journal article·2020-12

Effect of Fe content on low cycle fatigue behavior of squeeze cast Al-Zn-Mg-Cu alloys

Ke Hu, Chihao Lin, Songchao Xia, Chengkun Zheng, Bo Lin

Publisher page

Abstract

Abstract Results of different researches prove that Fe content plays a major role on the obtained mechanical properties of the aluminum alloys. Due to the importance of fatigue properties for the application of Al-Zn-Mg-Cu alloys in aviation industry and lack of study on the topic, this research was focused on the effect of Fe content on the low cycle fatigue behavior of these alloys processed by squeeze casting. The experimental alloys processed with different Fe contents of 0.01, 0.33 and 0.55 wt% exhibited similar cyclic behaviorsWhile cyclic hardening, owing to the dislocation multiplication, entanglement, accumulation, interaction with the second phases, and stress induced precipitation, was understood as the ruling mechanism at higher strain amplitudes (0.4%–0.6%), all the studied alloys showed cyclic stabilization at strain amplitudes below 0.4%. The fatigue life of the alloy with 0.33 wt% Fe (B alloy) was better than that of the alloy with 0.55 wt% Fe (C alloy) at all specific strain amplitudes. For the specific strain amplitudes of below 0.5%, the fatigue life of B alloy was much superior to that of the alloy with 0.01 wt% Fe (A alloy). On the other hand, due to the difference existing between the fatigue fracture mechanisms occurred under high strain amplitudes and low strain amplitudes, the fatigue life of A alloy was a little longer than that of B alloy at strain amplitude of 0.6%. It was understood that Fe-rich phases had a great potential to alter the crack propagation path at low strain amplitudes. The crack propagation rate accelerated under conditions that the cyclic stress was large enough to break Fe-rich phases at high strain amplitudes of 0.6%.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (24)

Show source-provided references
1. Effect of solution-treating temperature on the intergranular corrosion of a peak-aged Al-Zn-Mg-Cu alloy10.1016/j.jmrt.2020.04.035 ↗
2. Microstructures and tensile properties of a selective laser melted Al–Zn–Mg–Cu(Al7075) alloy by Si and Zr microalloying10.1016/j.msea.2020.139492 ↗
3. Microstructural evolution of Fe-rich particles in an Al–Zn–Mg–Cu alloy during equal-channel angular pressing10.1016/j.msea.2010.04.041 ↗
4. Solidification of aluminum-copper B206 alloys with iron and silicon additions10.1007/s11661-010-0293-4 ↗
5. Localized corrosion behavior associated with Al7Cu2Fe intermetallic in Al-Zn-Mg-Cu-Zr alloy10.1016/j.jallcom.2018.12.151 ↗
6. Influence of iron addition on the microstructure and the electrochemical corrosion of Al-Zn-Mg alloys10.1023/A:1017566002951 ↗
7. Evolution of voids during ductile crack propagation in an aluminium alloy sheet toughness test studied by synchrotron radiation computed tomography10.1016/j.actamat.2007.12.019 ↗
8. Influence of notch radius and microstructure on the fracture behavior of Al-Zn-Mg-Cu alloys of different purity10.1016/j.matdes.2009.11.018 ↗
9. Effect of iron content on fracture toughness and cracking processes in high strength Al-Zn-Mg-Cu alloy10.1016/0025-5416(86)90075-3 ↗
10. Effect of Fe-content on fatigue crack initiation and propagation in a cast aluminum-silicon alloy (A356-T6)10.1016/S0921-5093(04)00964-5 ↗
11. Effect of Fe content and microstructural features on the tensile and fatigue properties of the Al-Si10-Cu2 alloy10.1016/j.matdes.2011.11.047 ↗
12. Microstructure, tensile and fatigue properties of the Al-10% Si-2% Cu alloy with different Fe and Mn content cast under controlled conditions10.1016/j.jmatprotec.2009.05.030 ↗
13. Fatigue behavior of A356 T6 aluminum cast alloys. Part I. effect of casting defects10.1016/S1471-5317(00)00008-0 ↗
14. Fatigue behavior of A356/357 aluminum cast alloys. Part II. effect of microstructural constituents10.1016/S1471-5317(00)00009-2 ↗
15. Low cycle fatigue behavior of T4-treated Al–Zn–Mg–Cu alloys prepared by squeeze casting and gravity die casting10.1016/S1003-6326(15)63992-9 ↗
16. The effect of iron content on the iron-containing intermetallic phases in a cast 6060 aluminum alloy10.1007/s11661-010-0595-6 ↗
17. Microstructures and mechanical properties of heat-treated Al-5.0 Cu-0.5 Fe squeeze cast alloys with different Mn/Fe ratio10.1016/j.msea.2013.09.043 ↗
18. On the nature of the Fe-bearing particles influencing hard anodizing behavior of AA 7075 extrusion products10.1007/s11661-998-1007-z ↗
19. Solid-state transformation of Fe-rich intermetallic phases in Al–5.0Cu–0.6Mn squeeze cast alloy with variable Fe contents during solution heat treatment10.1016/j.matchar.2015.03.035 ↗
20. Tensile properties of Al-Cu 206 cast alloys with various iron contents10.1007/s11661-014-2207-3 ↗
21. Effects of Fe content on microstructure and mechanical properties of A206 alloy10.2320/matertrans1989.41.708 ↗
22. Chen · 2012
23. Characterization of AA6061 alloy processed by equal channel angular pressing and subjected to low cycle fatigue10.1007/s12666-012-0236-4 ↗
24. Dieter · 1986