In-situ investigation into the deformation behavior of Ti-6Al-4V processed by laser powder bed fusion
Source abstract
Abstract
In this work, we presented an investigation into the deformation behavior of laser powder bed fusion (LPBF) Ti-6Al-4V (Ti64), particularly how microstructure characteristics determined the grain deformation behavior by using in-situ SEM tensile characterization. Results demonstrated that α laths with their elongation directions 45° to the tensile loading axis and α laths with the larger thickness could induce severe strain accumulation during the uniaxial tensile process. Crystallographic orientations and grain morphologies of α lath were considered the key factors that could influence the deformation behavior. The strain localization was observed in the α laths dominated by multiple slip systems. Furthermore, the α laths with their elongation directions 45° to the tensile loading axis had the longest effective slip length, which could make α laths favorable for deformation. The dislocations multiplication of coarse α laths was much greater than in fine α laths, which could also result in strain localization. These findings could shed light on the deformation behavior related to lamellar structure in LPBF Ti64 and could further help the mechanical property manipulation.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Titanium Alloys Microstructure and Properties · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (59)
Show source-provided references
1. Additive manufacturing of metals10.1016/j.actamat.2016.07.019 ↗
2. Atomic-scale observation of non-classical nucleation-mediated phase transformation in a titanium alloy10.1038/s41563-021-01144-7 ↗
3. A review on wire and arc additive manufacturing of titanium alloy10.1016/j.jmapro.2021.08.018 ↗
4. A literature review of powder-based electron beam melting focusing on numerical simulations
5. Alloy design via additive manufacturing: advantages, challenges, applications and perspectives10.1016/j.mattod.2021.11.026 ↗
6. Additive manufacturing of metallic components – Process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
7. Titanium alloy production technology, market prospects and industry development10.1016/j.matdes.2010.09.011 ↗
8. Metal alloys for fusion-based additive manufacturing10.1002/adem.201700952 ↗
9. Additive manufacturing of Ti6Al4V alloy: A review10.1016/j.matdes.2018.107552 ↗
10. Perspectives on titanium science and technology10.1016/j.actamat.2012.10.043 ↗
11. Y. Zhu, K. Zhang, Z. Meng, K. Zhang, P. Hodgson, N. Birbilis, M. Weyland, H.L. Fraser, S. Chao, V. Lim, H. Peng, R. Yang, H. Wang, A. Huang, Ultrastrong Nanotwinned Titanium Alloys through Additive Manufacturing, (n.d). doi:https://doi.org/10.1038/s41563-022-01359-2.10.1038/s41563-022-01359-2 ↗
12. Effects of subtransus heat treatments on microstructure features and mechanical properties of wire and arc additive manufactured Ti–6Al–4V alloy10.1016/j.msea.2020.139020 ↗
13. Comparison study on microstructure and mechanical properties of Ti-6Al-4V alloys fabricated by powder-based selective-laser-melting and sintering methods10.1016/j.matchar.2020.110358 ↗
14. Microstructure and deformation behavior of Ti-6Al-4V alloy by high-power laser solid forming10.1016/j.actamat.2017.04.026 ↗
15. Isotropic and improved tensile properties of Ti-6Al-4V achieved by in-situ rolling in direct energy deposition
16. Refinement of the grain structure of additive manufactured titanium alloys via epitaxial recrystallization enabled by rapid heat treatment10.1016/j.scriptamat.2020.01.027 ↗
17. Grain structure control during metal 3D printing by high-intensity ultrasound10.1038/s41467-019-13874-z ↗
18. Achieving superior ductility for laser solid formed extra low interstitial Ti-6Al-4V titanium alloy through equiaxial alpha microstructure10.1016/j.scriptamat.2017.11.021 ↗
19. Materials & design effects of the morphology of grain boundary a -phase on the anisotropic deformation behaviors of additive manufactured Ti – 6Al – 4V10.1016/j.matdes.2022.111150 ↗
20. Influence of processing on microstructure and mechanical properties of (α + β) titanium alloys10.1016/S0921-5093(97)00778-8 ↗
21. The effect of microstructure on the mechanical properties of two-phase titanium alloys10.1016/S0924-0136(02)00248-0 ↗
22. The investigation of the influence of laser re-melting on density, surface quality and microstructure of selective laser melting parts10.1108/13552541111156450 ↗
23. Anisotropy and heterogeneity of microstructure and mechanical properties in metal additive manufacturing: A critical review10.1016/j.matdes.2017.11.021 ↗
24. The effectiveness of combining rolling deformation with Wire-Arc Additive Manufacture on β-grain refinement and texture modification in Ti-6Al-4V10.1016/j.matchar.2016.02.001 ↗
25. Effects of post heat treatments on microstructures and mechanical properties of selective laser melted Ti6AL4V alloy10.3390/met11101593 ↗
26. Formation and control of martensite in Ti-6Al-4V alloy produced by selective laser melting10.1016/j.matdes.2016.06.117 ↗
27. Characterization of fatigue crack growth behavior in LENS fabricated Ti-6Al-4V using high-energy synchrotron x-ray microtomography
28. Promoting the columnar to equiaxed transition and grain refinement of titanium alloys during additive manufacturing10.1016/j.actamat.2019.02.020 ↗
29. Anisotropic tensile behavior of Ti-6Al-4V components fabricated with directed energy deposition additive manufacturing10.1016/j.actamat.2014.12.054 ↗
30. Microstructure, static properties, and fatigue crack growth mechanisms in Ti-6Al-4V fabricated by additive manufacturing: LENS and EBM10.1016/j.engfailanal.2016.05.036 ↗
31. Additive manufacturing of strong and ductile Ti-6Al-4V by selective laser melting via in situ martensite decomposition10.1016/j.actamat.2014.11.028 ↗
32. Role of martensite decomposition in tensile properties of selective laser melted Ti-6Al-4V10.1016/j.jallcom.2018.02.111 ↗
33. Deformation and failure mechanisms of Ti–6Al–4V as built by selective laser melting10.1016/j.msea.2019.138456 ↗
34. Microstructure of Ti-6Al-4V produced by selective laser melting10.1088/1742-6596/371/1/012084 ↗
35. Effects of the crystallographic and spatial orientation of α lamellae on the anisotropic in-situ tensile behaviors of additive manufactured Ti–6Al–4V10.1016/j.jallcom.2020.156886 ↗
36. Phase transformations during cooling in α+β titanium alloys10.1016/S0921-5093(97)00802-2 ↗
37. In-situ characterization of laser-powder interaction and cooling rates through high-speed imaging of powder bed fusion additive manufacturing10.1016/j.matdes.2017.09.044 ↗
38. Formation of α-Widmanstätten structure: effects of grain size and cooling rate on the Widmanstätten morphologies and on the mechanical properties in Ti6Al4V alloy10.1016/S0925-8388(01)01571-7 ↗
39. Mechanical properties and deformation mechanisms of martensitic Ti6Al4V alloy processed by laser powder bed fusion and water quenching10.1016/j.msea.2022.142817 ↗
40. Micro-mechanical behaviour of selective laser melted Ti6Al4V under compression10.1016/j.msea.2021.141975 ↗
41. Grain boundary α-phase precipitation and coarsening: comparing laser powder bed fusion with as-cast Ti-6Al-4V10.1016/j.scriptamat.2021.114261 ↗
42. On the texture formation of selective laser melted Ti-6Al-4V10.1007/s11661-014-2218-0 ↗
43. Grain boundary discontinuity and performance improvement mechanism of wire arc additive manufactured Ti–6Al–4V10.1016/j.jallcom.2021.159287 ↗
44. Grain morphology evolution behavior of titanium alloy components during laser melting deposition additive manufacturing10.1016/j.jallcom.2015.01.256 ↗
45. Deformation behaviors of additive manufactured Ti – 6Al – 4V address
46. Fatigue crack initiation in as forged Ti-6Al-4V bars with macrozones present10.1016/j.ijfatigue.2015.05.020 ↗
47. Deformation behavior of Ti-6Al-4V microstructures under uniaxial loading: Equiaxed Vs. transformed-β microstructures10.1016/j.matchar.2020.110780 ↗
48. Process variation in laser powder bed fusion of Ti-6Al-4V
49. Surface roughness of selective laser melted Ti-6Al-4V alloy components
50. Role of martensite decomposition in tensile properties of selective laser melted Ti-6Al-4V10.1016/j.jallcom.2018.02.111 ↗
51. Effect of the build orientation on the mechanical properties and fracture modes of SLM Ti-6Al-4V10.1016/j.msea.2014.07.086 ↗
52. High resolution in situ mapping of microstrain and microstructure evolution reveals damage resistance criteria in dual phase steels10.1016/j.actamat.2015.05.038 ↗
53. Texture analysis with MTEX- free and open source software toolbox10.4028/www.scientific.net/SSP.160.63 ↗
54. In situ SEM investigation of slip transfer in Ti-6Al-4V: effect of applied stress10.1016/j.msea.2017.10.058 ↗
55. In situ EBSD investigation of deformation processes and strain partitioning in bi-modal Ti-6Al-4V using lattice rotations10.1016/j.actamat.2019.04.033 ↗
56. In situ SEM study of tensile deformation of a near-β titanium alloy10.1016/j.msea.2017.10.028 ↗
57. In-situ investigation on the deformation mechanism of duplex microstructure of a near α titanium alloy10.1016/j.jallcom.2021.162184 ↗
58. Fatigue crack initiation in as forged Ti–6Al–4V bars with macrozones present10.1016/j.ijfatigue.2015.05.020 ↗
59. The influence of soft, precipitate-free zones at grain boundaries in Ti and Al alloys on their fatigue and fracture behavior10.1016/j.msea.2006.07.168 ↗