journal article·2024-06

In-situ reinforced Ti6Al4V-TiB2 titanium matrix composite fabricated by selective laser melting: Microstructure, mechanical properties and heat treatment

Yinan Li, Weiping Fang, Shun Guo, Mengwei Duan, Bingbing Luo, Youkun Li, Jie Liu, Jieren Gu, Yong Peng, Qi Zhou, Kehong Wang

Publisher page

Abstract

Ti6Al4V-x wt%TiB 2 titanium matrix composites (x = 0, 0.01, 1, 3.4, 4.8) were prepared by selective laser melting (SLM), followed by solution-aging treatment. The microstructure and mechanical properties of the SLM-formed samples and the heat-treated ones were systematically investigated. In the SLM-formed samples, in-situ TiB whiskers clustered around the original position of the TiB 2 particles, which reacted with the matrix through dynamic dissolution. The phase transformation of α` → α + β and the coarsening of TiB whiskers occurred during solution-aging treatment. The microhardness of the samples was enhanced with the increase of TiB 2 , while the heat treatment was harmful to microhardness. The fine grain strengthening and the dispersion strengthening caused by TiB whiskers enhanced the quasi-static compressive strength of the samples. The samples were modified successfully by solution-aging, and the compressive strength and strain of the Ti6Al4V-0.01wt.%TiB 2 composite reached 1957 MPa and 23.7% respectively. The samples had higher ductility but lower strength under dynamic load, and the heat treatment had little effect on the dynamic properties.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Titanium Alloys Microstructure and Properties · Additive Manufacturing and 3D Printing Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. High-mass-proportion TiCp/Ti6Al4V titanium matrix composites prepared by directed energy deposition[J]
2. New insights into the evolution of TiB whisker and TiC particle during selective laser melting of titanium matrix composites[J]10.1016/j.msea.2023.145200 ↗
3. Tailoring strength-ductility of titanium matrix composites reinforced with graphene nanoplatelets[J]10.1016/j.msea.2022.144386 ↗
4. Improved mechanical properties in titanium matrix composites: controllable TiBw distribution by thermal deformation process[J]
5. TiBw reinforced titanium matrix composites fabricated by selective laser melting: influence of energy density on microstructure and tribological performance[J]10.1016/j.ceramint.2023.06.161 ↗
6. Effects of process parameters on the microstructure and mechanical properties of a laser micro-alloying TiB/Ti–6Al–4V titanium matrix composite[J]10.1016/j.msea.2023.144988 ↗
7. Nanostructure evolution of reticular nano-TiB whiskers reinforced titanium matrix composite subjected to ultrasonic shot peening[J]10.1016/j.jallcom.2023.169704 ↗
8. Rapid in-situ synthesis, microstructure and mechanical properties of titanium matrix composites with micro/nano-sized TiB/TiC hybrid structures[J]10.1016/j.vacuum.2022.111635 ↗
9. Multilayered gradient titanium-matrix composites fabricated by multi-material laser powder bed fusion using metallized ceramic: forming characteristics, microstructure evolution, and multifunctional properties[J]
10. Enhanced strength and ductility of nano-TiBw-reinforced titanium matrix composites fabricated by electron beam powder bed fusion using Ti6Al4V–TiBw composite powder[J]
11. Process induced multi-layered titanium – boron carbide composites via additive manufacturing[J]
12. The α phase recrystallization mechanism and mechanical properties of a near-α titanium matrix composite[J]10.1016/j.intermet.2022.107597 ↗
13. Microstructural evolution and mechanical properties of in-situ as-cast beta titanium matrix composites[J]10.1016/j.jallcom.2018.11.093 ↗
14. Investigation on mechanical characterization of titanium matrix composites produced through powder metallurgy[J]
15. In-situ synthesized TiC/Ti-6Al-4V composites by elemental powder mixing and spark plasma sintering: microstructural evolution and mechanical properties[J]10.1016/j.jallcom.2023.169557 ↗
16. Laser deposition-additive manufacturing of TiB-Ti composites with novel three-dimensional quasi-continuous network microstructure: effects on strengthening and toughening[J]10.1016/j.compositesb.2017.09.019 ↗
17. Agglomeration-free nanoscale TiC reinforced titanium matrix composites achieved by in-situ laser additive manufacturing[J]10.1016/j.scriptamat.2020.06.057 ↗
18. Influence of in situ ceramic reinforcement towards tailoring titanium matrix composites using laser-based additive manufacturing[J]
19. Effect of ceramic types on the microstructure and corrosion behavior of titanium matrix composites produced by selective laser melting[J]10.1016/j.jallcom.2022.165704 ↗
20. High strength and ductility of titanium matrix composites by nanoscale design in selective laser melting[J]10.1016/j.jmst.2021.12.020 ↗
21. First principle calculations and low cost SLM processing of Ti–TiB composite materials[J]
22. In-situ preparation and formation of TiB/Ti-6Al-4V nanocomposite via laser additive manufacturing: microstructure evolution and tribological behavior[J]10.1016/j.powtec.2018.09.088 ↗
23. Microstructure evolution and mechanical properties of in-situ Ti6Al4V–TiB composites manufactured by selective laser melting[J]10.1016/j.compositesb.2020.108567 ↗
24. Achieving near equiaxed α-Ti grains and significantly improved plasticity via heat treatment of TiB reinforced titanium matrix composite manufactured by selective laser melting[J]10.1016/j.jallcom.2020.155344 ↗
25. Tailorable microstructure and mechanical properties of selective laser melted TiB/Ti–6Al–4V composite by heat treatment[J]
26. A critical review on additive manufacturing of Ti-6Al-4V alloy: microstructure and mechanical properties[J]10.1016/j.jmrt.2022.04.055 ↗
27. New insights into the evolution of TiB whisker and TiC particle during selective laser melting of titanium matrix composites[J]10.1016/j.msea.2023.145200 ↗
28. Nano-TiB whiskers reinforced Ti–6Al–4V matrix composite fabricated by direct laser deposition: microstructure and mechanical properties[J]10.1016/j.jallcom.2022.166171 ↗
29. Microstructure and mechanical properties of (TiB+TiC)/Ti composites fabricated in situ via selective laser melting of Ti and B4C powders[J]
30. Selective laser melting of hybrid ex-situ/in-situ reinforced titanium matrix composites: laser/powder interaction, reinforcement formation mechanism, and non-equilibrium microstructural evolutions[J]10.1016/j.matdes.2019.108185 ↗
31. Refined microstructure and enhanced wear resistance of titanium matrix composites produced by selective laser melting[J]10.1016/j.optlastec.2020.106644 ↗
32. Mesoscopic study of thermal behavior, fluid dynamics and surface morphology during selective laser melting of Ti-based composites[J]10.1016/j.commatsci.2020.109598 ↗
33. Microstructure and mechanical properties of in situ synthesized (TiB+TiC)-reinforced Ti6Al4V composites produced by directed energy deposition of Ti and B4C powders[J]10.1016/j.msea.2022.144466 ↗
34. Microstructure evolution and mechanical properties of selective laser melted bulk-form titanium matrix nanocomposites with minor B4C additions[J]10.1016/j.matdes.2019.108245 ↗
35. Effect of build orientation on dynamic compressive behaviour of Ti-6Al-4V alloy fabricated by selective laser melting[J]10.1016/j.msea.2022.144440 ↗
36. Investigation into the microstructure and dynamic compressive properties of selective laser melted Ti–6Al–4V alloy with different heating treatments[J]10.1016/j.msea.2020.140561 ↗
37. The mechanical response and failure mechanism of a near α titanium alloy under high-strain-rate compression at different temperatures[J]10.1016/j.msea.2021.140749 ↗
38. Study of strain rate sensitivity exponent and strain hardening exponent of typical titanium alloys[J]
39. Dynamic compression deformation behavior of laser directed energy deposited α + β duplex titanium alloy with basket-weave morphology[J]
40. Dynamic compression behavior of multilayered titanium matrix composites[J]10.1016/j.matchar.2023.112698 ↗
41. Effect of heat treatment on microstructure evolution and mechanical properties of selective laser melted Ti–6Al–4V and TiB/Ti–6Al–4V composite: a comparative study[J]10.1016/j.msea.2020.140415 ↗
42. Constructing targeted bi-lamellar microstructure via heat treatment for high compressive strength and plasticity in selective laser melted Ti6Al4V-5vol%TiB composite[J]10.1016/j.msea.2022.143173 ↗
43. Ostwald ripening and grain growth in Ti(C,N)-based cermets during liquid phase sintering10.1016/j.ijrmhm.2016.03.008 ↗
44. Microstructure evolution of SiC whisker-reinforced Ti6Al4V matrix composites manufactured by selective laser melting during heat treatment[J]10.1016/j.matlet.2023.134394 ↗