journal article·2021-05

Erosion-corrosion of 304N austenitic steels in liquid Pb Bi flow perpendicular to steel surface

Cong Li, Yujing Liu, Feifei Zhang, Xiaodong Fang, Zheng Liu

Publisher page

Abstract

Abstract In this paper, corrosion performance of 304N austenitic stainless steel with 0.17 wt.% nitrogen was studied in flowing oxygen-saturated lead bismuth eutectic (LBE) at 400 °C. Perpendicular flow pattern was introduced to steel surface, on which various corrosion behaviors, i.e. oxidation, erosion, and dissolution, were simultaneously detected even at a low fluid rate of ~1 m/s after 1000 h. This allowed an investigation into their synergistic effects. Besides, degradation in chemical compositions and mechanical properties was profoundly identified within steel subsurface by means of multi-scale characterization. Role of subsurface degradation in different corrosion failure modes was then elucidated. With regard to breakaway oxidation, an interesting mechanism was proposed for this essential feature of austenitic steels. Plastic deformation microstructure within perpendicularly eroded austenitic steel subsurface, confirmed in other flowing corrosive media, was revealed in liquid LBE flow for the first time and explained in terms of stacking fault energy. Crack across the degraded steel subsurface was proven to be responsible for LBE penetration and selective dissolution attack on steel matrix.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Nuclear Materials and Properties · Fusion materials and technologies · Nuclear reactor physics and engineering

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (70)

Show source-provided references
1. Designing a high Si reduced activation ferritic/martensitic steel for nuclear power generation by using Calphad method10.1016/j.jmst.2018.07.002 ↗
2. Lead–Bismuth Eutectic (LBE): a coolant candidate for gen. IV Advanced nuclear reactor concepts10.1002/adem.201300296 ↗
3. Creep failure of a solution-annealed 15-15Ti steel exposed to stagnant lead-bismuth eutectic at 550 and 600 °C10.1016/j.msea.2020.140230 ↗
4. Materials selection for nuclear applications: challenges and opportunities10.1016/j.scriptamat.2017.04.027 ↗
5. 22 - Corrosion issues in lead-cooled fast reactor (LFR) and accelerator driven systems (ADS)
6. Interface morphologies and embrittlement behavior of α-Fe in liquid lead-bismuth eutectic at elevated temperature10.1016/j.matchar.2018.10.017 ↗
7. Microstructural evolution of liquid metal embrittlement in resistance-spot-welded galvanized TWinning-Induced Plasticity (TWIP) steel sheets10.1016/j.matchar.2018.11.008 ↗
8. Liquid metal embrittlement of an austenitic stainless steel in liquid sodium10.1016/j.corsci.2014.02.031 ↗
9. Oxidation mechanism of refractory Molybdenum exposed to oxygen-saturated lead-bismuth eutectic at 600 °C10.1016/j.corsci.2020.109132 ↗
10. Dissolution mechanism of 316L in lead–bismuth eutectic at 500°C10.1016/j.corsci.2011.05.031 ↗
11. Corrosion behaviour of steels and refractory metals and tensile features of steels exposed to flowing PbBi in the LECOR loop10.1016/S0022-3115(03)00009-6 ↗
12. Compatibility tests on steels in molten lead and lead–bismuth10.1016/S0022-3115(01)00538-4 ↗
13. Corrosion behaviour of stainless steels in flowing LBE at low and high oxygen concentration10.1016/j.jnucmat.2004.07.011 ↗
14. Behavior of steels in flowing liquid PbBi eutectic alloy at 420–600 °C after 4000–7200 h10.1016/j.jnucmat.2004.07.010 ↗
15. Quantification of the long-term performance of steels T91 and 316L in oxygen-containing flowing lead-bismuth eutectic at 550° C10.1115/1.4000364 ↗
16. Analysis of bi-layer oxide on austenitic stainless steel, 316L, exposed to Lead–Bismuth Eutectic (LBE) by X-ray Photoelectron Spectroscopy (XPS)10.1016/j.jnucmat.2013.03.093 ↗
17. Transmission electron microscopy (TEM) on oxide layers formed on D9 stainless steel in lead bismuth eutectic (LBE)10.1016/j.corsci.2012.09.019 ↗
18. Transmission electron microscopy study of complex oxide scales on DIN 1.4970 steel exposed to liquid Pb-Bi eutectic10.1016/j.corsci.2018.10.018 ↗
19. Oxidation mechanism of a Fe-9Cr-1Mo steel by liquid Pb–Bi eutectic alloy (Part III)10.1016/j.corsci.2008.06.049 ↗
20. Oxidation mechanism of an Fe–9Cr–1Mo steel by liquid Pb–Bi eutectic alloy at 470°C (Part II)10.1016/j.corsci.2008.06.051 ↗
21. A review of steel corrosion by liquid lead and lead–bismuth10.1016/j.corsci.2009.03.013 ↗
22. Analysis on liquid metal corrosion–oxidation interactions10.1016/j.corsci.2007.05.012 ↗
23. Modeling of flow-induced corrosion with nonuniform boundary conditions10.5006/1.3278386 ↗
24. Twin boundary-accelerated ferritization of austenitic stainless steels in liquid lead–bismuth eutectic10.1016/j.scriptamat.2016.02.029 ↗
25. Dissolution corrosion of 316L austenitic stainless steels in contact with static liquid lead-bismuth eutectic (LBE) at 500 °C10.1016/j.jnucmat.2017.04.004 ↗
26. Corrosion of T91 and pure iron in flowing and static Pb-Bi alloy between 450 °C and 540 °C: experiments, modelling and mechanism10.1016/j.corsci.2020.108897 ↗
27. Selective leaching of nickel and chromium from Type 316 austenitic steel in oxygen-containing lead–bismuth eutectic (LBE)10.1016/j.corsci.2014.03.016 ↗
28. Oxide scale formation on 316L and FeCrAl steels exposed to oxygen controlled static LBE at temperatures up to 800 °C10.1016/j.solmat.2015.09.007 ↗
29. Oxygen concentration measurement and control of lead-bismuth eutectic in a small, static experimental facility10.1080/00223131.2019.1700842 ↗
30. Control of oxygen concentration in liquid lead and lead–bismuth10.1016/S0022-3115(03)00250-2 ↗
31. Modelling of the oxide scale formation on Fe-Cr steel during exposure in liquid lead-bismuth eutectic in the 450–600°C temperature range10.1002/maco.201005871 ↗
32. Fazio · 2015
33. Dissolution and oxidation behaviour of various austenitic steels and Ni rich alloys in lead-bismuth eutectic at 520 °C10.1016/j.jnucmat.2015.11.005 ↗
34. A synergy of different corrosion failure modes pertaining to T91 steel impacted by extreme lead–bismuth eutectic flow pattern10.1016/j.corsci.2020.109214 ↗
35. Liquid metal corrosion/erosion investigations of structure materials in lead cooled systems: part 110.1016/j.jnucmat.2008.12.327 ↗
36. Long-term behaviors of oxide layer in liquid Lead–bismuth eutectic (LBE), part I: model development and validation10.1007/s11085-013-9450-7 ↗
37. Oxidation mechanism of T91 steel in liquid lead-bismuth eutectic: with consideration of internal oxidation10.1038/srep35268 ↗
38. A comparative study on the compatibility of liquid lead–gold eutectic and liquid lead–bismuth eutectic with T91 and SS 316LN steels10.1016/j.jnucmat.2012.04.015 ↗
39. Long term corrosion on T91 and AISI1 316L steel in flowing lead alloy and corrosion protection barrier development: experiments and models10.1016/j.jnucmat.2011.04.028 ↗
40. Flow-accelerated corrosion of type 316L stainless steel caused by turbulent lead–bismuth eutectic flow10.3390/met8080627 ↗
41. Cavitation wear behaviour of austenitic stainless steels with different grain sizes10.1016/j.wear.2004.03.024 ↗
42. Effect of nitrogen on the corrosion–erosion synergism in an austenitic stainless steel10.1016/j.triboint.2010.12.013 ↗
43. Erosion–corrosion resistance properties of 316L austenitic stainless steels after low-temperature liquid nitriding10.1016/j.apsusc.2018.01.225 ↗
44. Raman microspectroscopy of some iron oxides and oxyhydroxides10.1002/(SICI)1097-4555(199711)28:11<873::AID-JRS177>3.0.CO;2-B ↗
45. A Raman study of the systems Fe3-xCrxO4 and Fe2-xCrxO310.1016/0022-4596(89)90245-4 ↗
46. Composition, structure and properties of the oxide films formed on the stainless steel 316L in a primary type PWR environment10.1016/S0010-938X(97)00158-3 ↗
47. Mechanism of breakaway oxidation of Fe–Cr and Fe–Cr–Ni alloys in dry and wet carbon dioxide10.1016/j.corsci.2013.08.008 ↗
48. Young · 2016
49. Thermodynamic assessment of solubility and activity of iron, chromium, and nickel in lead bismuth eutectic10.1016/j.jnucmat.2014.03.011 ↗
50. Influence of temperature on the interaction mode of T91 and AISI 316L steels with Pb–Bi melt saturated by oxygen10.1016/j.corsci.2008.02.006 ↗
51. High-temperature oxidation of FeCr(Ni) alloys: the behaviour after breakaway10.1007/s11085-017-9731-7 ↗
52. Oxidation after breakdown of the chromium-rich scale on stainless steels at high temperature: internal oxidation10.1007/s11085-016-9610-7 ↗
53. New insights into the effects of surface nanocrystallization on the oxidation of 321 austenitic stainless steel in a humid oxygen environment at 1000°C10.1016/j.corsci.2018.11.024 ↗
54. Subsurface characterization of high-strength high-interstitial austenitic steels after impact wear10.1016/j.wear.2018.02.016 ↗
55. On the microstructural evolution pattern toward nano-scale of an AISI 304 stainless steel during high strain rate surface deformation10.1016/j.jmst.2020.01.027 ↗
56. XRD and EBSD studies of severe shot peening induced martensite transformation and grain refinements in austenitic stainless steel10.1016/j.matchar.2020.110574 ↗
57. Sub-surface measurements of the austenite microstructure in response to martensitic phase transformation10.1016/j.actamat.2019.08.036 ↗
58. Significant influence of rolling modes on martensitic transformation, microstructural evolution and texture development in a 304 stainless steel10.1016/j.matchar.2019.110073 ↗
59. Uncoupling the effects of strain rate and adiabatic heating on strain induced martensitic phase transformations in a metastable austenitic steel10.1016/j.actamat.2019.06.053 ↗
60. Effect of grain refinement on thermal stability of metastable austenitic steel10.2320/matertrans.45.2245 ↗
61. Breakaway oxidation of Fe10%Cr and Fe20%Cr at temperatures up to 600°C10.1016/0010-938X(77)90053-1 ↗
62. Oxidation of a Fe–18Cr–8Ni austenitic stainless steel at 850 °C in O2: microstructure evolution during breakaway oxidation10.1016/j.corsci.2016.10.029 ↗
63. Breakaway oxidation behaviour of ferritic stainless steels at 1150 °C in humid air10.1016/j.corsci.2016.02.042 ↗
64. Modelling impact angle effects on erosion–corrosion of pure metals: construction of materials performance maps10.1016/j.wear.2005.02.012 ↗
65. Effect of the amount of cold work on corrosion of 304 nuclear grade stainless steel in high temperature water10.5006/2436 ↗
66. Beneficial effect of cold-working on high temperature oxidation resistance of austenitic stainless steel10.1016/j.corsci.2019.108149 ↗
67. The role of surface deformation in the oxidation response of type 304 SS in high temperature deaerated water10.1016/j.corsci.2018.06.033 ↗
68. The effect of shot peening on steam oxidation of 304H stainless steel10.1007/s11085-019-09951-9 ↗
69. In situ X-ray diffraction of surface oxide on type 430 stainless steel in breakaway condition using synchrotron radiation10.1016/j.corsci.2011.10.018 ↗
70. Orientation relationship of the austenite-to-ferrite transformation in austenitic stainless steels due to dissolution corrosion in contact with liquid Pb-Bi eutectic10.1016/j.scriptamat.2019.03.035 ↗