Effect of lamellar α on the stress corrosion cracking of Ti-6Al-4 V alloy in simulated oilfield brine

Guangfang Chi, Bo Jiang, Danqing Yi, Lingyun Yang, Suping Pan, Huiqun Liu, Chun Feng, Weiguo Mao

Publisher page

Abstract

Abstract The stress corrosion cracking (SCC) behavior of Ti-6Al-4 V alloy with different lamellar α microstructures in simulated oilfield brine was investigated in this study. The SCC susceptibility of the Widmanstatten sample was 11.0%, lower than that of the bimodal and trimodal samples (19.9%, and 18.0%, respectively). In the Widmanstatten sample, the crack growth path transitioned from a zigzag to a linear path when the crack moved from one colony to another because of the sliding variations in the slip bands with different orientations. The decrease in a SCC resistance of bimodal and trimodal samples resulted from the decrease in α/β colony size. Owing to the larger thickness and different orientation of lamellar α, the trimodal sample exhibited a slightly higher SCC resistance and more circuitous crack propagation than that in the bimodal sample. The deflection angle of the crack increased with an increase in the angle between the slip system, and the favorable slip system was prismatic in three samples. It can be concluded that one of the strategies to improve the SCC and crack growth resistance of Ti-6Al-4 V alloy in oil field applications is to tailor the lamellar α microstructure with different orientations and larger α colonies.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Titanium Alloys Microstructure and Properties · Hydrogen embrittlement and corrosion behaviors in metals · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. Effects of degree of deformation on the microstructure, mechanical properties and texture of hybrid-reinforced titanium matrix composites10.1016/j.actamat.2012.01.032 ↗
2. Mechanical properties of Ti-6Al-4V/TiB composites with randomly oriented and aligned TiB reinforcements10.1016/S1359-6454(02)00510-4 ↗
3. Perspectives on titanium science and technology10.1016/j.actamat.2012.10.043 ↗
4. Micromechanics of Ti–10V–2Fe–3Al: in situ synchrotron characterisation and modelling10.1016/j.actamat.2007.08.049 ↗
5. Deformation mode dependent mechanism and kinetics of dynamic recrystallization in hot working of titanium alloy10.1016/j.msea.2019.138804 ↗
6. Grafting of the peppermint essential oil to a chemically treated Ti6Al4V alloy to counteract the bacterial adhesion10.1016/j.surfcoat.2019.125011 ↗
7. Evolution of equiaxed and lamellar α during hot compression in a near alpha titanium alloy with bimodal microstructure10.1016/j.matchar.2019.03.005 ↗
8. Hot salt stress corrosion resistance of Ti 6246 alloy10.1016/S0010-938X(98)00028-6 ↗
9. The stress-corrosion cracking susceptibility of near-α titanium alloy IMI 834 in presence of hot salt10.1016/j.corsci.2014.01.013 ↗
10. Stress corrosion cracking of sensitized type 316 austenitic stainless steel in hydrochloric acid solution–effect of sensitizing time10.1016/S0010-938X(03)00002-7 ↗
11. The stress corrosion cracking performance of pure zirconium and zirconium alloys in highly oxidizing nitric acid10.1016/0010-938X(95)00166-H ↗
12. The generation of corrosion under insulation and stress corrosion cracking due to sulphide stress cracking in an austenitic stainless steel hydrocarbon gas pipeline10.1016/j.engfailanal.2014.05.004 ↗
13. Corrosion behavior of Ti–8Al–1Mo–1V alloy compared to Ti–6Al–4V10.1016/j.matdes.2010.09.009 ↗
14. Corrosion and passivity of Ti-13% Nb-13% Zr in comparison to other biomedical implant alloys10.5006/1.3290281 ↗
15. Electrochemical stability of anodic titanium oxide films grown at potentials higher than 3V in a simulated physiological solution10.1016/j.corsci.2006.08.010 ↗
16. Gerhard · 1994
17. The role of hydrogen in the stress corrosion cracking of titanium alloys10.1016/0010-938X(74)90005-5 ↗
18. Metallurgical aspects of the stress corrosion cracking of titanium alloys
19. Effects of microtexture and Ti3Al (α2) precipitates on stress-corrosion cracking properties of a Ti-8Al-1Mo-1V alloy10.1016/j.corsci.2016.12.012 ↗
20. 10 - Stress corrosion cracking (SCC) and hydrogen-assisted cracking in titanium alloys
21. Stress corrosion cracking facet crystallography of Ti–8Al–1Mo–1V10.1016/j.corsci.2010.05.046 ↗
22. 2.09 - Stress Corrosion Cracking
23. A primary study of the effect of hydrostatic pressure on stress corrosion cracking of Ti-6Al-4V alloy in 3.5% NaCl solution10.1016/j.corsci.2019.108402 ↗
24. The mechanisms of hot salt stress corrosion cracking in titanium alloy Ti-6Al-2Sn-4Zr-6Mo10.1016/j.corsci.2018.02.025 ↗
25. Effect of long term exposure and hydrogen effects on HSSCC behaviour of titanium alloy IMI 83410.1016/j.matdes.2015.08.002 ↗
26. Static coarsening behaviour of lamellar microstructure in selective laser melted Ti–6Al–4V10.1016/j.jmst.2019.04.008 ↗
27. Twinning and sequential kinking in lamellar Ti-6Al-4V alloy10.1016/j.actamat.2019.10.010 ↗
28. Flow stress constitutive relationship between lamellar and equiaxed microstructure during hot deformation of Ti-6Al-4V10.1016/j.jmatprotec.2019.02.030 ↗
29. Effects of solution temperature and cooling rate on microstructure and micro-hardness of a hot compressed Ti-6Al-4V alloy10.1016/j.vacuum.2018.10.035 ↗
30. Mechanical properties of fully martensite microstructure in Ti-6Al-4V alloy transformed from refined beta grains obtained by rapid heat treatment (RHT)10.1016/j.scriptamat.2017.05.038 ↗
31. The relationship between crystallographic texture and salt water cracking susceptibility in Ti–6Al–4V10.1016/0921-5093(95)09820-8 ↗
32. The nucleation and growth of corrosion pits on stainless steel10.1016/0010-938X(93)90133-2 ↗
33. Fracture toughness of a lamellar orientation-controlled TiAl-based alloy processed by either one-step or two-step compression at high temperature10.1016/j.msea.2018.02.079 ↗
34. Al-based metal matrix composites reinforced with Al–Cu–Fe quasicrystalline particles: strengthening by interfacial reaction10.1016/j.jallcom.2014.04.086 ↗
35. Development of a trimodal microstructure with superior combined strength, ductility and creep-rupture properties in a near alpha titanium alloy10.1016/j.msea.2017.04.068 ↗
36. High strength Ti–Fe–Sn ultrafine composites with large plasticity10.1016/j.scriptamat.2007.03.031 ↗
37. Comparative analyses of the tensile and damage tolerance properties of tri-modal microstructure to widmanstätten and bimodal microstructures of TA15 titanium alloy10.1016/j.jallcom.2019.02.300 ↗
38. Motyka · 2012
39. Dependence of mechanical properties on the microstructural parameters of TA15 titanium alloy with tri-modal microstructure10.1016/j.msea.2018.10.030 ↗
40. Influence of processing on microstructure and mechanical properties of (α+β) titanium alloys10.1016/S0921-5093(97)00778-8 ↗
41. Understanding the “blue spot”: sodium chloride hot salt stress-corrosion cracking in titanium-6246 during fatigue testing at low pressure10.1016/j.engfailanal.2015.06.008 ↗
42. Stress corrosion cracking of Al-Zn-Mg alloy AA-7039 by slow strain-rate method10.1007/BF00563047 ↗
43. Mechanical properties, corrosion behavior and microstructures of a non-isothermal ageing treated Al-Zn-Mg-Cu alloy10.1016/j.msea.2017.01.086 ↗
44. The role of slip transfer at grain boundaries in the propagation of microstructurally short fatigue cracks in Ni-based superalloys10.1016/j.scriptamat.2018.11.008 ↗
45. Fatigue crack growth mechanisms in Ti6242 lamellar microstructures: influence of loading frequency and temperature10.1007/s11661-003-0016-1 ↗
46. An investigation of the effects of colony microstructure on fatigue crack growth in Ti–6Al–4V10.1016/S0921-5093(01)01014-0 ↗
47. Comparative study of crack growth behaviors of fully-lamellar and bi-lamellar Ti-6Al-3Nb-2Zr-1Mo alloy10.1016/j.jallcom.2019.02.302 ↗
48. Microstructure and fatigue crack growth mechanisms in high temperature titanium alloys10.1016/j.ijfatigue.2010.02.001 ↗
49. Anisotropy in the room-temperature deformation of α-β colonies in titanium alloys: role of the α-β interface10.1080/1478643032000158305 ↗
50. Room temperature deformation and mechanisms of slip transmission in oriented single-colony crystals of an α/β titanium alloy10.1016/S1359-6454(98)00364-4 ↗
51. Slip transfer and deformation structures resulting from the low cycle fatigue of near-alpha titanium alloy Ti-6242Si10.1016/j.ijplas.2017.09.012 ↗