journal article·2015-09

Microstructure evolution during heat treatment and mechanical properties of Mg–2.49Nd–1.82Gd–0.19Zn–0.4Zr cast alloy

S.J. Liu, G.Y. Yang, S.F. Luo, W.Q. Jie

Publisher page

Abstract

Abstract Microstructure evolution during heat treatment and mechanical properties of Mg–2.49Nd–1.82Gd–0.19Zn–0.4Zr cast alloy were investigated experimentally in different stages of heat treatment process. As-cast alloy was found to be consisting of dendritic α(Mg) grains, interdendritic α(Mg) + Mg12Nd eutectic. Within α(Mg) grains, needle-like Mg12Nd phase, quadrate-like Mg5Gd phase and α(Zr) particles were also observed. After a solution treatment at 515 °C for 18 h, α(Mg) + Mg12Nd eutectic was almost dissolved into α(Mg) grain, but a new Zn2Zr3 phase was observed within α(Mg) grains and along grain boundaries. After an aged treatment at 205 °C for 18 h, more dispersed interdendritic Mg12Nd precipitates, coarsened Zn2Zr3 and rod-shaped metastable precipitates of β″(Mg3Nd) and β′(Mg7Nd) were observed within α(Mg) grains. The ultimate tensile strength and the yield strength of the experimental alloy after the aged treatment were measured to be 287 MPa and 206 MPa at room temperature, 240 MPa and 175 MPa at 200 °C, and 220 MPa and 165 MPa at 250 °C, respectively. The improved mechanical properties were also discussed based on the observed microstructure evolution.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Hydrogen Storage and Materials · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. The effect of La or Ce on ageing response and mechanical properties of cast Mg–Gd–Zr alloys10.1016/j.matchar.2007.02.013 ↗
2. Massalski · 1986 · 355
3. Effects of Nd on microstructures and properties at the elevated temperature of a Mg–0.3Zn–0.32Zr alloy10.1016/j.matdes.2010.04.021 ↗
4. Deformation behaviour of Mg-0.7wt.% Nd alloy10.1016/j.jallcom.2003.11.172 ↗
5. Microstructure, mechanical properties, biocorrosion behavior and cytotoxicity of as-extruded Mg–Nd–Zn–Zr alloy with different extrusion ratios10.1016/j.jmbbm.2012.02.002 ↗
6. The effect of grain size on the tensile and creep properties of Mg–2.6Nd–0.35Zn–xZr alloys at 250°C10.1016/j.msea.2012.09.052 ↗
7. Microstructures and mechanical properties of Mg–8Gd–0.6Zr–xNd (x=0, 1, 2 and 3 mass%) alloys10.1007/s10853-006-0451-7 ↗
8. Effect of gadolinium on aged hardening behavior, microstructure and mechanical properties of Mg–Nd–Zn–Zr alloy10.1016/S1003-6326(10)60169-0 ↗
9. Effect of gadolinium on the microstructure and mechanical properties of Mg–Nd–Zn–Zr cast magnesium alloys
10. Microstructure and mechanical properties of high performance Mg–Gd based alloys10.1016/j.matdes.2008.04.069 ↗
11. Precipitation and its effect on the mechanical properties of a cast Mg–Gd–Nd–Zr alloy10.1016/j.msea.2007.11.080 ↗
12. The effect of zirconium grain refinement on the corrosion behaviour of magnesium-rare earth alloy MEZ10.1016/S1471-5317(02)00008-1 ↗
13. Precipitation and hardening in magnesium alloy10.1007/s11661-012-1217-2 ↗
14. Wilson RS, Ph.D. Thesis, Monash University, Victoria, Australia, 2006.
15. High cycle fatigue properties of cast Mg–xNd–0.2Zn–Zr alloys10.1007/s10853-014-8417-7 ↗
16. Effect of heat treatment on the microstructures and mechanical properties of the sand-cast Mg–2.7Nd–0.6Zn–0.5Zr alloy10.1016/j.jma.2014.01.006 ↗
17. Precipitates of γ-Mg17Al12 phase in AZ91 alloy
18. Microstructure and mechanical properties of as-quenched Mg–Gd–Zr alloys10.1016/S1003-6326(11)60773-5 ↗
19. Zhang · 1993 · 62
20. Heterogeneous nucleation of β-type precipitates on nanoscale Zr-rich particles in a Mg–6Zn–0.5Cu–0.6Zr alloy10.1186/1556-276X-7-300 ↗
21. Zr-containing precipitates in Mg-3wt.%Nd-0.2wt.%Zn-0.4wt.%Zr alloy during solution treatment at 540°C10.4028/www.scientific.net/MSF.546-549.97 ↗
22. Porter · 2009
23. Transmission electron microscopy of Zr–Zn precipitate rods in magnesium alloys containing Zr and Zn10.1080/09500830802524096 ↗
24. Creep behavior of Mg-2wt.%Nd binary alloy10.1016/j.msea.2009.06.008 ↗
25. Effects of heat treatments on microstructures and mechanical properties of Mg–4Y–2.5Nd–0.7Zr alloy10.1016/j.msea.2012.06.085 ↗
26. Effects of heat treatments on microstructure and mechanical properties of Mg–11Y–5Gd–2Zn–0.5Zr (wt.%) alloy10.1016/j.jallcom.2010.09.194 ↗
27. Rokhlin · 2003 · 159
28. Microstructure and mechanical properties in cast magnesium–neodymium binary alloys10.1016/j.msea.2007.05.058 ↗
29. Microstructure and strengthening mechanism of high strength Mg–10Gd–2Y–0.5Zr alloy10.1016/j.jallcom.2006.03.015 ↗
30. Microstructure and mechanical properties of the Mg–Gd–Y–Zn–Zr alloy fabricated by semi-continuous casting10.1016/j.msea.2012.04.018 ↗