Fatigue behaviour of monotectoid-based Zn–Al–Cu alloys in 3.5% NaCl and 1% HCl solutions
Source abstract
Abstract
Abstract One binary Zn–40Al and three Zn–40Al-based ternary alloys containing 1%, 3%, and 5% Cu were produced by permanent mold casting. Their fatigue behavior was investigated in 3.5% NaCl and 1% HCl solutions by a rotary bending fatigue test machine at a frequency of 33.3 Hz. The stress amplitude versus number of cycles to failure (S–N) curves of the alloys was plotted for both environments. Corrosion degradation factors of the alloys were determined. The corrosion environments reduced the fatigue strength and fatigue life of the alloys considerably. However, acid solution was found to be more detrimental for these alloys than the salt water. In addition, copper content was found to be less effective on the fatigue strength and fatigue life of the alloys in both salt water and acid solution than it was in air. Corrosion degradation factor of the alloys increased with increasing copper content up to approximately 3%, above which it decreased as the copper content increased. It was also shown that the fatigue data obtained from the monotectoid-based Zn–Al–Cu alloys in the corrosive environments obey the Basquin's law.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Goodwin · 1989 · 82
2. Microstructural observations on the frequency effect in the fatigue behaviour of superplastic Zn–Al eutectoid10.1179/msc.1977.11.3.103 ↗
3. Fatigue behaviour of zinc–aluminium casting alloys10.1179/026708301101510393 ↗
4. Fatigue properties of zinc–aluminium alloys in 3.5% NaCl and 1% HCl solutions10.1016/S0142-1123(03)00091-4 ↗
5. Wear resistance and microstructure of Zn–Al–Si and Zn–Al–Cu alloys10.1016/0043-1648(87)90245-6 ↗
6. Dry sliding friction and wear properties of zinc-based alloys10.1016/S0043-1648(02)00050-9 ↗
7. Relationships between secondary dendrite arm spacing and mechanical properties of Zn–40Al–Cu alloys10.1023/A:1024434602540 ↗
8. Corrosion fatigue behaviour of ion nitrided AISI 4140 steel10.1016/S0921-5093(00)00835-2 ↗
9. Fatigue behaviour of a commercial aluminium alloy in sea water at different temperatures10.1016/0013-7944(93)90015-K ↗
10. Effect of alloying content on high cycle fatigue behaviour of Cu–Ti alloys10.1016/S0142-1123(96)00041-2 ↗
11. Dieter GE. Mechanical metallurgy. New York: Mc-Graw Hill; 1976. p. 210–16, 433.
12. General aspects of corrosion fatigue in metals and alloys
13. Ashby · 1980 · 141
14. Comparison of corrosion fatigue cracking of Al–Li alloy AA2090-T8E41 in salt water10.5006/1.3577868 ↗
15. The role of environmental exposure in the fatigue behaviour of an aluminium alloy10.1016/S0010-938X(97)00095-4 ↗
16. Rolls · 1976 · 287
17. Avner · 1974 · 493
18. Jones · 1996 · 357
19. Atkins · 1997 · 77
20. Decomposition of Zn–Al alloys on quench-aging10.1179/mst.1990.6.8.695 ↗
21. Metallography of zinc–25% Al based alloys in the as-cast and aged conditions10.1515/pm-1987-240503 ↗