journal article·2023-12

Effects of laser power on the microstructural evolution and mechanical performance in laser dissimilar welding of TC4 to SiCp/6092Al composite

Hongliang Li, Hongyang Cao, Hongbo Xia, Ke Han, Zeyu Wang, Dan Wang, Yunbin Lu

Publisher page

Abstract

In this study, an overlap configuration for Ti6Al4V alloy (TC4) and SiC particle reinforced aluminum matrix composites (AMC) was achieved by laser welding process. The influence of laser power on the microstructural evolution, intermetallic compounds formation and mechanical properties of TC4/AMC joints were investigated. The presence of reinforced phase SiC complicated the metallurgical reaction in the molten pool, resulting in the formation of intermetallic compounds, such as Al 4C 3, TiC, TiAl, and TiAl 3. The influence of laser power was more pronounced on the penetration depth compared to its impact on the weld width. The thickness of Ti Al intermetallic compounds at the TC4/AMC interface increased as the laser power was raised. Abundant dislocations existed surrounding the TiAl 3 phase because of the different thermal-mechanical properties between Al matrix and TiAl 3 phase. The tensile shear force of TC4/AMC joints can be considerably improved by reducing the thickness of the TiAl 3 phase. The maximum tensile shear force of 1675.6 N for the TC4/AMC joint was obtained at a laser power of 1500 W when the thickness of the TiAl 3 layer reached the lowest value of 7.1 μm. The research results have the potential to improve laser welding techniques for TC4/AMC hybrid structures and provide valuable guidance for the design of TC4/AMC welded joints in the future.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Advanced Welding Techniques Analysis · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Self-propagating synthesis joining of Cf/Al composites and TC4 alloy using AgCu filler with Ni–Al–Zr interlayer10.1007/s12598-020-01520-3 ↗
2. Welding and joining of titanium aluminides10.3390/ma7074930 ↗
3. Effect of pulsed laser pretreatment induced pit-structure on the formation of intermetallic compounds in titanium-aluminum dissimilar welded joints10.1016/j.optlastec.2023.109589 ↗
4. Investigation of welding crack in laser welding-brazing welded TC4/6061 and TC4/2024 dissimilar butt joints10.1016/j.jmapro.2020.10.029 ↗
5. Effects of minor Zr addition on the microstructure and mechanical properties of laser welded joint of Al/SiCp metal-matrix composite10.1016/j.jmapro.2019.12.004 ↗
6. In situ SEM study on tensile fractured behavior of Al/steel laser welding-brazing interface10.1016/j.matdes.2022.111320 ↗
7. A theoretical investigation of the effect of Ga alloying on thermodynamic stability, electronic-structure, and oxidation resistance of Ti(2)AlC MAX phase10.1038/s41598-022-17365-y ↗
8. Microstructure and formation mechanism of SHS joining between Cf/Al composites and TiAl intermetallic with Al–Ni–CuO interlayer10.1007/s12598-013-0193-z ↗
9. Effects of joining conditions on microstructure and mechanical properties of Cf/Al composites and TiAl alloy combustion synthesis joints10.1007/s40195-015-0209-9 ↗
10. Vacuum brazing of the gr/2024Al composite and TC4 alloy using AgCuTi filler alloy with Ni-Al interlayer as auxiliary heat source10.1016/j.jallcom.2016.10.049 ↗
11. Electron beam welding of SiCp/Al composite to Ti-6Al-4V10.1179/1432891714Z.0000000001300 ↗
12. Laser welding of TC4 titanium alloy to 7075 aluminum alloy with infinite-shape oscillating beam10.1016/j.optlastec.2022.109044 ↗
13. Laser welding of dissimilar metal joint of 6061 Al alloy and Al matrix composite
14. Microstructure inhomogeneity of dissimilar steel/Al butt joints produced by laser offset welding10.1016/j.jmapro.2020.01.011 ↗
15. Pore formation and melt pool analysis of laser welded Al-cu joints using synchrotron radiation10.1016/j.jmatprotec.2022.117738 ↗
16. Microstructural evolution and characteristics of weld fusion zone in high speed dissimilar welding of Ti and Al10.1007/s12541-015-0274-z ↗
17. Phase equilibria in the Ti–Al binary system10.1016/S1359-6454(00)00118-X ↗
18. Effects of laser welding parameters on the porosity and acicular phase in SiCp/6092 aluminum matrix composite welded joints10.1016/j.jmrt.2023.02.153 ↗
19. Microstructural, porosity and mechanical properties of lap joint laser welding for 5182 and 6061 dissimilar aluminum alloys under different place configurations10.1016/j.matdes.2020.108625 ↗
20. Microstructure and mechanical properties of TC4/6061 and TC4/2024 dissimilar joints by autogenous laser welding-brazing10.1016/j.optlastec.2022.107867 ↗
21. Laser processing of aluminum–titanium-tailored blanks10.1016/j.optlaseng.2004.07.005 ↗
22. Molecular dynamics study on microscale residual stress of graphene/aluminum nanocomposites by selective laser sintering10.1007/s12598-022-02079-x ↗
23. Microstructure and mechanical properties of laser welded-brazed titanium/aluminum joints assisted by titanium mesh interlayer10.1016/j.jmatprotec.2022.117502 ↗
24. Effects of heat input on wettability, interface microstructure and properties of Al/steel butt joint in laser-metal inert-gas hybrid welding-brazing10.1016/j.jmatprotec.2017.11.063 ↗
25. Research on interfacial layer of laser-welded aluminum to titanium10.1016/j.matchar.2019.06.012 ↗
26. Effect of laser-arc offset and laser-deviation angle on the control of a Ti-Al interlayer10.1016/j.jmatprotec.2019.04.010 ↗
27. Tungsten inert gas welding of dissimilar metals aluminum to titanium with aluminum based wire10.1088/2053-1591/ab056f ↗
28. In-situ formation Ti-Al-C compounds reinforced SiCp/2A14 Al joint: microstructure evolution and mechanical properties10.1016/j.optlastec.2022.107896 ↗
29. Laser beam oscillation welded SiCp/2xx Al alloy: microstructure, phase interface and mechanical properties10.1016/j.msea.2021.141482 ↗
30. Study on laser welding of AA1100-16 vol.% B4C metal–matrix composites10.1016/j.compositesb.2011.11.044 ↗
31. Laser penetration welding of an overlap titanium-on-aluminum configuration10.1007/s00170-016-8732-z ↗
32. Microstructure evolution and its effect on the corrosion of dissimilar aluminum alloys friction stir welding joint[J]10.1016/j.corsci.2023.111249 ↗