Creep-induced microstructural evolution in a nickel-based superalloy designed for advanced ultra-supercritical boilers

Qingshuang Xu, Tieshan Cao, Fei Ye, Fanghong Xu, Huifang Li, Xudong Fang, Jie Zhao

Publisher page

Abstract

Abstract Long-term microstructural stability is a major concern for candidate materials used in advanced ultra-supercritical (A-USC) power plants. In the present work, precipitation behavior of a nickel based superalloy designed for A-USC boilers, with a base composition of Ni-25Cr-20Co, was investigated during long-term thermal exposure under different stresses at 1043 K. The results showed that the coarsening of γ′ precipitates in the grain interior had occurred during thermal exposure in the presence and absence of stress. The microstructure around grain boundary was altered remarkably under stress. The precipitate-free zones (PFZs) commonly existed near the grain boundary in the gauge sections of specimens after long-term creep. Coarsened and elongated particles in the PFZs were identified as γ′-Ni 3 (Ti, Al) precipitates by chemical composition analysis and diffraction pattern. Furthermore, the morphology and distribution of MC-type carbides have no significant changes observed due to their good stability, but discontinuous M 23 C 6 appeared under stress, due to formation of PFZs resulting in dissolution of the adjacent M 23 C 6 . Besides, the creep-rupture mechanism was discussed to explore a potential approach for improving creep properties.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High Temperature Alloys and Creep · Microstructure and Mechanical Properties of Steels · Advanced Materials Characterization Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. High-efficiency coal-fired power plants development and perspectives10.1016/j.energy.2005.05.025 ↗
2. Materials for ultra-supercritical coal-fired power plant boilers10.1016/j.ijpvp.2006.08.006 ↗
3. U.S. program on materials technology for ultra-supercritical coal power plants10.1361/10599490524039 ↗
4. Microstructural analysis of laser weld fusion zone in Haynes 282 superalloy10.1016/j.matchar.2011.12.009 ↗
5. Microstructure of long-term aged IN617 Ni-base superalloy10.1007/s11661-008-9618-y ↗
6. Effect of long-term service exposure on microstructure and mechanical properties of alloy 61710.1016/j.matdes.2011.01.017 ↗
7. Microstructural evolution of a Ni-based superalloy (617B) at 700 degrees C studied by electron microscopy and atom probe tomography10.1016/j.actamat.2011.11.020 ↗
8. Phase precipitation and phase stability in nimonic 26310.1007/s11661-001-0217-4 ↗
9. Microstructure and phase stability in INCONEL alloy 740 during creep10.1016/j.scriptamat.2004.05.047 ↗
10. Microstructure evolution and mechanical properties of Inconel 740H during aging at 750 degrees C10.1016/j.msea.2013.09.076 ↗
11. Nickel base superalloys for next generation coal fired AUSC power plants
12. Research and improvement on structure stability and corrosion resistance of nickel-base superalloy INCONEL alloy 74010.1016/j.matdes.2005.03.015 ↗
13. The microstructural evolution of Inconel alloy 740 during solution treatment, aging, and exposure at 760 °C10.1007/s11665-010-9731-0 ↗
14. Microstructure and phase precipitate behavior of Inconel 740H during aging10.1016/S1003-6326(16)64266-8 ↗
15. Detrimental effect of cellular precipitation on the creep strength of Inconel 740H10.1080/09500839.2013.847289 ↗
16. Coarsening behaviour of M23C6 carbides in creep-resistant steel exposed to high temperatures10.1038/srep29734 ↗
17. Microstructural changes and their effect on tensile properties of a Ni-Fe based alloy during long-term thermal exposure10.1016/j.msea.2016.06.018 ↗
18. Quantification of the detrimental effects of precipitate free zones on the yield strength of a superalloy10.1016/S1359-6462(02)00566-3 ↗
19. Denuded zones, diffusional creep, and grain boundary sliding10.1007/s11661-002-0084-7 ↗
20. The effects of precipitation free zones on order strengthening in NIMONIC PE16 bi-crystals10.1016/S0921-5093(00)02035-9 ↗
21. Microstructural evolution of INCONEL (R) alloy 740H((R)) fusion welds during creep10.1007/s11661-014-2682-6 ↗
22. Gamma prime coarsening and age-hardening behaviors in a new nickel base superalloy10.1016/j.matlet.2003.10.053 ↗
23. Review progress in Ostwald ripening theories and their applications to the γ′-precipitates in nickel-base superalloys part II nickel-base superalloys10.1023/A:1015408116016 ↗
24. Microstructural stability and mechanical properties of a newly developed Ni–Fe-base superalloy10.1016/j.msea.2014.11.010 ↗
25. Microstructural characteristics and mechanical properties of a Mo modified Ni–Fe–Cr based alloy10.1016/j.msea.2016.08.081 ↗
26. Evolution of the microstructure and microhardness of a new wrought Ni–Fe based superalloy during high temperature aging10.1016/j.jallcom.2015.04.184 ↗
27. Precipitation behaviour of γ′ phase in alloy 69310.1016/j.matchar.2016.07.007 ↗
28. Elasticity effects on the microstructure of alloys containing coherent precipitates10.1016/0079-6425(96)00001-1 ↗
29. Microstructural changes in Inconel (R) 740 after long-term aging in the presence and absence of stress10.1007/s11837-014-1208-4 ↗
30. Influence of Ru on solidification behavior, microstructure and hardness of re-free Ni-based equiaxed superalloys with high Cr content10.1016/j.jmst.2015.11.009 ↗
31. Development of microstructural damage in Ni-based alloys during creep10.1007/s11661-016-3346-5 ↗
32. Rafting in Superalloys10.1007/BF02648942 ↗
33. Strain-induced morphologies during homogeneous phase separation in alloys10.1080/01411599908224505 ↗
34. Discontinuous reactions in solids10.1179/095066001101528402 ↗
35. Creep deformation and rupture mechanism of an advanced wrought NiFe-based superalloy for 700 °C class A-USC steam turbine rotor application10.1016/j.jallcom.2016.06.120 ↗
36. Effect of PFZ and grain boundary precipitate on mechanical properties and fracture morphologies in Al-Zn-Mg(Ag) alloys10.4028/www.scientific.net/MSF.638-642.297 ↗
37. Softening of the superalloy NIMONIC PE16 by precipitate free zones along grain boundaries10.1016/j.msea.2004.01.075 ↗
38. Microstructure and texture study on an advanced heat-resistant alloy during creep10.1016/j.matchar.2017.05.037 ↗