journal article·2024-03

The relationship between an input energy density and the microstructure evolution of the Ti-6Al-4V alloy via laser remelting

Kangkai Hu, Wei Gao, Shicheng Wang, Xuzhou Jiang, Hongying Yu, Dongbai Sun

Publisher page

Abstract

Microstructure can affect the properties of the Ti-6Al-4V alloy. By defining the relationship between a microstructure evolution of the Ti-6Al-4V and an input energy density ( IED ) during laser remelting, it is possible to create an alloy with good surface quality and characteristics. Here, Ti-6Al-4V by laser remelting is obtained, containing transition β phase, primary/secondary α phase, α-martensite, α`-martensite, and α″-martensite. The plate transition β phase appears at the grain boundary of martensite structures, cellular and columnar crystals. Only the β → α`-martensite transition occurs in the range of 20–40 J/mm 2, while the β → α-martensite, β → α`-martensite, and β → α″-martensite transitions occur simultaneously in the range of 40–100 J/mm 2. As IED decreases, the coarse-plate α martensite decreases and acicular α` martensite increases. With the increase of IED , the grains in the melting zone of the specimen are larger, and the columnar crystals are easier to form in this zone. The results will provide a theoretical basis for surface modification of the titanium alloy by laser remelting technology to improve properties.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Titanium Alloys Microstructure and Properties · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (64)

Show source-provided references
1. Design of titanium alloys by additive manufacturing: a critical review
2. Three-dimensional temperature gradient mechanism in selective laser melting of Ti-6Al-4V10.1115/1.4028539 ↗
3. Perspectives on titanium science and technology10.1016/j.actamat.2012.10.043 ↗
4. On the process of transition of the cubic-body-centered modification into the hexagonal-close-packed modification of zirconium10.1016/S0031-8914(34)80244-3 ↗
5. Simultaneous improvement of strength and elongation of laser melting deposited Ti-6Al-4V titanium alloy through three-stage heat treatment10.1016/j.jmatprotec.2022.117607 ↗
6. Review of laser powder bed fusion (LPBF) fabricated Ti-6Al-4V: process, post-process treatment, microstructure, and property, light
7. High-strength titanium alloys for aerospace engineering applications: a review on melting-forging process10.1016/j.msea.2022.143260 ↗
8. Microstructure and corrosion properties of Ti-6Al-4V alloy by ultrasonic shot peening10.1016/S1452-3981(23)11168-0 ↗
9. Improving fatigue performance of metal parts with up-facing inclined surfaces produced by laser powder bed fusion and in-situ laser remelting
10. Understanding the behavior of laser surface remelting after directed energy deposition additive manufacturing through comparing the use of iron and Inconel powders10.1016/j.jmapro.2021.08.061 ↗
11. Fatigue life of titanium alloys fabricated by additive layer manufacturing techniques for dental implants10.1007/s11661-012-1470-4 ↗
12. Variant selection in additively manufactured alpha-beta titanium alloys10.1016/j.jmst.2021.10.021 ↗
13. In-situ grain structure control in directed energy deposition of Ti6Al4V
14. Impact toughness and deformation modes of Ti-6Al-4V alloy with different microstructures10.1016/j.msea.2020.140411 ↗
15. Study on the intrinsic factors determining impact toughness of TC21 alloy10.1016/j.matchar.2021.111164 ↗
16. Microstructural strengthening and toughening mechanisms in Fe-containing Ti-6Al-4V: a comparison between homogenization and aging treated states10.1016/j.jmst.2021.04.063 ↗
17. Microstructure and mechanical properties of the Ni-B-Ti composite coating on TA2 prepared by pre-plating and laser remelting10.1016/j.surfcoat.2020.126567 ↗
18. Microstructure and surface properties of laser-remelted titanium nitride coatings on titanium10.1016/j.surfcoat.2004.08.206 ↗
19. A digital twin for rapid qualification of 3D printed metallic components10.1016/j.apmt.2018.11.003 ↗
20. Martensitic transformations in Ti-6Al-4V (ELI) alloy manufactured by 3D printing10.1016/j.matchar.2018.09.042 ↗
21. Effect of laser surface remelting pretreatment with different energy density on MAO bioceramic coating10.1016/j.surfcoat.2020.125815 ↗
22. Additive manufacturing of strong and ductile Ti-6Al-4V by selective laser melting via in situ martensite decomposition10.1016/j.actamat.2014.11.028 ↗
23. A transmission electron microscopy and three-dimensional atom probe study of the oxygen-induced fine microstructural features in as-sintered Ti-6Al-4V and their impacts on ductility10.1016/j.actamat.2014.01.015 ↗
24. Mechanical properties of fully martensite microstructure in Ti-6Al-4V alloy transformed from refined beta grains obtained by rapid heat treatment (RHT)10.1016/j.scriptamat.2017.05.038 ↗
25. Effect of laser remelting and heat treatment on microstructure and wear resistance of 2A97 Al-Li alloy
26. Prediction of solidification microstructure of titanium aluminum intermetallic alloy by laser surface remelting10.1016/j.optlastec.2021.107606 ↗
27. Effect of laser remelting on deposition quality, residual stress, microstructure, and mechanical property of selective laser melting processed Ti-5Al-2.5Sn alloy10.1016/j.matchar.2019.02.010 ↗
28. Tudy of the laser remelting of a cold sprayed titanium layer10.1016/j.procir.2015.06.101 ↗
29. Microstructure and wear resistance of laser cladded Ni-Cr-Co-Ti-V high-entropy alloy coating after laser remelting processing10.1016/j.optlastec.2017.09.012 ↗
30. Urface grain formation mechanism in the laser remelting molten pool of a near-β titanium alloy10.1016/j.mtla.2022.101521 ↗
31. The formation mechanism of special globular surface grain during the solidification of laser surface remelted near β titanium alloys10.1016/j.commatsci.2021.110353 ↗
32. Effect of laser remelting on microstructural evolution and mechanical properties of Ti-35Nb-2Ta-3Zr alloy10.1016/j.matlet.2019.06.105 ↗
33. Structuring of the Ti6Al4V alloy surface by pulsed laser remelting10.1016/j.apsusc.2020.147618 ↗
34. Underwater surface remelting of selective laser melted titanium parts10.1016/j.jmrt.2020.07.060 ↗
35. Enhanced corrosion, tribocorrosion resistance and controllable osteogenic potential of stem cells on micro-rippled Ti6Al4V surfaces produced by pulsed laser remelting10.1016/j.jmapro.2021.03.023 ↗
36. Effect of laser surface remelting on the corrosion behavior of commercially pure titanium sheet10.1016/S0921-5093(02)00477-X ↗
37. Effect of laser surface remelting and low temperature aging treatments on microstructures and surface properties of Ti-55511 alloy10.1016/j.surfcoat.2016.11.097 ↗
38. Microstructural evolution and mechanical properties of Ti–Zr beta titanium alloy after laser surface remelting10.1016/j.jallcom.2013.08.160 ↗
39. In situ design of advanced titanium alloy with concentration modulations by additive manufacturing10.1126/science.abj3770 ↗
40. Laser polishing of additive manufactured Ti alloys10.1016/j.optlaseng.2017.02.005 ↗
41. Designing against phase and property heterogeneities in additively manufactured titanium alloys10.1038/s41467-022-32446-2 ↗
42. Microstructure evolution and performance of laser-remelted Ti-6Al-4V alloy10.4028/p-ipjl43 ↗
43. In situ synchrotron X-ray imaging of 4140 steel laser powder bed fusion, T
44. In-situ characterization and quantification of melt pool variation under constant input energy density in laser powder bed fusion additive manufacturing process
45. Microstructure and properties of pure titanium coating on Ti-6Al-4V alloy by laser cladding10.1016/j.surfcoat.2021.127137 ↗
46. Microstructural characterization and hardness variation of pure Ti surface-treated by pulsed laser10.1016/j.jallcom.2018.01.113 ↗
47. Correlation of microstructural, textural characteristics and hardness of Ti–6Al–4V sheet β-cooled at different rates10.1007/s10853-020-04603-9 ↗
48. Microstructural characterization and hardness variation of pure Ti surface-treated by pulsed laser10.1016/j.jallcom.2018.01.113 ↗
49. Characterization and correlation of microstructure and hardness of Ti-6Al-4V sheet surface-treated by pulsed laser10.1016/j.jallcom.2020.154243 ↗
50. Gradient microstructure and fatigue properties of TC21 titanium alloy processed by laser shock peening10.1016/j.jallcom.2022.168139 ↗
51. The effect of TiC on microstructure and mechanical properties of Ti-5553 beta phase titanium alloy
52. Understanding melt pool characteristics in laser powder bed fusion: an overview of single- and multi-track melt pools for process optimization
53. Microstructure tailoring and impact toughness of a newly developed high strength Ti-5Al-3Mo-3V-2Cr-2Zr-1Nb-1Fe alloy10.1016/j.matchar.2021.111103 ↗
54. Revealing the intensified preferred orientation and factors dominating the anisotropic mechanical properties of laser powder bed fusion Ti-6Al-4V alloy after heat treatment10.1016/j.jallcom.2023.169494 ↗
55. Optimisation of process parameters to address fundamental challenges during selective laser melting of Ti-6Al-4V: a review10.1016/j.ijmachtools.2018.01.003 ↗
56. Simultaneous optimization of hatching orientations and lattice density distribution for residual warpage reduction in laser powder bed fusion considering layerwise residual stress stacking
57. Weld toe modification using spherical-tip WC tool FSP in fatigue strength improvement of high-strength low-alloy steel joints10.1016/j.matdes.2018.10.036 ↗
58. Determination of the effect of scan strategy on residual stress in laser powder bed fusion additive manufacturing
59. Solid-state cold spraying of Ti and its alloys: a literature review10.1016/j.pmatsci.2019.100633 ↗
60. Online assessment of TiC decomposition in laser cladding ofmetal matrix composite coating10.1016/j.matdes.2017.02.061 ↗
61. Effect of superheated temperature and cooling rate on the solidification of undercooled Ti melt
62. Effect of melt superheating treatment on the latent heat release of Sn10.1007/s11661-016-3900-1 ↗
63. Selective laser melting of pure iron: multiscale characterization of hierarchical microstructure10.1016/j.matchar.2019.05.012 ↗
64. Phase transformations during cooling in α + β titanium alloys10.1016/S0921-5093(97)00802-2 ↗