Effects of current-assisted heat treatment time on microstructure evolution and superplastic properties of Ti-22Al-24Nb-0.5Mo alloy
Source abstract
Abstract
Abstract The Ti-22Al-24Nb-0.5Mo alloy was exposed at 1050 °C in the α2 + B2 two-phase region for various current-assisted heat treatment (CAHT) time. The effects that the heating time had on phase transformation, recrystallization, and texture evolution of the Ti-22Al-24Nb-0.5Mo alloy were systematically investigated using scanning electron microscopy coupled with electron backscattered diffraction (SEM-EBSD). The results showed that O → B2 + α2 and α2 → B2 transformation occurred during the CAHT process, where the O phase transformed into B2 phase at a relatively rapid rate, and the transformation rate of α2 to B2 was relatively slow. As the CAHT time increased, the B2 grains recrystallized (t = 0.5–10 min) and the secondary recrystallization (t = 15 min) were expressed as the Miller index of (112) [ 0 3 ¯ 1 ], and the microstructure and texture orientation changed significantly during the CAHT process. Tensile tests were performed at 970 °C to study the high-temperature performance of the as-received sheet and the sheets following the various CAHT time. The work hardening, dynamic recovery softening and grain coarsening process existed simultaneously in the alloy at high temperatures. When the CAHT time was 1 min, the superplastic tensile property of the sheet was the best with the elongation of 224.6%, which corresponded to the smallest and the largest sizes and the number of fracture cavities.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electromagnetic Effects on Materials · Intermetallics and Advanced Alloy Properties · Semiconductor materials and interfaces
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Phase stability and ordering behaviour of the O phase in Ti-Al-Nb alloys10.1016/0966-9795(95)98930-7 ↗
2. Intermetallic alloys based on orthorhombic titanium aluminide10.1002/1527-2648(200111)3:11<851::AID-ADEM851>3.0.CO;2-G ↗
3. Enhanced mechanical properties of orthorhombic Ti2AlNb-based intermetallic alloy10.1007/BF03027045 ↗
4. Microstructure, creep, and tensile behavior of a Ti-21Al-29Nb (at.%) orthorhombic + B2 alloy10.1016/j.intermet.2005.08.006 ↗
5. A new ordered orthorhombic phase in a Ti3Al-Nb alloy10.1016/0001-6160(88)90141-1 ↗
6. Investigation of the phase transformations in Ti22Al25Nb alloy10.1016/j.matchar.2016.02.011 ↗
7. High-temperature deformation behavior of the extruded Ti-22Al-25Nb alloy fabricated by powder metallurgy10.1016/j.matchar.2018.01.019 ↗
8. Effect of composition on the mechanical properties of newly developed Ti2AlNb-based titanium aluminide10.1016/j.intermet.2004.12.003 ↗
9. Microstructure and mechanical properties of orthorhombic alloys in the Ti-Al-Nb system10.1016/S0966-9795(98)00044-2 ↗
10. Displacive precursor phenomena in Ti-22Al-27Nb intermetallic compound prior to diffusional transformation
11. A review of electrically-assisted manufacturing10.1007/s40684-015-0045-4 ↗
12. Decoupling thermal and electrical effect in an electrically assisted uniaxial tensile test using finite element analysis10.1007/s11661-015-2879-3 ↗
13. Current assisted superplastic forming of titanium alloy bellows10.4028/www.scientific.net/MSF.838-839.135 ↗
14. Electric current-assisted deformation behavior of Al-Mg-Si alloy under uniaxial tension10.1016/j.ijplas.2016.09.010 ↗
15. Coarsening behavior of lamellar orthorhombic phase and its effect on tensile properties for the Ti-22Al-25Nb alloy10.1016/j.msea.2014.05.076 ↗
16. Instability of the O-phase in Ti-22Al-25Nb alloy during elevated-temperature deformation10.1016/j.jallcom.2013.05.018 ↗
17. Annealing response of the intermetallic alloy Ti-22Al-25Nb10.1016/j.intermet.2010.02.010 ↗
18. Microstructure evolution, B2 grain growth kinetics and fracture behaviour of a powder metallurgy Ti-22Al-25Nb alloy fabricated by spark plasma sintering10.1016/j.msea.2018.05.110 ↗
19. Dynamic recrystallization kinetics of a powder metallurgy Ti-22Al-25Nb alloy during hot compression10.1016/j.msea.2014.04.062 ↗
20. Phase transformation in the β phase of super α TiAl base alloys during static annealing and superplastic deformation at 700–1000 °C
21. Improved mechanical properties of Ti2AlNb-based intermetallic alloys and composites10.4028/www.scientific.net/AMR.59.105 ↗
22. Formability and microstructure of Ti22Al24.5Nb0.5Mo rolled sheet within hot gas bulging tests at constant equivalent strain rate10.1016/j.matdes.2016.06.109 ↗
23. The structural design and superplastic forming/diffusion bonding of Ti2AlNb based alloy for four-layer structure10.1016/j.matdes.2016.05.046 ↗
24. Stress-induced phase transformation during superplastic deformation in two-phase Ti-Al-Fe alloy
25. Part I. The microstructural evolution in Ti-Al-Nb O + Bcc orthorhombic alloys10.1007/s11661-999-0240-4 ↗
26. The evolution of recrystallization textures in body centred cubic metals
27. B2 grain growth and particle pinning effect of Ti-22Al-25Nb orthorhombic intermetallic alloy during heating process10.1016/j.intermet.2012.04.021 ↗
28. Application of high-density electropulsing to improve the performance of metallic materials: mechanisms, microstructure and properties10.3390/ma11020185 ↗
29. Microstructure evolution in metals induced by high density electric current pulses10.1179/1743284715Y.0000000001 ↗
30. The microstructure and property variations of metals induced by electric current treatment: a review10.1016/j.matchar.2018.08.058 ↗
31. Thermomechanical processing of alpha titanium alloys-an overview10.1016/S0921-5093(98)01155-1 ↗
32. Microstructure and mechanical properties of Ti2AlNb cup-shaped part prepared by hot gas forming: determining forming temperature, strain rate, and heat treatment10.1007/s00170-017-0501-0 ↗
33. Part 2: the creep behavior of Ti-Al-Nb O + bcc orthorhombic alloys10.1007/s11661-999-0244-0 ↗
34. B2 grain growth behavior of a Ti-22Al-25Nb alloy fabricated by hot pressing sintering10.1007/s11665-018-3353-3 ↗
35. Continuous cavity nucleation and creep fracture10.1016/0036-9748(83)90065-0 ↗