In-situ spherical TiB2/Cu composite powder: A new method of liquid phase reaction coupled with gas atomization
Source abstract
Abstract
The spherical TiB 2 /Cu composite powder was fabricated by a new method of liquid-phase in-situ reaction coupled with inert gas atomization. The powder morphology, characteristic indexes, microstructure and nanoindentation hardness were investigated. The effects of spheroidization time and solidification rate of atomized molten droplets on powder sphericity and the relationship between in-situ reaction control and TiB 2 distribution were discussed. Results indicate that the powder has a good sphericity and d 50 is 32.86 μm, in addition to 75% fine powder yield (<45 μm). The in-situ formed TiB 2 particles (TiB 2p ) were uniformly distributed in grain boundaries and intragrain. The rapid solidification of molten droplets and the inhibition of copper grain growth by TiB 2p refined the Cu matrix grain size (4.34 μm). The nanoindentation hardness of composite powder is 3.17 GPa, which is 1.9 times higher than that of spherical Cu powder, and the reasons for the increased hardness of powder are also discussed.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Advanced materials and composites · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. Material-structure-performance integrated laser-metal additive manufacturing10.1126/science.abg1487 ↗
2. In situ synthesis of TiC nano-reinforcements in aluminum matrix composites during mechanical alloying10.1016/j.compositesb.2018.02.023 ↗
3. Surface post-treatments for metal additive manufacturing: Progress, challenges, and opportunities
4. Fine spherical powder production during gas atomization of pressurized melts through melt nozzles with a small inner diameter10.1016/j.powtec.2019.09.023 ↗
5. Microstructure and mechanical properties of a TiB2-modified Al-Cu alloy processed by laser powder-bed fusion10.1016/j.msea.2020.140209 ↗
6. Enhanced strength and ductility of nano-TiBw-reinforced titanium matrix composites fabricated by electron beam powder bed fusion using Ti6Al4V-TiBw composite powder
7. Microstructural evolution and mechanical performance of in-situ TiB2/AlSi10Mg composite manufactured by selective laser melting10.1016/j.jallcom.2020.157287 ↗
8. Additively manufactured copper matrix composites: heterogeneous microstructures and combined strengthening effects10.1557/jmr.2020.62 ↗
9. Mechanical, thermal, and corrosion properties of Cu-10Sn alloy fabricated by laser-powder-bed-fusion additive manufacturing
10. Performance improvement of laser additive manufactured Cu-Cr alloy via continuous extrusion10.1016/j.jallcom.2021.160475 ↗
11. Obtaining of reinforced Cu-Ti, Cu-Ti-TiB2 foils through green compact laser sintering10.1016/j.jallcom.2018.05.135 ↗
12. Manufacturing Fe-TiC composite powder via inert gas atomization by forming reinforcement phase in-situ10.1002/adem.202000717 ↗
13. Laser additive manufacturing of nano-TiC reinforced Ni-based nanocomposites with tailored microstructure and performance10.1016/j.compositesb.2018.12.146 ↗
14. Fabrication and properties of the TiC reinforced high-strength steel matrix composite10.1016/j.ijrmhm.2016.03.013 ↗
15. In-situ fabrication and characterization of ultrafine structured Cu-TiC composites with high strength and high conductivity by mechanical milling10.1016/j.jallcom.2015.10.061 ↗
16. In-situ TiC particle reinforced Ti-Al matrix composites: powder fabrication by mechanical alloying and selective laser melting behavior10.1016/j.apsusc.2009.07.008 ↗
17. Thermodynamic analysis of Ti-Al-C inter-metallics formation by mechanical alloying10.1016/j.jallcom.2013.05.196 ↗
18. Progress in gas atomization of liquid metals by means of a De Laval nozzle10.1016/j.powtec.2008.04.071 ↗
19. TiB nano-whiskers reinforced titanium matrix composites with novel nano-reticulated microstructure and high performance via composite powder by selective laser melting10.1016/j.msea.2020.140137 ↗
20. Interaction mechanisms between ceramic particles and atomized metallic droplets10.1007/BF02651770 ↗
21. Relationship between microstructure, properties and reaction conditions for Cu-TiB2 alloys fabricated by in-situ reaction10.1016/j.actamat.2009.06.030 ↗
22. Phase selection of titanium boride in copper matrix composites during solidification10.1007/s10853-016-0592-2 ↗
23. Effect of La addition on the particle characteristics, mechanical and electrical properties of in-situ Cu-TiB2 composites10.1016/j.jallcom.2016.06.129 ↗
24. Pure copper components fabricated by cold spray (CS) and selective laser melting (SLM) technology10.1016/j.surfcoat.2020.125936 ↗
25. High-fidelity modelling of selective laser melting copper alloy: Laser reflection behavior and thermal-fluid dynamics10.1016/j.matdes.2021.109857 ↗
26. Strengthening mechanisms in particulate metal matrix composites10.1016/0956-716X(91)90349-6 ↗
27. The dispersion mechanism of TiB2 ceramic phase in molten aluminium and its alloys10.1016/S0261-3069(97)00068-X ↗
28. Comparison between current models for the strength of particulate reinforced metal matrix nanocomposites with emphasis on consideration of hall-Petch effect10.1016/j.msea.2011.10.043 ↗
29. Characterization of spherical AlSi10Mg powder produced by double-nozzle gas atomization using different parameters10.1016/S1003-6326(19)64947-2 ↗
30. Heat exchange between metal particles and gas in the atomization process10.1007/BF00774694 ↗
31. Determination of the thermophysical properties of liquid and solid Ti-6Al-4V alloy10.1007/s00339-016-9783-6 ↗
32. Non-contact measurements of surface tension and viscosity of niobium, zirconium, and titanium using an electrostatic levitation furnace10.1023/A:1015459222027 ↗
33. Impact of process flow conditions on particle morphology in metal powder production via gas atomization10.1016/j.apt.2019.10.022 ↗
34. Influence of the thermal history of a particle during atomization on the morphology of carbides in a hypereutectic iron-based alloy10.1016/j.jallcom.2012.01.139 ↗
35. Solidification behavior of in-situ TiB2/Cu composite powders during reactive gas atomization10.1007/s11595-021-2395-9 ↗
36. Redistribution of particles during solidification10.2355/isijinternational.35.693 ↗
37. Nanoparticle-inhibited growth of primary aluminum in Al-10Si alloys10.1016/j.actamat.2015.10.005 ↗
38. Particle engulfment and pushing by solidifying interfaces: part II: microgravity experiments and theoretical analysis10.1007/s11661-998-0092-3 ↗
39. Microstructural and mechanical characteristics of in-situ metal matrix composites10.1016/S0927-796X(00)00024-3 ↗
40. Effect of in-situ reaction conditions on the microstructure changes of Cu-TiB2 alloys by combining in-situ reaction and rapid solidification10.1016/j.matchemphys.2011.10.019 ↗
41. Effect of La addition on microstructures and properties of TiB2(-TiB)/Cu hybrid composites fabricated by in-situ reaction10.1016/j.msea.2020.139605 ↗
42. Dry sliding wear behavior of in-situ Cu-TiB2 nanocomposites against medium carbon steel10.1016/S0043-1648(03)00115-7 ↗
43. Tensile and fracture behavior of nano/micro TiB2 particle reinforced casting A356 aluminum alloy composites10.1016/j.matdes.2014.10.048 ↗