Ultrafine grained structure and improved mechanical properties of low temperature friction stir spot welded 6061-T6 Al alloys
Source abstract
Abstract
Abstract In this study, 1 mm thick 6061-T6 aluminum alloy plates were subjected to friction stir spot welding (FSSW) at a very low rotation speed of 30, 40 and 50 rpm, aiming to prevent the hardness reduction in the heat affected zone (HAZ) of this precipitate hardening Al joints. Two kinds of rotating tools, namely, one with a 1 mm long probe and the other one with a flat shoulder without a probe, were used and the corresponding force applied to the rotating tools was ranged from 4 to 8 tons. Under this special welding condition, the highest welding temperature was measured lower than 200 °C. As a result, no hardness reduction of the HAZ region could be detected and an ultrafine grain structure with a high density of dislocations was formed in the stir zone. The average grain size obtained in the stir zone was less than 500 nm for all the welds, which was much smaller than that in conventional FSSW processed 6061-T6 Al joints. In addition, no hook-like bonding ligaments were formed in the joints due to the very different material flows and the shear tensile tests showed that the spot welds prepared by the low speed FSSW can reach a maximum shear load of about 5400 N, much higher than those prepared by the conventional FSSW technique.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Welding Techniques Analysis · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. T. Iwashita, Mazda Motor Corporation. Method and apparatus for joining. Patent publication number: US6601751 B2, 2003.
2. Y. Kano, M. Inuzuka, S. Yamashita, Y. Nakashima, Y. Nagao, T. Iwashita. Japanese patents application no. P2000-355770; 2000.
3. Stir zone microstructure and strain rate during Al 7075-T6 friction stir spot welding10.1007/BF02586110 ↗
4. Effect of welding parameters on microstructure and mechanical properties of friction stir spot welded 5052 aluminum alloy10.1016/j.matdes.2011.03.058 ↗
5. Effects of heating process on the microstructures and tensile properties of friction stir spot welded AZ31 magnesium alloy plates10.1016/j.matdes.2011.05.046 ↗
6. Effect of tool design and process parameters on properties of Al alloy 6016 friction stir spot welds10.1016/j.jmatprotec.2010.12.014 ↗
7. Effects of process parameters on strength of Mg alloy AZ61 friction stir spot welds10.1016/j.matdes.2011.08.050 ↗
8. Microstructure and mechanical properties of mild steel joints prepared by a flat friction stir spot welding technique10.1016/j.matdes.2012.01.027 ↗
9. Effect of friction stir spot weld parameters on Cu/CuZn30 bimetal joints10.1007/s00170-015-6998-1 ↗
10. Friction stir spot welding of hot-stamped boron steel10.1016/j.scriptamat.2007.06.060 ↗
11. Resistance and friction stir spot welding of DP600: a comparative study10.1179/174329307X159801 ↗
12. Friction stir welding of aluminum cuts energy costs by 99
13. Badarinarayan · 2007 · 235
14. Stir zone microstructure and strain rate during al 7075-T6 friction stir spot welding10.1007/BF02586110 ↗
15. Effect of welding parameters on the strain rate and microstructure of friction stir spot welded 2024 aluminum alloy10.1007/s10853-006-1103-7 ↗
16. Microstructure and mechanical properties of friction stir spot welds of AA6061-T4 sheets10.1016/j.matdes.2013.08.021 ↗
17. J.F. Dos Santos, et al. mechanical and microstructural investigation of friction stir welded AA6181-T4 aluminum alloy10.1016/j.matdes.2010.11.017 ↗
18. Hook formation and mechanical properties of friction spot welding in alloy 6061-T610.1016/j.jmatprotec.2015.11.026 ↗
19. The influence of refill FSSW parameters on the microstructure and shear strength of 5042 aluminum welds10.1016/j.jmatprotec.2012.12.009 ↗
20. Sato · 2015
21. Energy utilization and generation during friction stir spot welding10.1179/174329306X84373 ↗
22. Strain rates and grain growth in Al 5754 and Al 6061 friction stir spot welds10.1007/s11661-007-9155-0 ↗
23. The new grain formation during warm and hot deformation of copper10.1115/1.1925284 ↗
24. Grain structure formation during friction stir welding observed by the ‘stop action technique10.1016/j.actamat.2005.03.044 ↗
25. Effect of welding temperature on microstructure of friction stir welded Al alloy 105010.1007/s11661-014-2651-0 ↗
26. Strength, grain refinement and solute nanostructures of an Al–Mg–Si alloy (AA6060) processed by high-pressure torsion10.1016/j.actamat.2013.10.022 ↗
27. Dynamic and post-dynamic recrystallization under hot, cold and severe plastic deformation conditions10.1016/j.pmatsci.2013.09.002 ↗
28. Atom probe studies on the early stages of precipitation in Al-Mg-Si alloys10.1016/S0921-5093(98)00548-6 ↗
29. The precipitation sequence in Al-Mg-Si alloy10.1016/S1359-6454(98)00059-7 ↗
30. Parameters controlling microstructure and hardness during friction-stir welding of precipitation-hardenable aluminum alloy 606310.1007/s11661-002-0124-3 ↗
31. Precipitation phenomena in ultrafine grained Al-Mg-Si alloy with heterogeneous microstructure10.1016/j.actamat.2015.10.030 ↗
32. Material interactions in a novel pinless tool approach to friction stir spot welding thin aluminum sheet10.1007/s11661-010-0514-x ↗
33. Comparison of microstructure and mechanical properties of conventional and refilled friction stir spot welds in AA6061-T6 using filler plate10.1016/S1003-6326(13)62804-6 ↗
34. Mechanical properties and failure mechanisms of friction stir spot welds of AA 6061-T4 sheets10.1016/j.matdes.2013.01.066 ↗
35. Novel spot friction stir welding of 6061 and 5052 Al alloys10.1179/1362171811Y.0000000043 ↗
36. Microstructural analysis of stir zone of Al alloy produced by friction stir spot welding10.1179/136217108X347601 ↗