journal article·2019-07

The determining role of intercritical annealing condition on retained austenite and mechanical properties of a low carbon steel: Experimental and theoretical analysis

Z.J. Xie, G. Han, Y.S. Yu, C.J. Shang, R.D.K. Misra

Publisher page

Abstract

Abstract The impact of intercritical annealing (IA) temperature and time on retained austenite and mechanical properties are elucidated in a low carbon steel containing 2.85 wt% Mn. Experimental studies indicated that the multi-phase microstructure consisted of intercritical ferrite, martensite/bainite, retained austenite and fine dispersion of precipitations. The volume fraction of retained austenite attained a maximum value of 14% on IA at 680 °C for 30 min. The partition behavior of alloying elements during intercritical annealing was studied by scanning transmission electron microscopy (STEM) and analyzed kinetically by DICTRA simulation. Appropriate fraction of retained austenite obtained at 680 °C for 30 min was attributed to the extent of partitioning of carbon and manganese into the reverted austenite that contributed to best balance of mechanical properties.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. State-of-the-art and development trends of HSLA steels in China
2. The microstructure and properties of high performance steels with low yield-to-tensile ratio10.1016/j.jallcom.2012.05.129 ↗
3. Strain hardening behavior and stress ratio of high deformability pipeline steel with ferrite/bainite multi-phase microstructure
4. Micromechanical behavior and failure mechanism of F/B multi-phase high performance steel10.1016/S1006-706X(16)30077-2 ↗
5. Stability of retained austenite in multi-phase microstructure during austempering and its effect on the ductility of a low carbon steel10.1016/j.msea.2014.02.059 ↗
6. Effect of annealing temperature and time on microstructure evolution of 0.2C–5Mn steel during intercritical annealing process10.1179/1743284713Y.0000000416 ↗
7. Low-carbon manganese TRIP steels10.4028/www.scientific.net/MSF.539-543.4327 ↗
8. Enhanced work-hardening behavior and mechanical properties in ultrafine-grained steels with large-fractioned metastable austenite10.1016/j.scriptamat.2010.06.023 ↗
9. Ultrafine-grained microstructures and mechanical properties of alloy steels10.1007/BF02647665 ↗
10. Heat treatment effects on the microstructure and mechanical properties of a medium manganese steel (0.2C–5Mn)10.1016/j.msea.2011.11.009 ↗
11. High strength and ductility combination in nano-/ultrafine-grained medium-Mn steel by tuningthe stability of reverted austenite involving intercritical annealing10.1007/s10853-018-03291-w ↗
12. Development of ultrafine lamellar ferrite and austenite duplex structure in 0.2 C5Mn steel during ART-annealing10.2355/isijinternational.51.651 ↗
13. Austenite stability effects on tensile behavior of manganese-enriched-austenite transformation-induced plasticity steel10.1007/s11661-011-0687-y ↗
14. Austenite stabilization through manganese enrichment10.1016/j.scriptamat.2010.09.040 ↗
15. Grain boundary segregation engineering and austenite reversion turn embrittlement into toughness: example of a 9 wt.% medium Mn steel10.1016/j.actamat.2014.12.021 ↗
16. A study of grain boundary embrittlement in an Fe–8% Mn alloy10.1016/S0921-5093(99)00734-0 ↗
17. Characterization of microstructure obtained by quenching and partitioning process in low alloy martensitic steel10.1016/j.msea.2010.02.020 ↗
18. Thermo-Calc and DICTRA, computational tools for materials science10.1016/S0364-5916(02)00037-8 ↗
19. Stabilization of retained austenite by the two-step intercritical heat treatment and its effect on the toughness of a low alloyed steel10.1016/j.matdes.2014.02.035 ↗
20. Study of retained austenite and nano-scale precipitation and their effects on properties of a low alloyed multi-phase steel by the two-step intercritical treatment10.1016/j.matchar.2016.01.009 ↗
21. A novel multi-step intercritical heat treatment induces multi-phase microstructure with ultra-low yield ratio and high ductility in advanced high-strength steel10.1016/j.scriptamat.2018.06.042 ↗
22. Thermal stability of retained austenite and properties of a multi-phase low alloy steel10.3390/met8100807 ↗
23. On the sources of work hardening in multiphase steels assisted by transformation-induced plasticity10.1080/01418610108216637 ↗
24. Design method for TRIP-aided multiphase steel based on a microstructure-based modelling for transformation-induced plasticity and mechanically induced martensitic transformation10.1016/j.msea.2008.09.026 ↗
25. Effect of heat treatment on microstructure and mechanical properties of cold rolled C–Mn–Si TRIP-aided steel10.1016/j.matchar.2006.01.010 ↗
26. Recent process in medium-Mn steels made with new designing strategies, a review10.1016/j.jmst.2017.06.017 ↗
27. Growth of austenite from as-quenched martensite during intercritical annealing in an Fe–0.1C–3Mn–1.5Si alloy10.1016/j.actamat.2012.10.019 ↗
28. Experimental and numerical analysis on formation of stable austenite during the intercritical annealing of 5Mn steel10.1016/j.actamat.2011.03.025 ↗