Understanding the dynamic recrystallization behaviors of a hot-rolled Mg-1.0wt%Ca plate by compressing along different original orientations
Source abstract
Abstract
The effects of original orientations on the dynamic recrystallization (DRX) behaviors of a hot-rolled Mg-1.0wt%Ca plate were investigated in this work. Using hot compression along the rolling direction (RD) and the normal direction (ND) at 400 °C, 430 °C and 460 °C, the microstructural and textural evolutions closely related to the DRX behaviors were analyzed in detail. At the same temperature, DRX occurred more easily in the ND sample. But as the compressive temperature increased, both the area fraction and the size of the DRXed grains improved faster in the RD sample. During hot compressing, very few dislocations persisted in the DRXed grains of the RD sample and the discontinuous DRX mechanism was confirmed. Differently, dislocation tangles composed the grain boundaries of the DRXed grains of the ND sample and the continuous DRX mechanism was confirmed. Besides, compared to commercial Mg alloys such as ZK60 and AZ31, Mg-1.0wt%Ca alloy significantly postponed both the continuous DRX and discontinuous DRX processes. The Mg Ca based alloys with great microstructural stability now offer more possibilities for developing high creep-resistant and high burn-resistant Mg components with free rare-earth addition.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (63)
Show source-provided references
1. Effects of initial texture on the three-dimensional creep anisotropic behaviors of dilute Mg–Y binary alloy sheets10.1016/j.msea.2019.138336 ↗
2. Towards magnesium alloys for high-volume automotive applications10.1016/j.scriptamat.2016.07.035 ↗
3. Effect of heat treatment on magnesium alloys used in automotive industry: a review
4. Microstructure, tensile properties, and corrosion resistance of extruded Mg-1Bi-1Zn alloy: the influence of minor Ca addition10.1016/j.jallcom.2019.152414 ↗
5. Anisotropy in the tensile creep behaviors of a hot-rolled Mg-5.5wt%Y alloy sheet10.1016/j.matchar.2020.110843 ↗
6. Recent developments in rare-earth free wrought magnesium alloys having high strength: a review10.1016/j.jallcom.2015.12.057 ↗
7. Effects of original orientation on compressive creep behaviors of hot-extruded Mg–3Al–1Zn alloy rod10.1016/j.jallcom.2019.07.193 ↗
8. Enhanced plasticity and creep in an extruded Mg–Zn–Zr alloy10.1016/j.scriptamat.2010.05.044 ↗
9. Current development of creep-resistant magnesium cast alloys: a review10.1016/j.matdes.2018.06.032 ↗
10. High temperature mechanical properties and strain hardening mechanism of directionally solidified Mg-Gd-Y alloy10.1016/j.msea.2021.142337 ↗
11. Recent research and developments on wrought magnesium alloys10.1016/j.jma.2017.09.001 ↗
12. The formation mechanism of a novel interfacial phase with high thermal stability in a Mg-Gd-Y-Ag-Zr alloy10.1016/j.actamat.2018.10.005 ↗
13. Tension-compression asymmetry in hot-rolled Mg-3wt%Gd alloy under creep loading10.1016/j.msea.2021.142124 ↗
14. Effect of temperature on the hot deformation behavior of AZ80 magnesium alloy10.1016/j.msea.2020.139923 ↗
15. Optimizing the mechanical properties of a Mg–Y–Nd–Zn–Zr alloy via interrupted compression with an intermediate annealing10.1016/j.msea.2021.141102 ↗
16. Dynamic recrystallization of a wrought magnesium alloy: grain size and texture maps and their application for mechanical behavior predictions10.1016/j.matdes.2021.109562 ↗
17. Microstructural evolutions and mechanical properties of Mg-xY-2Nd-0.2Zn-0.5Zr (x = 0, 2, 4, 6 and 8) alloy under hot compression10.1016/j.msea.2019.138816 ↗
18. Effects of pretwins on texture and microstructural evolutions of AZ31 magnesium alloy during high temperature deformation10.1016/j.jallcom.2021.162412 ↗
19. Effect of initial texture on dynamic recrystallization of AZ31 Mg alloy during hot rolling10.1016/j.msea.2010.11.069 ↗
20. Effect of sample orientation and initial microstructures on the dynamic recrystallization of a magnesium alloy10.1016/j.msea.2017.03.047 ↗
21. Role of compression direction on recrystallization behavior and texture evolution during hot deformation of extruded ZK60 magnesium alloy10.1016/j.jallcom.2017.01.236 ↗
22. Interaction between texture evolution and dynamic recrystallization of extruded AZ80 magnesium alloy during hot deformation10.1016/j.msea.2020.139537 ↗
23. Improving ductility of a Mg alloy via non-basal slip induced by Ca addition10.1016/j.ijplas.2019.04.020 ↗
24. Effect of extrusion speed on microstructure and mechanical properties of the Mg-Ca binary alloy10.1016/j.jma.2020.05.011 ↗
25. Role of Al addition in modifying microstructure and mechanical properties of Mg-1.0 wt% Ca based alloys10.1016/j.matchar.2020.110608 ↗
26. Precipitation and hardening in magnesium alloys10.1007/s11661-012-1217-2 ↗
27. The Ca-Mg (calcium-magnesium) system10.1007/BF02868900 ↗
28. Microstructure and mechanical properties of non-flammable Mg-8Al-0.3Zn-0.1Mn-0.3Ca-0.2Y alloy subjected to low-temperature, low-speed extrusion10.1016/j.jallcom.2017.12.229 ↗
29. Improving mechanical properties and yield asymmetry in high-speed extrudable Mg-1.1Al-0.24Ca (wt%) alloy by high Mn addition10.1016/j.msea.2017.11.085 ↗
30. Dynamic recrystallization behavior of AZ31-0.5Ca magnesium alloy during warm rolling10.1016/j.msea.2019.138085 ↗
31. Microstructure evolution and deformation behaviors of AZ31 Mg alloy with different grain orientation during uniaxial compression10.1016/j.jallcom.2017.12.312 ↗
32. Dynamic recrystallization kinetics and microstructure evolution of an AZ91D magnesium alloy during hot compression10.1016/j.matchar.2018.08.028 ↗
33. Dynamic recrystallization behavior and hot workability of AZ41M magnesium alloy during hot deformation10.1016/j.jallcom.2016.02.033 ↗
34. Modeling of flow stress for magnesium alloy during hot deformation10.1016/j.msea.2010.01.035 ↗
35. Texture evolution during dynamic recrystallization in a magnesium alloy at 450°C10.1016/j.actamat.2013.12.025 ↗
36. Microstructural and textural evolution of AZ61 magnesium alloy sheet during bidirectional cyclic bending10.1016/j.matchar.2013.03.001 ↗
37. Contribution of extension twinning to plastic strain at low stress stage deformation of a mg-3Al-1Zn alloy10.1016/j.msea.2017.10.038 ↗
38. Hardening evolution of AZ31B Mg sheet10.1016/j.ijplas.2006.03.005 ↗
39. Geometrical criterion for the activation of prismatic slip in AZ61 Mg alloy sheets deformed at room temperature10.1016/j.actamat.2005.01.008 ↗
40. Tension-compression asymmetry and the underlying slip/twinning activity in extruded Mg-Y sheets10.1016/j.ijplas.2020.102878 ↗
41. Mobility of pinned twin boundaries during mechanical loading of extruded binary Mg-1Zn alloy10.1016/j.matchar.2018.02.034 ↗
42. Static recrystallization behavior of multi-directional impact forged Mg-Gd-Y-Zr alloy10.1016/j.jallcom.2019.07.086 ↗
43. Stress-strain hysteresis and strain hardening during cyclic tensile test of Mg-0.6at%Y alloy10.1016/j.msea.2016.10.008 ↗
44. Phase field modeling of discontinuous dynamic recrystallization in hot deformation of magnesium alloys10.1016/j.ijplas.2020.102773 ↗
45. A review of dynamic recrystallization phenomena in metallic materials10.1016/j.matdes.2016.09.012 ↗
46. Dynamic and post-dynamic recrystallization under hot, cold and severe plastic deformation conditions10.1016/j.pmatsci.2013.09.002 ↗
47. Dynamic continuous recrystallization characteristics in two stage deformation of Mg–3Al–1Zn alloy sheet10.1016/S0921-5093(02)00096-5 ↗
48. Dynamic recrystallization during high temperature deformation of magnesium10.1016/j.msea.2008.02.004 ↗
49. Enhanced deformation mechanisms by anisotropic plasticity in polycrystalline Mg alloys at room temperature10.1007/s11661-005-0032-4 ↗
50. Texture weakening of AZ31 magnesium alloy sheet obtained by a combination of bidirectional cyclic bending at low temperature and static recrystallization10.1007/s10853-012-6814-3 ↗
51. Correlation of plastic deformation and dynamic recrystallization in magnesium alloy ZK6010.1016/S1359-6454(01)00020-9 ↗
52. Influence of texture on dynamic recrystallization and deformation mechanisms in rolled or ECAPed AZ31 magnesium alloy10.1016/j.msea.2007.11.024 ↗
53. Modeling of strain hardening and dynamic recrystallization of ZK60 magnesium alloy during hot deformation10.1016/S1003-6326(11)61167-9 ↗
54. Effect of prior strain on continuous recrystallization in AZ31 magnesium alloy after hot deformation10.1016/j.msea.2011.12.066 ↗
55. Dynamic nucleation of new grains in magnesium alloy during hot deformation10.2320/matertrans.44.197 ↗
56. Effect of deformation modes on continuous dynamic recrystallization of extruded AZ31 Mg alloy10.1016/j.jallcom.2021.163086 ↗
57. Flow softening and dynamic recrystallization behavior of a Mg-Gd-Y-Nd-Zr alloy under elevated temperature compressions
58. Modeling of flow behavior and microstructure evolution for Mg-6Gd-5Y-0.3Zr alloy during hot deformation using a unified internal state variable method10.1016/j.jmrt.2020.04.099 ↗
59. Modeling discontinuous dynamic recrystallization containing second phase particles in magnesium alloys utilizing phase field method10.1016/j.commatsci.2021.110858 ↗
60. Enhancement of tensile ductility and stretch formability of AZ31 magnesium alloy sheet processed by cross-wavy bending10.1016/j.jallcom.2013.06.185 ↗
61. Experimental investigation and thermodynamic modeling of the Mg–Cu–Ca ternary system10.1016/j.calphad.2021.102325 ↗
62. Development of low-alloyed and rare-earth-free magnesium alloys having ultra-high strength10.1016/j.actamat.2018.03.002 ↗
63. Grain boundary co-segregation in magnesium alloys with multiple substitutional elements10.1016/j.actamat.2021.116749 ↗