Intergranular corrosion resistance of Zn modified 5××× series Al alloy during retrogression and re-aging treatment
Source abstract
Abstract
Abstract The effects of retrogression and re-aging treatment on the intergranular corrosion behavior of Al-5.0Mg-3.0Zn alloys are systematically studied. The alloy's strength increases when retrogression temperature increases from 390 °C to 420 °C. Samples retrogressed at 390 °C then re-aged are very susceptible to intergranular corrosion and those retrogressed at 405 °C and 420 °C express good corrosion resistance. Then the alloy's corrosion susceptibility rises with increasing retrogression temperature. Grain boundary precipitates are coarsened and distributed discontinuously with decreasing retrogression temperature. Higher retrogression temperature results in higher Mg and Zn content difference and intergranular corrosion susceptibility.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Corrosion Behavior and Inhibition · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Jones · Metall. Mater. Trans. A · 2001 · 32 · 169910.1007/s11661-001-0148-0 ↗
2. Kramer · J. Mater. Eng. Perform. · 2012 · 21 · 102510.1007/s11665-011-9998-9 ↗
3. Gupta · Corrosion · 2013 · 69 · 108110.5006/0948 ↗
4. Searles · Metall. Mater. Trans. A · 2001 · 32 · 285910.1007/s11661-001-1036-3 ↗
5. Searles · Mater. Sci. Forum · 2002 · 396–402 · 143710.4028/www.scientific.net/MSF.396-402.1437 ↗
6. Halap · Metall. Mater. Trans. A · 2014 · 45A · 457210.1007/s11661-014-2386-y ↗
7. Carroll · Scr. Mater. · 2000 · 42 · 33510.1016/S1359-6462(99)00349-8 ↗
8. Meng · J. Alloys Compd. · 2014 · 617 · 92510.1016/j.jallcom.2014.08.099 ↗
9. Meng · J. Alloys Compd. · 2016 · 655 · 17810.1016/j.jallcom.2015.09.159 ↗
10. Hou · J. Mater. Sci. · 2018 · 53 · 384610.1007/s10853-017-1811-1 ↗
11. Barbucci · J. Alloys Compd. · 1998 · 268 · 29510.1016/S0925-8388(97)00605-1 ↗
12. C. Wu10.1016/j.jallcom.2014.04.185 ↗
13. Afify · Mater. Sci. Appl. · 2011 · 2 · 427
14. Bigot · Microsc. Microanal. Microstruct. · 1997 · 8 · 10310.1051/mmm:1997109 ↗
15. Bergquist · Mater. Sci. Eng. A · 2011 · 528 · 873310.1016/j.msea.2011.08.046 ↗
16. B. Cina: Reducing the susceptibility of alloys particularly aluminium alloys to stress corrosion cracking, US Patent, 1974.
17. Reda · Mater. Sci. Eng. A · 2008 · 485 · 46810.1016/j.msea.2007.08.025 ↗
18. Chen · Mater. Des. · 2012 · 35 · 9310.1016/j.matdes.2011.09.033 ↗
19. Wang · Mater. Des. · 2014 · 55 · 85710.1016/j.matdes.2013.09.063 ↗
20. Han · Mater. Sci. Eng. A · 2011 · 528 · 371410.1016/j.msea.2011.01.068 ↗
21. Abúndez · Mater. Sci. Eng. A · 2016 · 668 · 20110.1016/j.msea.2016.05.062 ↗
22. Thakur · Acta Mater. · 1996 · 45 · 132310.1016/S1359-6454(96)00287-X ↗
23. V. Komisaro, M. Talianker and B. Cina. 221(1996) 113–121.
24. Zhang · Corros. Sci. · 2018
25. A China National Standard · 2005
26. Hou · J.Mater.Sci. · 2018 · 53 · 3846-3841
27. Li · Mater. Charact. · 2009 · 60 · 133410.1016/j.matchar.2009.06.007 ↗
28. Feng · Mater. Des. · 2014 · 60 · 20810.1016/j.matdes.2014.03.064 ↗
29. Liu · Mater. Des. · 2014 · 56 · 102010.1016/j.matdes.2013.12.006 ↗
30. Cao · Mater. Sci. Eng. A · 2016 · 666 · 3410.1016/j.msea.2016.04.022 ↗
31. Fang · J. Alloys Compd. · 2015 · 622 · 16610.1016/j.jallcom.2014.10.044 ↗
32. Svenningsen · Corros. Sci. · 2006 · 48 · 396910.1016/j.corsci.2006.03.018 ↗
33. Liu · J. Alloys Compd. · 2015 · 639 · 26310.1016/j.jallcom.2015.03.174 ↗
34. Davis · 1999 · 25
35. Knight · Corros. Sci. · 2010 · 52 · 407310.1016/j.corsci.2010.08.024 ↗
36. Ramgopal · Corrosion · 2002 · 58 · 68710.5006/1.3287699 ↗