Effect of multi-stage aging on the precipitation strengthening and mechanical properties for an Al-Mg-Si-Ag alloy
Source abstract
Abstract
Multi-step aging and microalloying are the methods that can effectively facilitate the precipitation strengthening and enhance the performance of Al-Mg-Si alloys. The effect of multi-step aging on the precipitation and properties for an Ag-microalloying Al-Mg-Si alloy is systematically investigated in this article. Controlling temperatures of the primary and secondary aging steps are essential for promoting the effectiveness of the multi-stage aging. The optimal multi-stage aging treatment is identified as: 100 °C × 2 h + 180 °C × 2 h, which gives a peak hardness of 142.4 HV (13.7 HV higher than that of the single-stage aging) for this alloy. It is demonstrated that the primary aging at 100 °C can promote the formation of high density of Cluster(2), and the secondary aging at 180 °C accelerates the transformation of Cluster(2) to β″ caused by the good combination of thermodynamics and kinetics of the transformation. The incorporation of Ag atoms can further promote the nucleation of the β” phase.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Design of solute clustering during thermomechanical processing of AA6016 Al–Mg–Si alloy10.1016/j.actamat.2020.10.074 ↗
2. Atomic scale investigation of the crystal structure and interfaces of the B′ precipitate in Al-Mg-Si alloys10.1016/j.actamat.2019.11.059 ↗
3. Precipitation phenomena in ultrafine grained Al–Mg–Si alloy with heterogeneous microstructure10.1016/j.actamat.2015.10.030 ↗
4. Precipitation strengthening of aluminum alloys by room-temperature cyclic plasticity10.1126/science.aav7086 ↗
5. Study of precipitation in Al–Mg–Si alloys by atom probe tomography I. Microstructural changes as a function of ageing temperature10.1016/j.actamat.2015.08.017 ↗
6. Cluster evolution mechanisms during aging in Al–Mg–Si alloys10.1016/j.actamat.2015.09.027 ↗
7. The precipitation sequence in Al-Mg-Si alloys10.1016/S1359-6454(98)00059-7 ↗
8. Transmission electron microscopy study of the β’ phase (Al–Mg–Si alloys) and QC phase (Al–Cu–Mg–Si alloys): ordering mechanism and crystallographic structure10.1016/S1359-6454(00)00057-4 ↗
9. Hexagonal tabular β-phase in Al–Mg–Si–Cu alloy10.1016/S1359-6462(02)00173-2 ↗
10. Crystal structure of the orthorhombic U2-Al4Mg4Si4 precipitate in the Al–Mg–Si alloy system and its relation to the β’ and β″ phases10.1016/j.msea.2004.09.019 ↗
11. Detailed atomistic insight into the β″ phase in Al–Mg–Si alloys10.1016/j.actamat.2014.01.052 ↗
12. Density functional study of the β″ phase in Al-Mg-Si alloys10.1007/s11661-014-2214-4 ↗
13. TEM study of β’ precipitate interaction mechanisms with dislocations and β’ interfaces with the aluminium matrix in Al–Mg–Si alloys10.1016/j.matchar.2012.10.003 ↗
14. Precipitate characteristics and selected area diffraction patterns of the β’ and Q′ precipitates in Al–Mg–Si–Cu alloys10.1080/09500839.2010.541165 ↗
15. The multiple orientation relationships and morphology of β' phase in Al-Mg-Si-Cu alloy10.1016/j.jallcom.2018.07.077 ↗
16. The effect of interrupted aging on the yield strength and uniform elongation of precipitation-hardened Al alloys10.1016/j.actamat.2013.06.036 ↗
17. A systematic study of the effect of interrupted ageing conditions on the strength and toughness development of AA606110.1016/j.msea.2009.06.044 ↗
18. Secondary precipitation in an Al–Mg–Si–Cu alloy10.1016/j.actamat.2007.01.006 ↗
19. Pre-aging to improve bake hardening in a twin-roll cast Al–Mg–Si alloy10.1016/j.msea.2004.08.069 ↗
20. Three-dimensional atom probe characterization of nanoclusters responsible for multistep aging behavior of an Al-Mg-Si alloy10.1007/s11661-007-9438-5 ↗
21. Effect of Ag and Cu additions on natural aging and precipitation hardening behavior in Al-Mg-Si alloys10.1016/j.jallcom.2016.11.140 ↗
22. DSC and HRTEM investigation of the precipitates in Al–1.0%Mg2 Si–0.5%Ag alloy10.1179/026708304X6086 ↗
23. HAADF-STEM study of β’-type precipitates in an over-aged Al–Mg–Si–Ag alloy10.1080/14786435.2011.642319 ↗
24. Effect of Ag addition on the precipitation evolution and interfacial segregation for Al–Mg–Si alloy10.1016/j.actamat.2019.09.015 ↗
25. Combined effect of pre-aging and Ag/Cu addition on the natural aging and bake hardening in Al-Mg-Si alloys10.1016/j.pnsc.2018.04.007 ↗
26. Atomistic structure of Cu-containing β″ precipitates in an Al–Mg–Si–Cu alloy10.1016/j.scriptamat.2013.11.030 ↗
27. Studies of orientations of β″ precipitates in Al-Mg-Si-(Cu) alloys by Electron diffraction and transition matrix analysis10.1007/s11661-011-0680-5 ↗
28. The diffraction patterns from β″ precipitates in 12 orientations in Al–Mg–Si alloy10.1016/j.scriptamat.2010.01.039 ↗
29. Early stages of solute clustering in an Al–Mg–Si alloy10.1016/j.actamat.2015.02.019 ↗
30. Early stage ageing effects and shallow positron traps in Al–Mg–Si alloys10.1080/14786435.2015.1031848 ↗
31. Clustering and vacancy behavior in high- and low-solute Al-Mg-Si alloys10.1007/s11661-014-2527-3 ↗
32. Solute–vacancy binding in aluminum10.1016/j.actamat.2007.06.039 ↗
33. First-principles calculation of interaction energies between solutes and/or vacancies for predicting atomistic behaviors of microalloying elements in aluminum alloys10.4028/www.scientific.net/MSF.561-565.283 ↗