Hierarchical tungsten-copper composite reinforced by a concrete skeleton of particulate and fibrous tungsten with coherent Cr precipitates in the copper matrix
Source abstract
Abstract
The substitution of a precipitation-hardenable alloy of Cu-0.5wt.%Cr for the widely adopted pure Cu has been proposed for infiltration into the pre-sintered concrete skeleton of particulate and fibrous W. By the reinforcement of a concrete skeleton of particulate and fibrous W along with coherent Cr precipitates in the Cu matrix, the composite exhibited superior comprehensive properties. Specifically, the proposed composite here exhibited a high tensile strength of 601.2 MPa improved by 22.7%, a low friction coefficient of 0.567 decreased by 27.3% and high electrical breakdown strength of 9.07 × 10 7 V/m increased by 101.5%. Notably, due to the precipitation of the coherent Cr particles to lower the solute content in the Cu matrix, the composite exhibited rather good electrical conductivity of 51.4%IACS. The proposed strategy by infiltration of precipitation-hardenable Cu-based alloys into the W skeleton here provides a new clue for the microstructure design and performance enhancement of novel W Cu composites.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Advanced materials and composites · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. Microstructural investigation after vacuum electrical breakdown of the W-30wt.%Cu contact material10.1016/j.vacuum.2018.01.004 ↗
2. Progress, challenges and potentials/trends of tungsten-copper (W Cu) composites/pseudo-alloys: fabrication, regulation and application10.1016/j.ijrmhm.2021.105648 ↗
3. Enhanced mechanical and arc erosion resistant properties by homogenously precipitated nanocrystalline fcc-Nb in the hierarchical W-Nb-Cu composite10.1016/j.compositesb.2018.11.025 ↗
4. The effect of interface stress on the grain boundary grooving in nanomaterials: Application to the thermal degradation of Cu/W nano-multilayers10.1016/j.scriptamat.2021.113866 ↗
5. Persistence of crystal orientations across sub-micron-scale “super-grains” in self-organized cu-W nanocomposites10.1016/j.scriptamat.2020.113677 ↗
6. Electroless copper plating of tungsten powders and preparation of WCu20 composites by microwave sintering10.1016/j.jallcom.2018.06.061 ↗
7. Ultra-rapid processing of high-hardness tungsten–copper nanocomposites10.1016/j.scriptamat.2015.11.012 ↗
8. A novel process for manufacturing copper with size-controlled in-situ tungsten nanoparticles by casting10.1016/j.jmatprotec.2021.117187 ↗
9. Selective laser melting of tungsten-copper functionally graded material10.1016/j.matlet.2018.11.127 ↗
10. W–Cu composites with submicron- and nanostructures: progress and challenges10.1038/s41427-019-0179-x ↗
11. In-situ synthesis of core-shell structure W(WC) composite grains in W-Cu composites fabricated by infiltration10.1016/j.jallcom.2021.158633 ↗
12. Tailoring the microstructure and properties of tungsten-copper composites by minor addition of SiC particles for nuclear fusion reactor application10.1016/j.jnucmat.2020.152220 ↗
13. Novel nanocrystalline W-Cu-Cr-ZrC composite with ultra-high hardness10.1088/1361-6528/ab5d75 ↗
14. Microstructure and properties of ultrafine-grained W-25 wt.%Cu composites doped with CNTs10.1016/j.jmrt.2018.11.003 ↗
15. W-cu composites reinforced by copper coated graphene prepared using infiltration sintering and spark plasma sintering: a comparative study10.1016/j.ijrmhm.2019.03.026 ↗
16. Insight into the microstructure and tensile behavior of the W-Cu composite reinforced with tungsten fibers and particulates10.1002/adem.202000502 ↗
17. Fabrication and properties of the W-30wt.%Cu gradient composite with W@WC core-shell structure10.1016/j.jallcom.2017.03.064 ↗
18. A modification of the rule of mixture in estimating strengths of a composite10.1002/mawe.19820130805 ↗
19. The phase transformation and strengthening of a Cu-0.71 wt% Cr alloy10.1016/j.jallcom.2017.03.069 ↗
20. Microstructure and strength of pure Cu with large grains processed by equal channel angular pressing10.1016/j.matdes.2013.05.029 ↗
21. Mechanical properties of Cu-Cr system alloys with and without Zr and Ag10.1007/s10853-007-2159-8 ↗
22. Influence of tungsten Nanopowders on enhancing the aging behavior of a copper-chromium alloy
23. A study on the sintering of ultrafine grained tungsten with Ti-based additives10.1016/j.ijrmhm.2016.11.013 ↗
24. Theoretical modeling of densification during activated solid-state sintering10.1007/BF02648421 ↗
25. Effect of alloying interlayer on interfacial bond strength of CuW/CuCr integral materials10.1016/j.msea.2010.05.041 ↗
26. Comparison of X-ray and electron backscatter diffraction textures for back-annealed Al–Mg alloys10.1107/S0021889809041685 ↗
27. Precipitation of chromium in copper and copper-nickel base alloys10.1007/BF02669380 ↗
28. Precipitation at coherency loss in Cu-0.35 wt pct Cr10.1007/BF02658413 ↗
29. Accelerated sintering in phase-separating nanostructured alloys10.1038/ncomms7858 ↗
30. Duplex nanocrystalline alloys: entropic nanostructure stabilization and a case study on W-Cr10.1557/jmr.2014.385 ↗
31. On the sequence of clustering and ordering in a meltspun cu-Ti alloy10.1016/S0921-5093(03)00440-4 ↗
32. Spinodal decomposition in age hardening copper-titanium alloys10.1016/0001-6160(75)90125-X ↗
33. Design of stable nanocrystalline alloys10.1126/science.1224737 ↗
34. Nanoscale segregation behavior and high-temperature stability of nanocrystalline W-20at.% Ti10.1016/j.actamat.2014.03.039 ↗
35. About quantitative EBSD analysis of deformation and recovery substructures in pure Tantalum, IOP conference series
36. Some geometrical relations in dislocated crystals10.1016/0001-6160(53)90054-6 ↗
37. Evolution of intragranular stresses and dislocation densities during cyclic deformation of polycrystalline copper10.1016/j.actamat.2015.04.031 ↗
38. Grain size dependent texture evolution in severely rolled pure copper10.1016/j.matchar.2015.02.003 ↗
39. The orientation and strain dependence of dislocation structure evolution in monotonically deformed polycrystalline copper10.1016/j.ijplas.2015.02.005 ↗
40. Fracture toughness of polycrystalline tungsten alloys10.1016/j.ijrmhm.2010.04.007 ↗
41. Extraordinary strain hardening by gradient structure10.1073/pnas.1324069111 ↗
42. Fatigue crack growth in SiC particle reinforced Al alloy matrix composites at high and low R-ratios by in situ X-ray synchrotron tomography10.1016/j.ijfatigue.2014.05.010 ↗
43. Recrystallization kinetics of warm-rolled tungsten in the temperature range 1150-1350 °C10.1016/j.jnucmat.2014.08.037 ↗
44. Dislocation velocities, dislocation densities, and plastic flow in Lithium fluoride crystals10.1063/1.1735121 ↗
45. On the nature of the yield point phenomenon10.1016/j.actamat.2012.12.003 ↗
46. The effect of submicron-sized initial tungsten powders on microstructure and properties of infiltrated W-25wt.% Cu alloys10.1016/j.ijrmhm.2016.05.014 ↗
47. Effect of electron concentration on electrical conductivity in in situ Al-TiB2 nanocomposites10.1063/1.5129817 ↗
48. Facet-dependent trapping and dynamics of excess electrons at anatase TiO2 surfaces and aqueous interfaces10.1038/nmat4672 ↗
49. Interfacial valence electron localization and the corrosion resistance of Al-SiC nanocomposite
50. High-strength and high-conductivity in situ Cu-TiB2 nanocomposites10.1016/j.msea.2021.141952 ↗