Abstract

In order to study the effect of magnetic field on the spraying process, a thermal spraying technique of ferromagnetic metal powder assisted by pulsed magnetic field is presented. The Ni60 coating with different Fe content was prepared by pulsed magnetic field assisted supersonic plasma spraying. This process can improve the microstructure, porosity, mechanical properties and tribological properties of the coating. In this paper, a diagram depicting the mechanism for coating formation by pulsed magnetic field assisted spraying was prepared according to the test results for the coatings. We found that the pulsed magnetic field formed at the edge of the poles, and, compared with the Ni base material, the Fe phase material was easily attracted by the magnetic poles, which accelerated its downward movement. During this downward movement, a mixing effect developed within the coating that decreased the coating porosity, made the Cr strengthening phase more uniform, and, as the matrix provided many nucleation sites, further promoted the production of amorphous nanocrystalline phases. Finally, the service performance of the coatings was continuously improved. This process provides a new approach to the design and development of advanced coatings, and it shows great promise for applications in next-generation ferromagnetic metal-based coatings.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · High-Temperature Coating Behaviors · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Grain refinement effect of pulsed magnetic field on solidified microstructure of superalloy IN718[J]10.1557/jmr.2009.0382 ↗
2. Microstructure and mechanical properties of Mg-Al-Zn alloy under a low-voltage pulsed magnetic field[J]10.1016/j.matlet.2011.09.021 ↗
3. Fabrication of textured Ti3SiC2 ceramic by slip casting in a strong magnetic field and pressureless sintering[J]10.2109/jcersj2.122.817 ↗
4. Revealing the mechanisms for the nucleation and formation of equiaxed grains in commercial purity aluminum by fluid-solid coupling induced by a pulsed magnetic field - ScienceDirect[J]
5. Effect of Al2O3 addition on texturing in a rotating strong magnetic field and densification of B4C[J]10.1016/j.ceramint.2019.06.032 ↗
6. Influence of an axial magnetic field on microstructures and alignment in directionally solidified Ni-based superalloy[J]10.2355/isijinternational.ISIJINT-2016-352 ↗
7. Effects of pulsed magnetic field on microsegregation of solute elements in a Ni-based single crystal superalloy[J]10.1016/j.jmst.2015.12.021 ↗
8. Improvement in uniformity of alloy steel by pulsed magnetic field treatment[J]
9. Ultrafast actuation of Ni-Mn-Ga micropillars by pulsed magnetic field[J]10.1016/j.scriptamat.2018.12.009 ↗
10. Effects of high temperature treatment on microstructure and mechanical properties of laser-clad NiCrBSi/WC coatings on titanium alloy substrate[J]10.1016/j.matchar.2014.10.003 ↗
11. Microstructure, interface characteristics and tribological properties of laser cladded NiCrBSi-WC coatings on PH 13-8 Mo steel[J]10.1016/j.triboint.2021.106873 ↗
12. High temperature phase stability and wear behavior of laser clad Ta reinforced NiCrBSi coating[J]10.1016/j.apsusc.2021.149171 ↗
13. Wetting and interfacial behaviour in the TiB2-NiCrBSiC system[J]10.1016/j.jallcom.2018.11.102 ↗
14. Allowing and post-heat treatment of thermal sprayed coatings of self-fluxing Al-loys [J]
15. APS prepared NiCrBSi-YSZ composite coatings for protection against cavitation erosion[J]10.1016/j.jallcom.2017.01.034 ↗
16. Effect of heated laser cladding Ni Cr BSi coated strengthened by tantalum [J]
17. Effects of a high-voltage pulsed magnetic field on the solidification structures of biodegradable Zn-Ag alloys[J]10.1016/j.matchar.2020.110274 ↗
18. Suppression effect of a steady magnetic field on molten pool during laser remelting[J]
19. Influence on the microstructure of laser cladding NiCrBSi coatings with electromagnetic compound field [J]10.4028/www.scientific.net/SSP.295.15 ↗
20. Effect of pulsed magnetic field treatment on the residual stress of 20Cr2Ni4A steel[J]10.1016/j.jmmm.2018.12.105 ↗
21. Tribological behavior of plasma sprayed carbon nanotubes reinforced TiO 2 coatings[J]
22. Microstructures and tribological properties of Fe-based amorphous metallic coatings deposited via supersonic plasma spraying[J]10.1007/s11666-017-0582-1 ↗
23. Microstructures and wear resistance of Al-25 wt.%Si coatings prepared by high-efficiency supersonic plasma spraying[J]10.1007/s11666-019-00898-6 ↗
24. Investigation of sprayed particle filling qualities within the texture on the bonding behavior of Ni-based coating[J]
25. Effects of electromagnetic compound field on the escape behavior of pores in molten pool during laser cladding[J]
26. How does substrate roughness affect the service life of a superhydrophobic coating? [J]10.1016/j.apsusc.2018.01.232 ↗
27. Residual stress and thermo-mechanical properties of cold spray metal coatings[J]10.1016/j.actamat.2010.10.058 ↗
28. Effects of Marangoni convection on the embedding dynamic behavior of SiC nano-particles into the Al molten pool during laser micro-melting[J]10.1016/j.matdes.2018.02.010 ↗
29. Microstructure and nanoindentation measurement of residual stress in Fe-based coating by laser cladding[J]10.1007/s10853-011-6012-8 ↗
30. Residual stress distribution in thermally sprayed self-fluxing alloy coatings[J]
31. The relationship between residual stress and process parameters in TiN coatings on copper alloy substrates.[J]10.1016/S1044-5803(02)00256-5 ↗
32. Effect of ceramic coating thickness on residual stress and fatigue characteristic of 1Cr-1Mo-0.25V steel[J]10.1142/S0217979202009627 ↗
33. Research on the promotion mechanism of surface burnishing process by two-dimensional ultrasonic vibration[J]10.1016/j.jmrt.2021.05.038 ↗