Microstructure and corrosion behavior of linear friction welded TA15 and TC17 dissimilar joint
Source abstract
Abstract
TA15 and TC17 titanium alloys were joined by linear friction welding (LFW) method. The microstructure investigation indicated that the TC17 side welding zone (WZ) was composed of coarse β phases, α phase at grain boundaries and martensite α’ phase at the grain interior, while the TA15 side WZ consisted of abundant acicular martensite α’ phases and few retained β phases. Electrochemical test result indicated that TA15 base metal (BM) has better corrosion resistance than the TC17 BM. Numerous corrosion pits were formed on the TC17 BM and TC17 side WZ after immersion and salt spray tests. The worse corrosion resistance of the TC17 BM could be attributed to its high content α/β phase boundaries.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Welding Techniques Analysis · Titanium Alloys Microstructure and Properties · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. The role of microtexture on the faceted fracture morphology in Ti-6Al-4V subjected to high-cycle fatigue10.1016/j.actamat.2010.03.036 ↗
2. Evolution of microstructure, texture and mechanical properties of special friction stir welded T-joints for an α titanium alloy10.1016/j.matchar.2021.111152 ↗
3. Perspective on titanium science and technology10.1016/j.actamat.2012.10.043 ↗
4. Microstructure characterization and mechanical properties of linear friction welded Ti-6Al-4V alloy10.1002/adem.200700034 ↗
5. Microstructure and mechanical properties of a high nitrogen titanium alloy10.1016/j.msea.2007.08.074 ↗
6. Through analysis of the microstructure changes during linear friction welding of the near-α titanium alloy Ti-6Al-2Sn-4Zr-2Mo(Ti6242) towards microstructure optimization10.1016/j.matchar.2019.02.027 ↗
7. On the mechanism of porosity formation during welding of titanium alloys10.1016/j.actamat.2012.02.035 ↗
8. Linear friction welding of Ti-6Al-4V alloy fabricated below β-phase transformation temperature10.1016/j.scriptamat.2020.09.013 ↗
9. Linear and rotary friction welding review10.1080/09506608.2015.1109214 ↗
10. High frequency linear friction welding of a titanium alloy10.1016/S0043-1648(98)00145-8 ↗
11. On the extrusion stage of linear friction welding of Ti-6Al-4V10.1016/S0921-5093(99)00449-9 ↗
12. Dissimilar linear friction welding of selective laser melted Inconel 718 to forged Ni-based superalloy AD730TM: evolution of strengthening phases10.1016/j.jmst.2021.03.086 ↗
13. On the microstructure and property differences in a linear friction welded near-alpha titanium alloy joint10.1016/j.jmapro.2018.10.017 ↗
14. Effect of welding parameters on the microstructure and mechanical properties of linear friction welded Ti-6.5Al-3.5Mo-1.5Zr-0.3Si titanium alloy joint10.1016/j.jmapro.2019.08.031 ↗
15. Strain hardening behavior of linear friction welded joints between TC11 and TC17 dissimilar titanium alloys10.1016/j.msea.2014.10.044 ↗
16. Interfacial characteristics and cohesion mechanisms of linear friction welded dissimilar titanium alloys: Ti-5Al-2Sn-2Zr-4Mo-4Cr (Ti17) and Ti-6Al-2Sn-4Zr-2Mo (Ti6242)10.1016/j.matchar.2019.109942 ↗
17. Multi-length scale characterization of microstructure evolution and its consequence on mechanical properties in dissimilar friction stir welding of titanium to aluminum10.1007/s11661-019-05409-4 ↗
18. Role of plastic deformation mechanisms during the microstructural evolution and intermetallics formation in dissimilar friction stir weld10.1016/j.matchar.2020.110371 ↗
19. A new method to elucidate fracture mechanism and microstructure evolution in titanium during dissimilar friction stir welding of aluminum and titanium10.1016/j.matchar.2020.110791 ↗
20. Microstructural evolution and mechanical properties of a linear friction welded two-phase Ti-6.5Al-3.5Mo-1.5Zr-0.3Si titanium alloy joint10.1016/j.msea.2018.11.059 ↗
21. Low cycle fatigue properties of linear friction welded joint of TC11 and TC17 titanium alloys10.1016/j.jallcom.2016.03.113 ↗
22. A literature review of Ti-6Al-4V linear friction welding10.1016/j.pmatsci.2017.10.003 ↗
23. Solid state joining of metals by linear friction welding: a literature review10.1179/026708310X520510 ↗
24. A review on inertia and linear friction welding of Ni-based superalloy10.1007/s11661-015-2752-4 ↗
25. Modelling of workpiece geometry effects on Ti-6Al-4V linear friction welds10.1016/j.matdes.2015.09.080 ↗
26. Effect of the forging pressure on the microstructure and residual stress development in Ti-6Al-4V linear friction welds10.1016/j.actamat.2009.07.055 ↗
27. Effect of post-weld heat treatment on microstructure and property of linear friction welded Ti17 titanium alloy joint10.1179/1362171811Y.0000000079 ↗
28. Visualization of local electrochemical activity and local nickel ion release on laser-welded NiTi/steel joints using combined alternating current mode and stripping mode SECM10.1039/b804718a ↗
29. Exploring the functional and corrosion behavior of friction stir welded NiTI shape memory alloy10.1016/j.jmapro.2019.09.017 ↗
30. Part II.: dissimilar friction stir welding of nickel titanium shape memory alloy to stainless steel – microstructure, mechanical and corrosion behavior
31. Transformation mechanism of secondary phase and its effect on intergranular corrosion in laser wire filling welding Ni-based alloy/304 stainless steel10.1016/S1003-6326(21)65532-2 ↗
32. Correlation between the microstructure and corrosion behaviour of copper/316L stainless-steel dissimilar-metal welded joints10.1016/j.corsci.2021.109729 ↗
33. Refill friction stir spot welded AA5754-H22/Ti-6Al-4V joints: microstructural characterization and electrochemical corrosion behavior of aluminum surfaces
34. Effect of heat treatment on corrosion behavior of Ti-6Al-4V alloy weldments10.1016/j.jmatprotec.2007.12.065 ↗
35. Hot working of Ti-6Al-3Mo-2Zr-0.3Si alloy with lamellar α+β starting structure using processing map10.1016/j.matdes.2008.07.031 ↗
36. The heat treatment improving the mechanical and fatigue property of TA15 alloy joint by friction welding10.1016/j.matchar.2021.111399 ↗
37. Microstructure evolution mechanism and mechanical properties of TC11-TC17 dual alloy annealing treatment10.1016/j.jallcom.2020.155874 ↗
38. Nucleation and growth mechanical of α-lamellae of Ti alloy TA15 cooling from an α+β phase field10.1016/j.actamat.2012.12.025 ↗
39. Thermal deformation mechanism of TC11/TC17 linear friction welded joint during isothermal compression10.1016/j.matchar.2021.111319 ↗
40. Comparison of the corrosion and passivity behavior between CrMnFeCoNi and CrFeCoNi coatings prepared by argon arc cladding10.1016/j.jmrt.2020.05.093 ↗
41. Microstructure evolution and corrosion behavior of dissimilar 304/430 stainless steel welded joints10.1016/j.jmapro.2019.12.015 ↗
42. Characterization of passive films on shape memory stainless steels10.1016/j.corsci.2011.12.022 ↗
43. Comparative studies on microstructure evolution and corrosion resistance of 304 and a newly developed high Mn and N austenitic stainless steel welded joints10.1016/j.corsci.2021.109338 ↗
44. Insights into the intergranular corrosion of overlay welded joints of X65-Inconel 625 clad pipe and its relationship to damage penetration10.1016/j.corsci.2019.108169 ↗
45. Local electrochemical properties of fusion boundary region in SA508-309L/308L overlay welded joint10.1016/j.corsci.2019.04.021 ↗
46. Behavior of crevice corrosion of iron10.1016/j.corsci.2004.08.001 ↗
47. The significance of the local electrode potential within pits, crevices and cracks10.1016/0010-938X(89)90039-5 ↗
48. The role of acetic acid oh H+ in initiating crevice corrosion of N80 carbon steel in CO2-saturated NaCl solution10.1016/j.corsci.2017.08.028 ↗
49. The crevice corrosion behaviour of stainless steel in sodium chloride solution10.1016/j.corsci.2011.08.012 ↗