Effect of processing parameters on the formation of Cf/LAS composites/Ag Cu Ti/TC4 brazed joint
Source abstract
Abstract
Abstract Cf/LAS composites were successfully jointed to TC4 alloy with Ag Cu Ti filler by vacuum brazing. The interfacial microstructure of TC4/Cf/LAS composites joints was characterized by employing scanning electron microscope (SEM), energy dispersive spectrometer (EDS), X-diffraction (XRD) and transmission electron microscopy (TEM). The determination of the thin interfacial reaction layer (TiSi2 + TiC layer) was realized by TEM. The effect of holding time on the interfacial microstructure and shear strength were investigated. With the increasing holding time, the thickness of diffusion layer, Ti3Cu4 layer, and TiSi2 + TiC layer increased obviously, on the contrary, that of Ti Cu intermetallic compound layers decreased gradually. Besides, blocky Ti3Cu4 phase was coarsened when the joint was brazed at 890 °C for 20 min, which deteriorated the mechanical properties of the joint dramatically. The interfacial evolution of TC4/Cf/LAS composites joint and the formation of TiSi2, TiC, Ti3Cu4, TiCu and Ti2Cu phases were expounded. The maximum shear strength of 26.4 MPa was obtained when brazed at 890 °C for 10 min.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Intermetallics and Advanced Alloy Properties · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. Effect of graphite intercalation compounds in the interfacial on the mechanical and thermal properties of unidirectional carbon fiber reinforced spodumene composite10.1016/j.actamat.2013.02.046 ↗
2. Effect of SiC nanowires on the thermal shock resistance of joint between carbon/carbon composites and Li2O–Al2O3–SiO2 glass ceramics10.1016/j.jeurceramsoc.2014.03.011 ↗
3. Effect of boron doping on the thermal properties of carbon fiber reinforced lithium aluminosilicate matrix composites10.1016/j.jeurceramsoc.2015.03.010 ↗
4. Brazing TC4 alloy to Si3N4 ceramic using nano-Si3N4 reinforced AgCu composites filler10.1016/j.matdes.2015.03.046 ↗
5. Microstructure and mechanical properties of Al2O3 ceramic and TiAl alloy joints brazed with Ag-Cu-Ti filler metal10.1016/j.ceramint.2016.01.078 ↗
6. Microstructure and mechanical properties of SiO2-BN ceramic and Invar alloy joints brazed with Ag-Cu-Ti+TiH2+BN composite filler10.1016/j.jmat.2015.10.003 ↗
7. Microstructure and mechanical properties of C/C composites/TC4 joint with inactive AgCu filler metal10.1016/j.ceramint.2015.02.006 ↗
8. Study of joining of carbon/carbon composites for ultrastable structures10.1016/j.jeurceramsoc.2009.12.013 ↗
9. 2012. The study on joining carbon/carbon composites using Ti–Ni–Si compound10.1016/j.msea.2012.03.059 ↗
10. Microstructure and mechanical properties of C/C composites/TC4 joint using AgCuTi filler metal10.1016/j.msea.2006.11.056 ↗
11. Joining of C/C composites to TC4 using SiC particle-reinforced brazing alloy10.1016/j.matchar.2010.03.008 ↗
12. Active brazing carbon/carbon composite to TC4 with Cu and Mo composite interlayers10.1016/j.msea.2009.06.049 ↗
13. Microstructural evolution and mechanical properties of vacuum-brazed C/C composites with AgCuTi foil10.1016/j.msea.2012.11.057 ↗
14. Active metal brazing and characterization of brazed joints in titanium to carbon–carbon composites10.1016/j.msea.2005.08.179 ↗
15. An innovative joint structure for brazing Cf/SiC composites to titanium alloy10.1007/s11665-014-1074-9 ↗
16. Joining of Cf/SiC composites with a Cu–Au–Pd–V brazing filler and interfacial reactions10.1016/j.jeurceramsoc.2013.12.022 ↗
17. Interfacial reactions and joining characteristics of a Cu–Pd–V system filler alloy with Cf/SiC composites10.1016/j.ceramint.2013.12.131 ↗
18. Brazing of carbon fiber reinforced SiC composites and TC4 using Ag–Cu–Ti active brazing alloy10.1016/j.msea.2009.09.024 ↗
19. Joints of carbon fiber-reinforced SiC composites to Ti-alloy brazed by Ag–Cu–Ti short carbon fibers10.1016/j.jmatprotec.2007.01.031 ↗
20. Microstructure of reactive composite brazing joints of Cf/SiC composites and Ti alloy with Cu-Ti-C filler material
21. Microstructures and mechanical properties of Cf/SiC composite and TC4 alloy joints brazed with (Ti–Zr–Cu–Ni)+W composite filler materials10.1016/j.compscitech.2014.03.021 ↗
22. Microstructural evolution and mechanical properties of the joint of TiAl alloys and C/SiC composites vacuum brazed with Ag–Cu filler metal10.1016/j.matchar.2011.05.007 ↗
23. Interfacial microstructure and mechanical properties of TiAl and C/SiC joint brazed with TiH2–Ni–B brazing powder10.1016/j.matchar.2013.02.010 ↗
24. Brazing continuous carbon fiber reinforced Li2O–Al2O3–SiO2 ceramic matrix composites to Ti–6Al–4V alloy using Ag–Cu–Ti active filler metal10.1016/j.matdes.2015.08.005 ↗
25. Microstructure and interfacial reactions during active metal brazing of stainless steel to titanium10.1007/s11661-012-1599-1 ↗