journal article·2020-12

Characterization of the interpass microstructure in low alloy steel/Alloy 625 HW-GTAW narrow groove welds

Ryan Buntain, Boian Alexandrov, Gopal Viswanathan

Publisher page

Abstract

Abstract A dissimilar weld between a low alloy steel (LAS) butter weld joined to a F65 steel pipe using a narrow groove hot wire gas tungsten arc welding (HW-GTAW) procedure with Alloy 625 filler metal was investigated. The weld interpass microstructure is comprised of large swirls formed by a macrosegregation mechanism involving partial, non-uniform mixing of liquid base metal with the lower melting temperature weld pool, followed by fast solidification. This mechanism produces steep gradients in composition and solidification behavior. The resulting swirls are composed of alternating iron-rich peninsulas and partially mixed zones (PMXZ) that are surrounded by planar and cellular zones exhibiting multiple solidification directions. Large austenitic grains, encompassing planar, cellular, and dendritic morphologies, nucleate off peninsulas in direct contact with the weld pool. The highest hardness was found in nickel and chromium rich PMXZs that exhibited a lath martensite microstructure. In the event of exposure to hydrogen containing environments, the PMXZs could serve as nucleation sites for hydrogen assisted cracking.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. Burk · 2010
2. Recent experiences with cracking of load bearing dissimilar metal welds on subsea production systems
3. Failure of an AISI 8630-Mod low alloy steel to C-Mn steel dissimilar metal weld made using nickel alloy UNS N06625 welding consumables
4. Experience with qualification and use of stainless steels in subsea pipelines
5. Dodge · 2014
6. Microstructure and hydrogen-induced failure mechanisms in Fe and Ni alloy weldments10.1007/s11661-012-1129-1 ↗
7. Fusion boundary microstructure evolution associated with embrittlement of Ni – base alloy overlays applied to carbon steel10.1007/s40194-012-0007-1 ↗
8. Dodge · 2012 · 1
9. Resistance of dissimilar joints between steel and nickel alloys to hydrogen-assisted cracking
10. Hydrogen embrittlement of 8630M / 625 subsea dissimilar joints: Factors that influence the performance
11. Subsea dissimilar joints: failure mechanisms and opportunities for mitigation
12. Fenske · 2010
13. Effect of post-weld heat treatment on fusion boundary microstructure in dissimilar metal welds for subsea service10.3139/120.111039 ↗
14. A new test for evaluation of susceptibility to hydrogen assisted cracking in dissimilar metal welds
15. The effect of postweld heat treatment on hydrogen-assisted cracking of 8630/Alloy 625 overlay10.1007/s40194-018-0578-6 ↗
16. The effect of PWHT on the material properties and micro structure in Inconel 625 and Inconel 725 buttered joints
17. Characterization of the Interface of an Alloy 625 overlay on steels using Nanoindentation10.1007/s11665-018-3444-1 ↗
18. Tempering effect on the fusion boundary region of alloy 625 weld overlay on 8630 steel10.1007/s40194-018-0560-3 ↗
19. Fusion zone micostructure associated with embrittlement of subsea dissimilar joints
20. Fusion boundary macrosegregation in dissimilar-filler welds
21. Assessing the integrity of subsea dissimilar joints to ensure safe operations
22. A study of weld Interface phenomena in a low alloy steel
23. Application of orientation imaging microscopy to study phase transformations in steels10.1016/S1044-5803(01)00140-1 ↗
24. Characterization of dual-phase steel microstructure by combined submicrometer EBSD and EPMA carbon measurements10.1017/S1431927613001554 ↗
25. New method of characterizing and quantifying complex microstructures in steels10.1080/10426910903143415 ↗