Effect of TiB2 on the microstructure and mechanical properties of TiAl alloy produced by laser direct energy deposition
Source abstract
Abstract
A Ti-48Al-2Cr-2Nb alloy was prepared by laser directed energy deposition (DED). The microstructure of the DED-produced Ti-48Al-2Cr-2Nb alloy exhibited a coarse columnar structure along the building direction. Through a combination of experiment and numerical simulation, the temperature gradient and solidification rate of the single-track sample were calculated theoretically. The columnar to equiaxed transition (CET) behavior of molten pool solidification was quantitatively analyzed, and the microstructure transition diagram was established. The effect of TiB 2 on the microstructure and mechanical properties of the TiAl alloy was investigated. The columnar changed to equiaxed grains in the vertical cross section by adding nanometer-sized TiB 2 particles and the microstructure was significantly refined. The grain size was reduced from 48.5 μm to 4.9 μm. Some equiaxed γ grains were distributed around the banded TiB 2. The compressive properties were improved from 628.4 MPa to 698.8 MPa by adding nanometer-sized TiB 2 particles. Finally, the solidification behavior and the microstructure refinement mechanism caused by the addition of TiB 2 particles were discussed.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · Additive Manufacturing Materials and Processes · Surface Treatment and Coatings
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Gamma titanium aluminide alloys—an assessment within the competition of aerospace structural materials10.1016/S0921-5093(98)01158-7 ↗
2. Novel design concepts for gamma-base titanium aluminide alloys10.1016/S0966-9795(00)00036-4 ↗
3. Polysynthetic twinned TiAl single crystals for high-temperature applications10.1038/nmat4677 ↗
4. Additive manufacturing of gamma titanium aluminide alloys: a review10.1007/s10853-022-06896-4 ↗
5. Development of gamma titanium aluminide (γ-TiAl) alloys: a review10.1016/j.jallcom.2022.167262 ↗
6. Microstructure and high-temperature tensile property of TiAl alloy produced by selective electron beam melting10.1007/s12598-020-01683-z ↗
7. Microstructure and mechanical properties of Y2O3-bearing Ti–48Al–2Cr–2Nb alloy prepared by selective electron beam melting10.1016/j.msea.2022.142960 ↗
8. Study on microstructure and tribological properties of nano/micron TiC/TC4 composites fabricated by laser melting deposition10.1016/j.jmapro.2022.07.068 ↗
9. Titanium aluminides processing by additive manufacturing - a review10.1007/s00170-022-08728-w ↗
10. Microstructure and mechanical properties of laser melting deposited γ-TiAl intermetallic alloys10.1016/j.msea.2007.02.073 ↗
11. Enhanced tensile properties and wear resistance of additively manufactured CoCrFeMnNi high-entropy alloy at cryogenic temperature10.1007/s12598-021-01867-1 ↗
12. Variations of microstructure and tensile property of γ-TiAl alloys with 0–0.5 at% C additives10.1016/j.msea.2017.06.019 ↗
13. Additive manufacturing of micro/nano multiphase synergistically reinforced Ti-55Al-7.5Nb with a reticular boundary precipitate via direct laser deposition
14. Microstructure and compression behavior of in-situ synthesized Ti2AlC reinforced Ti-48Al-2Cr alloy with carbon nanotubes addition10.1016/j.jallcom.2021.158646 ↗
15. Microstructure characterization, mechanical properties and toughening mechanism of TiB2-containing conventional cast TiAl-based alloy10.1016/j.msea.2015.07.092 ↗
16. TiAl/B4C composite fabricated by high energy ball milling and hot press sintering processes and its mechanical properties10.1016/j.msea.2010.08.041 ↗
17. Influence of nano-Y2O3 addition on microstructure and tensile properties of high-Al TiAl alloys10.1016/j.msea.2020.139803 ↗
18. The significant impact of grain refiner on γ -TiAl intermetallic fabricated by laser-based additive manufacturing
19. Mechanical, tribological and electrochemical corrosion properties of in-situ synthesized Al2O3/TiAl composites10.1016/j.intermet.2020.106758 ↗
20. Simultaneously enhanced tensile strength and ductility of nano-Y2O+reinforced TiAl alloy prepared by directed energy deposition10.1016/j.matchar.2023.113472 ↗
21. The effects of the formation of a multi-scale reinforcing phase on the microstructure evolution and mechanical properties of a Ti2AlC/TiAl alloy10.1039/D1NR02435C ↗
22. Carbon nanotube and in-situ titanium carbide reinforced titanium diboride matrix composites synthesized by reactive spark plasma sintering10.1016/j.msea.2016.03.098 ↗
23. Enhanced nanohardness and new insights into texture evolution and phase transformation of TiAl/TiB2 in-situ metal matrix composites prepared via selective laser melting10.1016/j.actamat.2017.07.003 ↗
24. Grain refinement of TiAl-based alloys: the role of TiB2 crystallography and growth10.1016/j.actamat.2010.08.040 ↗
25. Microstructural characteristics of Ti-45A1-8.5Nb/TiB2 composites by powder metallurgy
26. Phase transformations in XDTM TiB2-reinforced near-γ Ti48Al2Nb2Mn10.1016/0921-5093(94)90902-4 ↗
27. Wunderlich, surface tension and viscosity of industrial Ti-alloys measured by the oscillating drop method on board parabolic flights
28. Temperature analysis of the powder streams in coaxial laser cladding10.1016/S0030-3992(99)00115-2 ↗
29. Numerical modelling of heat transfer, mass transport and microstructure formation in a high deposition rate laser directed energy deposition process
30. The Al–B–Nb–Ti system: III. Thermodynamic re-evaluation of the constituent binary system Al–Ti10.1016/j.jallcom.2007.10.061 ↗
31. Columnar to equiaxed transition in additively manufactured CoCrFeMnNi high entropy alloy10.1016/j.matdes.2020.109262 ↗
32. Modelling of microstructure formation in solidification processes10.1179/imr.1989.34.1.93 ↗
33. Hot working behavior and processing map of a γ-TiAl alloy synthesized by powder metallurgy10.1016/j.matdes.2011.06.003 ↗
34. High temperature micromechanical behavior of Ti2AlN particle reinforced TiAl based composites investigated by insitu high-energy X-ray diffraction10.1016/j.matdes.2021.110225 ↗
35. Achieving superior high-temperature strength and oxidation resistance of TiAl nanocomposite through in situ semicoherent MAX phase precipitation10.1021/acsami.1c21719 ↗
36. A numerical and experimental investigation of convective heat transfer during laser-powder bed fusion
37. Epitaxial laser metal forming: analysis of microstructure formation10.1016/S0921-5093(99)00202-6 ↗
38. Parental time devoted to children in two- and one-wage-earner families10.1016/0272-7757(84)90010-4 ↗
39. Promoting the columnar to equiaxed transition and grain refinement of titanium alloys during additive manufacturing10.1016/j.actamat.2019.02.020 ↗
40. Single-crystal laser deposition of superalloys: processing–microstructure maps10.1016/S1359-6454(00)00367-0 ↗
41. Formation of fully equiaxed grain microstructure in additively manufactured AlCoCrFeNiTi0.5 high entropy alloy10.1016/j.matdes.2019.108202 ↗
42. The Al–B–Nb–Ti system10.1016/j.jallcom.2008.06.128 ↗
43. Boron solubility and boride compositions in α2 + γ titanium aluminides10.1016/S0966-9795(97)00016-2 ↗
44. Evolution of boride morphologies in TiAl-B alloys10.1007/BF02667377 ↗
45. Role of boron in TiAl alloy development: a review10.1007/s12598-015-0615-1 ↗
46. As-cast structure refinement of Ti-46Al alloy by hafnium and boron additions