Crystal growth mechanism and mechanical properties of Ti-6Al-4 V alloy during selective laser melting
Source abstract
Abstract
In this study, the microstructure evolution and mechanical properties of Ti-6Al-4 V alloy fabricated by SLM were investigated with various energy densities. Experimental results showed that the fast solidification induced by high-speed laser scanning resulted in a prior β columnar grain and multistage acicular α` phase within the final solidified microstructure, and that a high energy density could cause the size of β columnar crystals and α` phase to rise. During SLM solidification, different crystallization types were found of the molten pool due to different temperature gradients and heat flow directions. Furthermore, the results indicated that grain size and densification degree, both of which are affected by energy densities, could have a considerable impact on mechanical properties. Additionally, the anisotropy of the material`s tensile characteristics was determined by the geometry of the molten pool boundary and the growth direction of the microstructure. As the energy density was selected at the optimal value of 74.07 J/mm 3 , the largest tensile strength of 1138 MPa with a strain of 5.1% was obtained.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Preparation and mechanical properties of titanium alloy matrix composites reinforced by Ti3AlC and TiC ceramic particulates10.1016/j.jallcom.2021.161216 ↗
2. Machinability of titanium alloys (Ti-6Al-4V and Ti555.3)[J]10.1016/j.jmatprotec.2008.06.020 ↗
3. Processing window and evaporation phenomena for Ti–6Al–4V produced by selective electron beam melting10.1016/j.actamat.2014.05.037 ↗
4. Steels in additive manufacturing: a review of their microstructure and properties
5. Polymers for 3D printing and customized additive manufacturing10.1021/acs.chemrev.7b00074 ↗
6. Optimization of laser energy density and scanning strategy on the forming quality of 24CrNiMo low alloy steel manufactured by SLM10.1016/j.matchar.2020.110718 ↗
7. Tailorable microstructure and mechanical properties of selective laser melted TiB/Ti–6Al–4V composite by heat treatment
8. Ductility of a Ti-6Al-4V alloy produced by selective laser melting of prealloyed powders10.1108/13552541011083371 ↗
9. Comparative study of fatigue properties of Ti-6Al-4V specimens built by electron beam melting (EBM) and selective laser melting (SLM)10.1016/j.matchar.2018.03.028 ↗
10. Formation and control of martensite in Ti-6Al-4V alloy produced by selective laser melting10.1016/j.matdes.2016.06.117 ↗
11. Role of molten pool mode on formability, microstructure and mechanical properties of selective laser melted Ti-6Al-4V alloy10.1016/j.matdes.2016.08.036 ↗
12. Effect of scanning strategy on mechanical properties of selective laser melted Inconel 71810.1016/j.msea.2019.03.007 ↗
13. Experimental realisation of build orientation effects on the mechanical properties of truly as-built Ti-6Al-4V SLM parts10.1016/j.jmapro.2021.01.027 ↗
14. Comparison of the microstructures and mechanical properties of Ti–6Al–4V fabricated by selective laser melting and electron beam melting10.1016/j.matdes.2015.12.135 ↗
15. The effect of SLM process parameters on density, hardness, tensile strength and surface quality of Ti-6Al-4V
16. Role of impinging powder particles on melt pool hydrodynamics, thermal behaviour and microstructure in laser-assisted DED process: a particle-scale DEM – CFD – CA approach10.1016/j.ijheatmasstransfer.2020.119989 ↗
17. Effect of build geometry on the β-grain structure and texture in additive manufacture of Ti 6Al 4V by selective electron beam melting10.1016/j.matchar.2013.07.012 ↗
18. A pragmatic part scale model for residual stress and distortion prediction in powder bed fusion
19. Dynamic loading of direct metal laser sintered AlSi10Mg alloy: strengthening behavior in different building directions10.1016/j.matdes.2018.08.045 ↗
20. Microstructural evolution and mechanical behavior of nickel aluminum bronze Cu-9Al-4Fe-4Ni-1Mn fabricated through wire-arc additive manufacturing
21. Additive manufacturing of metals: microstructure evolution and multistage control10.1016/j.jmst.2021.06.011 ↗
22. Investigation of crystal growth mechanism during selective laser melting and mechanical property characterization of 316L stainless steel parts10.1016/j.matdes.2016.03.111 ↗
23. Influence of SLM scan-speed on microstructure, precipitation of Al3Sc particles and mechanical properties in Sc- and Zr-modified Al-Mg alloys - ScienceDirect10.1016/j.matdes.2017.11.053 ↗
24. Size dependence of microstructure of AlSi10Mg alloy fabricated by selective laser melting
25. Selective laser melting of in situ titanium–titanium boride composites: processing, microstructure and mechanical properties10.1016/j.actamat.2014.05.022 ↗
26. Phase transformations during cooling in α+β titanium alloys10.1016/S0921-5093(97)00802-2 ↗
27. Comparison of the microstructures and mechanical properties of Ti-6Al-4V fabricated by selective laser melting and electron beam melting10.1016/j.matdes.2015.12.135 ↗
28. Microstructure and mechanical properties of laser welded lap joints of Ti-6Al-4V alloy10.4028/www.scientific.net/AMR.311-313.2375 ↗
29. Dendritic growth velocity and diffusive speed in solidification of undercooled dilute Ni-Zr melts10.1016/S0921-5093(96)10656-0 ↗
30. Sintering of commercially pure titanium powder with a Nd:YAG laser source10.1016/S1359-6454(02)00567-0 ↗
31. The microstructure evolution and softening processes during high-temperature deformation of a 21Cr–10Ni–3Mo duplex stainless steel10.1016/j.actamat.2016.01.012 ↗
32. Microstructure evolution, wear behavior, and corrosion performance of alloy steel gradient material fabricated by direct laser deposition10.1016/j.jmrt.2020.08.074 ↗
33. Texture and microstructure characterization in laser additive manufactured Ti–6Al–2Zr–2Sn–3Mo–1.5Cr–2Nb titanium alloy10.1016/j.matdes.2015.09.053 ↗
34. Experimental investigation and statistical optimisation of the selective laser melting process of a maraging steel10.1016/j.optlastec.2014.07.021 ↗
35. On the role of melt flow into the surface structure and porosity development during selective laser melting10.1016/j.actamat.2015.06.004 ↗
36. Densification behavior, microstructure evolution, and wear performance of selective laser melting processed commercially pure titanium10.1016/j.actamat.2012.04.006 ↗
37. Density and mechanical properties in selective laser melting of Invar 36 and stainless steel 316L10.1016/j.jmatprotec.2018.11.006 ↗
38. Additive manufacturing of metals: a brief review of the characteristic microstructures and properties of steels, Ti-6Al-4V and high-entropy alloys10.1080/14686996.2017.1361305 ↗
39. Origin of dislocation structures in an additively manufactured austenitic stainless steel 316L10.1016/j.actamat.2020.07.063 ↗
40. Solute clustering and supersaturated solid solution of AlSi10Mg alloy fabricated by selective laser melting10.1016/j.heliyon.2019.e01186 ↗
41. Effect of selective laser melting parameters on morphology, microstructure, densification and mechanical properties of supersaturated silver alloy10.1016/j.matdes.2019.107697 ↗
42. Intragranular cellular segregation network structure strengthening 316L stainless steel prepared by selective laser melting10.1016/j.jnucmat.2015.12.034 ↗