Microstructure evolution and mechanical performance of nickel based superalloy C1023 at elevated temperatures
Source abstract
Abstract
Abstract Microstructure evolution of polycrystalline nickel based superalloy C1023 casting was investigated by comparing as cast superalloy and heat treated superalloy in the paper. Influences of strengtheners and carbides on the tensile behaviors of heat treated superalloy at different temperatures (20 °C, 650 °C, and 850 °C) were studied. Resulting data from deep corrosion suggested that growth mode of scripted carbide included nucleation on the vertex of blocky carbonitride, expansion of dendrite arm in C-rich area, and enlargement of dendrite cap. Decomposition of MC carbide generated numerous octahedral M23C6 carbide as well as nanoscale Cr-Mo-rich nuclei. Diffusion of Mo from γ to precipitates such as γ', MC, and M23C6, occurred during the heat treatment while irregular γ' (4 nm–500 nm) transformed into cuboidal particles. At 650 °C, no significant deterioration of tensile strength was found while plastic deformation ability of γ base was improved. Oxidation of grain boundaries (GBs) dominated the crack behavior of the superalloy at 850 °C.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High Temperature Alloys and Creep · High-Temperature Coating Behaviors · Advanced Materials Characterization Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Effects of Cr content on microstructure and mechanical properties of single crystal superalloy10.1016/S1003-6326(15)63663-9 ↗
2. Effect of minor carbon additions on the high-temperature creep behavior of a single-crystal nickel-based superalloy10.1016/j.matchar.2015.04.007 ↗
3. The effect of γ′ content on the densities of Ni-based superalloys10.1007/s11663-006-0060-5 ↗
4. Coarsening kinetics of γ′ precipitates in the commercial nickel base Superalloy René 88 DT10.1016/j.actamat.2009.02.010 ↗
5. Effect of carbon addition on carbide morphology of single crystal Ni-based superalloy10.1016/S1003-6326(14)63066-1 ↗
6. Identification of Mo-rich M23C6 carbides in alloy 71810.1007/s11661-016-3593-5 ↗
7. Carbide precipitation in nickel base superalloys 718 and 625 and their effect on mechanical properties
8. Effect of melt heat treatment on MC carbide formation in nickel-based superalloy K46510.1016/j.rinp.2017.06.020 ↗
9. Effect of melt treatment on carbides formation in a cast nickel-base superalloy M96310.1016/j.jmatprotec.2006.11.002 ↗
10. Donachie · 2002
11. Investigation of solidification and segregation characteristics of cast Ni-base superalloy K417G
12. Effects of heat treatments on the microstructure and mechanical properties of Rene 8010.1016/j.matdes.2012.06.039 ↗
13. Site preference of metallic elements in M23C6 carbide in a Ni-based single crystal superalloy10.1016/j.matdes.2017.05.023 ↗
14. Thermal stability of primary MC carbide and its influence on the performance of cast Ni-base superalloys10.1016/j.matdes.2014.12.038 ↗
15. Influence of cooling rate on the development of multiple generations of γ′ precipitates in a commercial nickel base superalloy10.1016/j.matchar.2011.06.002 ↗
16. Mechanisms related to different generations of γ′ precipitation during continuous cooling of a nickel base superalloy10.1016/j.actamat.2012.09.058 ↗
17. Key aspects of carbide precipitation during solidification in the Ni-base superalloy, MAR M00210.1016/j.jallcom.2017.01.104 ↗
18. Influence of high-temperature annealing on morphological and compositional changes of phases in Ni-base single crystal superalloy10.1016/j.matchar.2017.07.021 ↗
19. Time-resolved synchrotron diffractometry of phase transformations in high strength nickel-based superalloys10.1016/j.actamat.2015.04.046 ↗
20. EELS analysis of the nitrogen content of carbide particles in a commercial γ′-strengthened nickel-base superalloy10.1016/j.scriptamat.2015.05.016 ↗
21. Effect of solidification condition and carbon content on the morphology of MC carbide in directionally solidified nickel-base superalloys10.1016/j.jmst.2014.06.010 ↗
22. Effects of microporosity and precipitates on the cracking behavior in polycrystalline superalloy Inconel 71810.1016/j.matchar.2017.08.012 ↗
23. Role of shrinkage pores, carbides on cyclic deformation behaviour of conventionally cast nickel base superalloy CM247LC® at 870 °C10.1016/j.msea.2015.12.054 ↗
24. Formation of carbides and their effects on stress rupture of a Ni-base single crystal superalloy10.1016/S0921-5093(03)00517-3 ↗
25. Thermo-mechanical fatigue behaviour and life prediction of C-1023 nickel based superalloy
26. Failure analysis of gas turbine first stage blade made of nickel-based superalloy10.1016/j.csefa.2017.04.002 ↗
27. Thermomechanical fatigue tests development and life prediction of a nickel base superalloy10.1007/s40799-016-0078-9 ↗
28. Investigation of oxidation characteristics and atomic partitioning in platinum and ruthenium bearing single-crystal Ni-based superalloys10.1007/s11661-006-0083-1 ↗
29. Application-oriented description of time−/temperature dependent crack growth in a conventionally cast nickel-based superalloy10.1016/j.ijfatigue.2016.11.025 ↗