Thermal stability of a Stellite/steel hardfacing interface during long-term aging
Source abstract
Abstract
Abstract Disbonding and delamination of Stellite hardfacing used in high-temperature valves have caused serious challenges in the power generation industry in recent years. To determine the microstructural factors that may contribute to the failures, Stellite 21 and Stellite 6 hardfacing alloys were deposited onto an F91 steel substrate using plasma-transferred arc welding. A series of aging experiments simulating service temperatures were conducted at temperatures between 550 and 650 °C for exposure times ranging from 1008 to 8760 h. The F91/S21 interface was found to be unstable during aging; a hard layer was formed, consisting mainly of three phases. This layer follows a parabolic rate of growth; its thickness increases as the square root of aging time. The activation energy was determined, which might be associated with carbon diffusion. Complementary characterization methods showed that the three phases in the hard layer are: a BCC-like intermetallic compound, FexCoy; a Cr-rich M23C6-type carbide; and an (Fe,Co)(Cr,Mo)-type σ phase. The area fraction and the equivalent diameter of the M23C6 carbides increase with aging temperature and time, while the area fraction of the σ phase decreases with temperature. Nanoindentation maps showed that both the M23C6 carbides and the σ phase in the interfacial layer are significantly harder than the other phases. The σ phase contributes more in the increase of the interfacial layer's hardness at lower temperatures than that at higher temperatures. These hard phases may affect high-temperature valve integrity.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal Alloys Wear and Properties · Advanced materials and composites · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (52)
Show source-provided references
1. Elevated temperature ferritic and martensitic steels and their application to future nuclear reactors10.1179/174328005X41140 ↗
2. Ferritic/martensitic steels for next-generation reactors10.1016/j.jnucmat.2007.05.005 ↗
3. Hardfacing, weld cladding, and dissimilar metal joining
4. Wrought and P/M superalloys
5. High temperature sliding wear behaviour of Inconel 617 and Stellite 6 alloys10.1016/j.wear.2010.07.005 ↗
6. Purdy · 2015
7. Valves didn’t get the respect they deserved
8. Inspect steam valves for stellite delamination
9. Integrated multiphysics modeling in materials and manufacturing processes
10. Interface microstructure of Stellite-6 coatings on a 12%Cr steel after long term thermal exposure
11. ISO 14577-1 · 2002 · 2002
12. Delamination failures of Stellite hardfacing in power plants: a microstructural characterisation study10.1179/1362171814Y.0000000213 ↗
13. Why new U.S. supercritical units should consider T/P92 piping
14. ASTM A182/A182M-18 · 2018
15. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
16. Narlikar · 2014
17. Inhomogeneous nano-mechanical properties in the multi-phase microstructure of long-term aged type 316 stainless steel10.1557/jmr.2006.0143 ↗
18. Precipitation kinetics of M23C6 in T/P92 heat-resistant steel by applying soft-impingement correction10.1557/jmr.2013.116 ↗
19. Hosford · 2010
20. Rehman · 2016
21. Interdiffusion in the Fe-Ni, Ni-Co, and Fe-Co systems10.1002/pssa.2210200129 ↗
22. Correlations for diffusion constants10.1016/0001-6160(80)90092-9 ↗
23. Diffusion of carbon in cobalt10.2320/matertrans1989.30.984 ↗
24. Vacancy-mediated diffusion of carbon in cobalt and its influence on CO activation10.1039/b925764k ↗
25. Structure and thermomagnetic properties of new FeCo-based nanocrystalline ferromagnets10.1109/20.951142 ↗
26. Pinning effect of the grain boundaries on magnetic domain wall in FeCo-based magnetic alloys10.1063/1.370175 ↗
27. Direct observations of sigma phase formation in duplex stainless steels using in-situ synchrotron X-ray diffraction10.1007/s11661-006-9076-3 ↗
28. Kinetics of sigma phase formation in a duplex stainless steel
29. The influence of temperature on σ-phase formation and the resulting hardening of Fe–Cr–Mo-alloys10.1023/A:1017012831969 ↗
30. Kinetics of reactive diffusion between Au and Sn during annealing at solid-state temperatures10.1016/j.msea.2004.08.053 ↗
31. Reactive diffusion between Ag-5Pt alloy and Sn at solid-state temperatures10.2320/matertrans.MRA2007149 ↗
32. Heitjans · 2005
33. Detecting transformation of delta-ferrite to sigma-phase in stainless steels by advanced metallographic techniques
34. Comparative study on sigma phase precipitation of three types of stainless steels: austenitic, superferritic and duplex10.1179/174328406X109230 ↗
35. The influence of Mo on the formation of the σ-phase in Fe-Cr alloys10.1023/A:1011009315770 ↗
36. Kinetics of transformation of delta ferrite during creep in a type 316(N) stainless steel weld metal10.1016/S0921-5093(03)00371-X ↗
37. Influence of Si on sigma phase precipitation and pitting corrosion in superaustenitic stainless steel weld metal10.1016/j.matchemphys.2017.12.055 ↗
38. Topologically close-packed structures of transition metal alloys10.1016/0079-6425(72)90002-3 ↗
39. Application of small punch test to evaluate sigma-phase embrittlement of pressure vessel cladding material10.1080/18811248.2003.9715404 ↗
40. Effect of intermetallic precipitations on the properties of duplex stainless steel10.1016/j.matchar.2006.03.015 ↗
41. Influence of σ-phase on mechanical properties and corrosion resistance of duplex stainless steels10.1016/S0010-938X(99)00009-8 ↗
42. Tribological behavior of Stellite 21 modified with yttrium10.1016/j.wear.2004.07.013 ↗
43. Microstructure and wear behavior of stellite 6 cladding on 17-4 PH stainless steel10.1016/j.jallcom.2010.09.216 ↗
44. Strengthening mechanisms of creep resistant tempered martensitic steel10.2355/isijinternational.41.641 ↗
45. Precipitate design for creep strengthening of 9% Cr tempered martensitic steel for ultra-supercritical power plants10.1088/1468-6996/9/1/013002 ↗
46. Analysis of creep rates of tempered martensitic 9%Cr steel based on microstructure evolution10.1016/j.msea.2008.04.118 ↗
47. Creep deformation behavior of 9Cr1MoVNb (ASME Grade 91) steel10.1016/j.msea.2016.10.112 ↗
48. Precipitation of M23C6 and its effect on tensile properties of 0.3C–20Cr–11Mn–1Mo–0.35N steel10.1016/j.matdes.2015.04.016 ↗
49. Lee · 2015 · 46
50. Influence of grain boundary carbides on mechanical properties of high nitrogen austenitic stainless steel10.1016/j.matdes.2012.01.024 ↗
51. M23C6 precipitation behavior in a Ni-base superalloy M96310.1007/s10853-005-2418-5 ↗
52. Coarsening of precipitates in an advanced creep resistant 9% chromium steel—quantitative microscopy and simulations10.1016/S0921-5093(01)01874-3 ↗