journal article·2016-11

Microstructural and hardness investigations on a dissimilar metal weld between low alloy steel and Alloy 82 weld metal

Z.R. Chen, Y.H. Lu, X.F. Ding, T. Shoji

Publisher page

Abstract

Abstract The investigation on microstructure and hardness at the fusion boundary (FB) region of a dissimilar metal weld (DMW) between low alloy steel (LAS) A508-III and Alloy 82 weld metal (WM) was carried out. The results indicated that there were two kinds of FBs, martensite FB and sharp FB, with obvious different microstructures, alternately distributed in the same FB. The martensite FB region had a gradual change of elemental concentration across FB, columnar WM grains with high length/width ratios, a thick martensite layer and a wide heat affected zone (HAZ) with large prior austenite grains. By comparison, the sharp FB region had a relatively sharp change of elemental concentration across the FB, WM grains with low length/width ratios and a narrow HAZ with smaller prior austenite grains. The martensite possessed a K-S orientation relationship with WM grains, while no orientation relationship was found between the HAZ grains and WM grains at the sharp FB. Compared with sharp FB there were much more Σ3 boundaries in the HAZ beside martensite FB. The hardness maximum of the martensite FB was much higher than that of the sharp FB, which was attributed to the martensite layer at the martensite FB.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Welding Techniques and Residual Stresses · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Bamford · 2001
2. Crack initiation and propagation close to the interface in a ferrite–austenite joint10.1016/j.msea.2005.01.056 ↗
3. Local mechanical properties of Alloy 82/182 dissimilar weld joint between SA508 Gr.1a and F316 SS at RT and 320°C10.1016/j.jnucmat.2008.11.019 ↗
4. Local mechanical properties of a dissimilar metal welded joint in nuclear power systems10.1016/j.msea.2013.01.037 ↗
5. Microstructure and stress corrosion cracking of the fusion boundary region in an alloy 182-A533B low alloy steel dissimilar weld joint10.1016/j.corsci.2010.08.002 ↗
6. Microstructure and mechanical property of the fusion boundary region in an Alloy 182-low alloy steel dissmilar weld joint10.1007/s10853-010-4581-6 ↗
7. Role of water chemistry and microstructure in stress corrosion cracking in the fusion boundary region of an Alloy 182-A533B low alloy steel dissmilar weld joint in high temperature water10.1016/j.corsci.2011.08.046 ↗
8. Peng · 2005 · 589
9. Microstructure and stress corrosion cracking behavior of the weld metal in Alloy 52-A508 dissimialr welds10.2320/matertrans.M2010294 ↗
10. Effects of thermal aging on microstructures of low alloy steel–Ni base alloy dissimilar metal weld interfaces10.1016/j.jnucmat.2013.07.003 ↗
11. Nano-structural and nano-chemical analysis of Ni-base alloy/low alloy steel dissimilar metal weld interfaces10.5516/NET.07.2012.009 ↗
12. Dissimilar metal welds-transition joints literature review
13. Stainless steel weld deposits on mild and alloy steels
14. The interfacial microstructure of weld overlay of corrosion resistant alloys10.1016/0956-716X(94)90327-1 ↗
15. The effect of PWHT on the material properties and micro structure in Inconel 625 and Inconel 725 buttered joints
16. Characterisation of microstructures in nickel based transition joints10.1023/A:1004846607046 ↗
17. Direct TEM observation of microstructures of the austenitic10.1007/BF00587687 ↗
18. Morphologies of the transition region in dissimilar austenitic-ferritic welds10.1016/1044-5803(95)00249-9 ↗
19. Characteristic of the weld interface in dissimilar austenitic-pearlitic steel welds10.1016/1044-5803(94)90070-1 ↗
20. TEM observation of martensite layer at the weld interface of an A508III to Inconel 82 dissimilar metal weld joint10.1007/s11661-015-3171-2 ↗
21. Characterization of low alloy ferritic steel–Ni base alloy dissimilar metal weld interface by SPM techniques, SEM/EDS, TEM/EDS and SVET10.1016/j.matchar.2014.12.007 ↗
22. Über den mechanismus der stahlhärtung10.1007/BF01397346 ↗
23. Kou · 2002
24. Martensite formation in austenitic/ferritic dissimilar alloy welds
25. DuPont · 2010
26. Microstructures and microhardness at fusion boundary of 316 stainless steel/Inconel 182 dissimilar welding10.1016/j.matchar.2015.07.018 ↗
27. Toughness of CGHAZs of welds in Q&T steels
28. Grain refinement of HAZ in multi-pass welding10.1016/j.jmatprotec.2013.12.017 ↗
29. Temperature distribution during multipass welding of plates10.1016/S0308-0161(98)00094-5 ↗