental study on fretting wear behavior of cross-contacting Inconel 690 tubes10.1016/j.nucengdes.2011.08.024 ↗
19. Experimental investigation on sliding and fretting wear of steam generator tube materials10.1016/S0043-1648(01)00676-7 ↗
20. Introduction of a new sliding regime criterion to quantify partial, mixed and gross slip fretting regimes: correlation with wear and cracking processes10.1016/j.wear.2010.05.002 ↗
21. Study of the tribologically transformed structure created during fretting tests10.1016/S0301-679X(00)00088-8 ↗
22. Microstructural evolution of subsurface on Inconel 690TT alloy subjected to fretting wear at elevated temperature10.1016/j.matdes.2016.05.030 ↗
23. Electrochemical properties and growth mechanism of passive films on Alloy 690 in high-temperature alkaline environments10.1016/j.corsci.2010.06.016 ↗
24. The mechanism of oxide film formation on Alloy 690 in oxygenated high temperature water10.1016/j.corsci.2011.07.038 ↗
25. The effects of electrochemical polarization condition and applied potential on tribocorrosion behaviors of Inconel 690 alloys in water environment10.1016/j.matdes.2017.01.032 ↗
26. Pitting corrosion of Alloy 690 in thiosulfate-containing chloride solutions10.1016/S0022-3115(99)00209-3 ↗
27. A mechanistic study on thiosulfate-enhanced passivity degradation of Alloy 800 in chloride solutions10.1016/j.electacta.2013.08.030 ↗
28. The effect of rapidly varying contact stress fields on fretting fatigue10.1016/S0142-1123(01)00191-8 ↗
29. Nucleation and early growth of tribologically transformed structure (TTS) induced by fretting10.1016/S0043-1648(97)00141-5 ↗
30. In situ investigation of crevice corrosion on UNS S32101 duplex stainless steel in sodium chloride solution10.1016/j.corsci.2013.06.039 ↗
31. The crevice corrosion behaviour of stainless steel in sodium chloride solution10.1016/j.corsci.2011.08.012 ↗