In-situ EBSD analysis of microstructural evolution and damage behavior of Mg-Al-Ca-Mn alloys with different extrusion ratios
Source abstract
Abstract
In this study, the Mg-3Al-0.4Ca-0.7Mn (wt%) alloys with three extrusion ratios were produced via hot extrusion. The microstructure and damage behaviors of the alloy were studied by scanning electron microscopy (SEM), transmission electron microscopy (TEM), electron backscattered diffraction (EBSD), and in-situ tensile testing. As the extrusion ratio increased, the texture component was gradually deflected from ED to TD owing to the formation of twins, which resulted in slightly different types of extruded fiber texture. Two kinds of typical damage behaviors were observed in the alloy. One type of crack initiation sites occurred due to twinning-induced grain damage in the specimen with an extrusion ratio of 10. The high-density non-basal dislocations-induced damage predominated the other sample lack of twins with the extrusion ratio of 25. According to the results, the deformation mode and damage behavior in the second case endowed the alloy with the best strength and ductility.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (56)
Show source-provided references
1. Strength and ductility optimization of Mg–Y–Nd–Zr alloy by microstructural design10.1016/j.ijplas.2014.11.003 ↗
2. Effect of texture types on microstructure evolution and mechanical properties of AZ31 magnesium alloy undergoing uniaxial tension deformation at room temperature10.1016/j.msea.2019.138497 ↗
3. Twinning and slip behaviors and microstructural evolutions of extruded Mg-1Gd alloy with rare-earth texture during tensile deformation10.1016/j.jallcom.2019.03.316 ↗
4. Theoretical study on the {1¯ 012} deformation twinning and cracking in coarse-grained magnesium alloys10.1016/j.ijplas.2016.02.001 ↗
5. Grain size effect on tensile properties and slip systems of pure magnesium10.1016/j.actamat.2020.116604 ↗
6. Influence of ca content on microstructure and mechanical properties of extruded Mg–Al–Ca–Mn alloys
7. Effects of initial texture on the three-dimensional creep anisotropic behaviors of dilute Mg–Y binary alloy sheets10.1016/j.msea.2019.138336 ↗
8. Exploring the mechanism of “rare earth” texture evolution in a lean Mg–Zn–Ca alloy10.1038/s41598-019-43415-z ↗
9. Deformation behavior and texture evolution in an extruded MgLi sheet with non-basal texture during tensile deformation10.1016/j.matchar.2019.110041 ↗
10. Enhanced ductility of Mg–1Zn–0.2 Zr alloy with dilute ca addition achieved by activation of non-basal slip and twinning10.1016/j.msea.2021.141128 ↗
11. Tailoring the mechanical properties of Mg–Zn magnesium alloy by calcium addition and hot extrusion process10.1016/j.msea.2020.138929 ↗
12. High-speed extrusion of dilute Mg-Zn-Ca-Mn alloys and its effect on microstructure, texture and mechanical properties10.1016/j.msea.2016.10.007 ↗
13. Texture weakening and ductility variation of Mg–2Zn alloy with CA or RE addition10.1016/j.msea.2015.08.025 ↗
14. Effect of extrusion ratio on microstructure, texture and mechanical properties of indirectly extruded Mg–Zn–Ca alloy10.1016/j.msea.2013.01.052 ↗
15. Effect of deformation temperature on the slip activity in pure Mg and AZX21110.1016/j.jmrt.2022.06.050 ↗
16. Microstructure, texture evolution and tensile properties of extruded Mg-4.58 Zn-2.6 Gd-0.16 Zr alloy10.1016/j.msea.2018.11.142 ↗
17. Effect of extrusion conditions on microstructure, texture, and yield asymmetry in Mg–6Y–7Gd–0.5 wt% Zr alloy10.1016/j.msea.2011.05.075 ↗
18. Modifying microstructures and tensile properties of Mg-Sm based alloy via extrusion ratio10.1016/j.jma.2020.12.004 ↗
19. Microstructure and mechanical properties of as-extruded Mg-Sn-Zn-Ca alloy with different extrusion ratios10.1016/S1003-6326(18)64864-2 ↗
20. The effect of stress state and strain partition mode on the damage behavior of a Mg-Ca alloy10.1016/j.ijplas.2021.103040 ↗
21. Fatigue damage development in extruded Mg-3Al-Zn magnesium alloy10.1016/j.msea.2016.05.009 ↗
22. The evolution of local stress during deformation twinning in a Mg-Gd-Y-Zn alloy10.1016/j.actamat.2021.117452 ↗
23. In-situ analysis of microscopic plastic and failure behaviors of extruded magnesium alloy10.1016/j.msea.2019.02.024 ↗
24. Crack propagation along grain boundaries and twins in Mg and Mg–0.3 at.% Y alloy during in-situ straining in transmission electron microscope10.1016/j.scriptamat.2017.08.023 ↗
25. Cyclic deformation and fatigue damage in single-crystal magnesium under fully reversed strain-controlled tension–compression in the [1 0 1¯ 0] direction10.1016/j.scriptamat.2014.10.020 ↗
26. Notch strength and notch fracture mechanisms of a cast Mg-Gd-Y alloy10.1016/j.msea.2022.142668 ↗
27. An investigation of the deformation and cracking mechanism of Mg–1Al–12Y alloys based on in-situ SEM/EBSD slip trace analysis10.1016/j.msea.2022.144016 ↗
28. Basal slip mediated tension twin variant selection in magnesium WE43 alloy10.1016/j.actamat.2019.03.018 ↗
29. Activation of second-order pyramidal slip and other secondary mechanisms in solid solution Mg-Zn alloys and their effect on tensile ductility10.1016/j.actamat.2022.118555 ↗
30. Identification and analysis of anomalous {101− 2} twins in an extruded Mg-2wt% Y alloy sheet during uniaxial tensile loading10.1016/j.msea.2020.139699 ↗
31. {101¯ 2} twinning mechanism during in situ micro-tensile loading of pure Mg: Role of basal slip and twin-twin interactions
32. Significant disparity of non-basal dislocation activities in hot-rolled highly-textured Mg and Mg-3Al-1Zn alloy under tension10.1016/j.actamat.2021.116691 ↗
33. Inhomogeneous deformation of AZ31 magnesium sheet in uniaxial tension
34. Comparison of edge cracking and tensile cracking in in-situ deformation at 150° C of Mg-2Zn-1.5 Mn alloy sheet10.1016/j.jmst.2021.09.033 ↗
35. Notch strength and notch fracture mechanisms of a cast Mg-Gd-Y alloy10.1016/j.msea.2022.142668 ↗
36. Underlying mechanisms of variation in yield asymmetry and strain hardening behavior of extruded pure Mg with Gd addition
37. Influence of twinning deformation and lattice rotation on strength differential effect in polycrystalline pure magnesium with rolling texture10.1016/j.commatsci.2009.09.009 ↗
38. Observation of non-basal slip in Mg-Y by in situ three-dimensional X-ray diffraction10.1016/j.scriptamat.2017.09.011 ↗
39. Enhanced extra-long life fatigue resistance of a bimodal titanium alloy by laser shock peening10.1016/j.ijfatigue.2020.105868 ↗
40. Comparison on crack propagation under tension at 150° C of Mg-2Zn-1.5 Mn alloy sheets with and without crack notch
41. Twinning, dynamic recrystallization, and crack in AZ31 magnesium alloy during high strain rate plane strain compression across a wide temperature10.1016/j.msea.2018.07.030 ↗
42. The role of {10–12} tensile twinning in plastic deformation and fracture prevention of magnesium alloys10.1016/j.msea.2022.143678 ↗
43. Fracture behavior of magnesium alloys–role of tensile twinning10.1016/j.actamat.2015.04.054 ↗
44. Optimization in strength-ductility of heterogeneous Mg-13Gd alloy via small extrusion ratio combined with pre-aging10.1016/j.msea.2021.142540 ↗
45. Effect of deformation modes on continuous dynamic recrystallization of extruded AZ31 Mg alloy10.1016/j.jallcom.2021.163086 ↗
46. Internal microstructure observation of enhanced grain-boundary sliding at room temperature in AZ31 magnesium alloy10.1016/j.msea.2016.04.030 ↗
47. Predicting grain boundary damage by machine learning10.1016/j.ijplas.2021.103186 ↗
48. Improving ductility of a Mg alloy via non-basal< a> slip induced by Ca addition10.1016/j.ijplas.2019.04.020 ↗
49. Calculation of Schmid factors in magnesium: analysis of deformation behaviors10.1016/j.scriptamat.2012.05.042 ↗
50. Enhanced strength in pure Ti via design of alternating coarse-and fine-grain layers10.1016/j.actamat.2021.116627 ↗
51. Effect of grain boundary segregation on microstructure and mechanical properties of ultra-fine grained Mg–Al–Ca–Mn alloy wires10.1016/j.msea.2022.143423 ↗
52. Highly deformable Mg–Al–Ca alloy with Al2Ca precipitates10.1016/j.actamat.2020.09.006 ↗
53. Weak strengthening effect of the precipitated lamellar phase in the homogenized Mg-8Gd-4Y-1.6 Zn-0.5 Zr (wt%) alloy followed by furnace cooling10.1016/j.msea.2018.08.056 ↗
54. Effects of precipitate shape and orientation on dispersion strengthening in magnesium alloys10.1016/S1359-6462(02)00497-9 ↗
55. Effect of aluminum or zinc solute addition on enhancing impact fracture toughness in Mg–Ca alloys10.1016/j.actamat.2015.11.045 ↗
56. Non-basal dislocation nucleation site of solid solution magnesium alloy10.2320/matertrans.MT-M2020040 ↗