Micro-crystallographically unraveling strength-enhanced behaviors of the heavy-thick Ti-6Al-4V welded joint
Source abstract
Abstract
Developing high-strength welded joint of heavy-thick titanium alloy plates is in immediate need to unravel the strength-enhanced behaviors for high-pressure and low-temperature performance of deep-sea submersibles. Here, we synergistically employed transmission electron microscope (TEM) and electron back-scattered diffraction (EBSD) technologies to micro-crystallographically unravel the evolution behaviors of weld microstructure, grain orientation and grain boundaries for the welded joint of the heavy-thick Ti-6Al-4V plates with the thickness of up to 60 mm. Resulted, the strength-enhanced welded joint was evidently ascribed to the transformation of lath martensite into basketweave-martensite and the rigid-flexible mixture strategy of the enhanced conical-texture and the weakened basal-texture and cylindrical-texture. Furthermore, the remarkably lowered geometrically necessary dislocations (GNDs) density and the greatly decreased deformation-prone grains number due to the transformation of low-into-high angle grain boundaries indispensably strengthened the joint strength. Therefore, this work has made clear the strength-enhanced behaviors of Ti-6Al-4V welded joints for substantially improving high-strength welded structure of heavy-thick titanium alloy plates, and sufficiently promoting the service safety for deep-sea submersibles.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Welding Techniques and Residual Stresses · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Mechanical properties and microstructure of a high-power laser-welded Ti6Al4V titanium alloy10.1007/s11665-020-04737-6 ↗
2. Microstructural and mechanical properties of a beta-type titanium alloy joint fabricated by friction stir welding10.1016/j.msea.2017.11.006 ↗
3. Joint formation and mechanical properties of back heating assisted friction stir welded Ti–6Al–4V alloy10.1016/j.matdes.2016.10.012 ↗
4. Residual stress in laser welding of TC4 titanium alloy based on ultrasonic laser technology10.3390/app8101997 ↗
5. Evaluation of microstructural development in electron beam melted Ti-6Al-4V10.1016/j.matchar.2011.12.008 ↗
6. Pitting corrosion studies on Ti6Al4V alloy weldments in marine environment
7. Grain size and orientation effects when microcutting AISI 1045 steel10.1016/j.cirp.2007.05.016 ↗
8. Revealing competitive columnar grain growth behavior and periodic microstructural banding in additively manufactured Ti-6Al-4V parts by selective electron beam melting10.1016/j.mtla.2019.100365 ↗
9. Crystal orientation evolution during friction stir welding of 6082 aluminum alloys
10. Microstructure evolution and metallurgical characteristic of bead-on-plate TIG welding of Ti-6Al-4V alloy10.1016/j.jmatprotec.2018.10.002 ↗
11. Characterization of keyhole gas tungsten arc welded AISI 430 steel and joint performance optimization10.1007/s00170-018-2257-6 ↗
12. Microstructure and mechanical behavior of a titanium-to-stainless steel dissimilar joint brazed with Ag-Cu alloy filler and an Ag interlayer10.1016/j.matchar.2017.04.032 ↗
13. The development of high strength brazing technique for Ti-6Al-4V using TiZrCuNi amorphous filler10.1016/j.matchar.2017.07.039 ↗
14. Fabrication of high-quality Ti joint with ultrafine grains using submerged friction stirring technology and its microstructural evolution mechanism10.1016/j.actamat.2018.12.059 ↗
15. Effect of electron beam welding on the microstructures and mechanical properties of thick TC4-DT alloy10.1016/j.matdes.2011.09.004 ↗
16. Inhomogeneous fatigue characteristics of welded Ti–6Al–4V thick plate by the electron beam method
17. Microstructure, texture and mechanical properties of commercial high-purity thick titanium plates jointed by electron beam welding10.1016/j.msea.2016.09.030 ↗
18. Relationship between the textures and the elastic moduli of electron beam welded joint in Ti-6al-4v titanium alloy10.4028/www.scientific.net/AMR.936.1910 ↗
19. Microstructure and stress distribution of TC4 titanium alloy joint using laser-multi-pass-narrow-gap welding10.1007/s00170-020-05623-0 ↗
20. Narrow-gap tungsten inert gas welding of 78-mm-thick Ti–6Al–4V alloy10.1080/02670836.2015.1131941 ↗
21. Microstructure, texture, and mechanical properties of Ti-6Al-4V joints by K-TIG welding10.1016/j.jmapro.2018.12.022 ↗
22. Solidification of laser deposition shaping for TC4 alloy based on cellular automation10.1016/j.jallcom.2016.03.204 ↗
23. Influence of microstructure on mechanical properties of laser metal wire-deposited Ti-6Al-4V10.1016/j.msea.2016.07.038 ↗
24. Residual stress and texture control in Ti-6Al-4V wire+ arc additively manufactured intersections by stress relief and rolling10.1016/j.matdes.2018.03.065 ↗
25. Recent progresses in competitive grain growth during directional solidification
26. Comparison of bead shape, microstructure and mechanical properties of fiber laser beam welding of 2 mm thick plates of Ti-6Al-4V alloy10.1016/j.optlastec.2018.02.021 ↗
27. Microstructure characterization of laser welded Ti-6Al-4V fusion zones10.1016/j.matchar.2013.11.005 ↗
28. Strengthening mechanism of two-phase titanium alloys with basketweave microstructure10.1016/j.jallcom.2014.03.057 ↗
29. Fracture toughness of electron beam welded Ti6Al4V10.1016/j.jmatprotec.2007.08.001 ↗
30. Effects of deep cryogenic treatment on the residual stress and mechanical properties of electron-beam-welded Ti–6Al–4V joints10.1016/j.msea.2016.07.101 ↗
31. Thermodynamic character of phase transformation of TC4 titanium alloy electron beam welded joint
32. Tensile deformation mechanism and micro-void nucleation of Ti-55531 alloy with bimodal microstructure10.1016/j.jmrt.2020.11.008 ↗
33. Investigation of welding parameter dependent microstructure and mechanical properties in friction stir welded pure Ti joints10.1016/j.msea.2010.02.023 ↗
34. Deformation behavior of HCP Ti-Al alloy single crystals10.1007/s11661-002-0153-y ↗
35. Microstructure and mechanical properties of a thick-section high-strength steel welded joint by novel double-sided hybrid fibre laser-arc welding10.1016/j.msea.2013.05.077 ↗