journal article·2023-11

A shortened process of tri-modal microstructure developing in Ti-6Al-4V alloy via electropulsing-induces grain spheroidization

Lai Wei, Xiaofeng Xu, Yang Zhao, Yachong Zhou, Xudong Yan, Zhicheng Wu, Yongqiang Yu, Chao Wu

Publisher page

Abstract

A shortened process combining electropulsing treatment (EPT) and conventional heat treatment (HT) has been applied to develop a tri-modal microstructure in Ti-6Al-4V alloy. The tri-modal microstructure produced by this process has good overall mechanical properties (tensile strength ∼1110 MPa, elongation ∼22.7%). The rapid development of the tri-modal microstructure is attributed to the EPT production of low aspect ratio (LAR) V-poor martensite, which results from the EPT limiting the growth of high-temperature β grains and the diffusion of elements. The α grains decomposed from LAR martensite during the HT process retain a low aspect ratio morphology which can be easily spheroidized. LAR α grains do not undergo phase transformation at two-phase temperature (950 °C) but follow the cylinderization mechanism of spheroidization that relies more on the geometry of the grains than on the high density of dislocation substructures . In this study, the effects of the three types of grains on material strength and ductility are analyzed in detail.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electromagnetic Effects on Materials · Surface Treatment and Residual Stress · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. Characterization of titanium alloy Ti-6Al-4V for chemical, marine and industrial applications10.1016/j.matchar.2003.10.006 ↗
2. Review on titanium and titanium based alloys as biomaterials for orthopaedic applications10.1016/j.msec.2019.04.064 ↗
3. High-strength titanium alloys for aerospace engineering applications: a review on melting-forging process10.1016/j.msea.2022.143260 ↗
4. Factors determining room temperature mechanical properties of bimodal microstructures in Ti-6Al-4V alloy10.1016/j.msea.2018.06.019 ↗
5. Lütjering · 2023
6. Achieving bi-lamellar microstructure with both high tensile strength and large ductility in Ti–6Al–4V alloy by novel thermomechanical processing10.1016/j.mtla.2019.100479 ↗
7. An investigation of a new near-beta forging process for titanium alloys and its application in aviation components10.1016/j.msea.2004.10.016 ↗
8. A new high-temperature deformation strenthening and toughening process for titanium alloys10.1016/S0921-5093(96)10386-5 ↗
9. Low-cycle fatigue behavior and property of TA15 titanium alloy with tri-modal microstructure10.1016/j.msea.2018.08.080 ↗
10. Development of a trimodal microstructure with superior combined strength, ductility and creep-rupture properties in a near alpha titanium alloy10.1016/j.msea.2017.04.068 ↗
11. Tri-modal microstructure in high temperature toughening and low temperature strengthening treatments of near-β forged TA15 Ti-alloy10.1016/j.matchar.2016.10.010 ↗
12. Microstructure characterization and nano & micro hardness of tri-modal microstructure of titanium alloy under different hot working conditions10.1016/j.matchar.2017.10.027 ↗
13. Microstructures and mechanical properties of Ti6Al4V alloy repaired by the technology of point-mode forging and laser repairing10.1016/j.optlastec.2021.107410 ↗
14. Achieving an ideal combination of strength and plasticity in additive manufactured Ti–6.5Al–2Zr–1Mo–1V alloy through the development of tri-modal microstructure10.1016/j.msea.2022.142944 ↗
15. The microstructure and tensile properties of additively manufactured Ti–6Al–2Zr–1Mo–1V with a trimodal microstructure obtained by multiple annealing heat treatment10.1016/j.msea.2021.142241 ↗
16. Globularization using heat treatment in additively manufactured Ti-6Al-4V for high strength and toughness10.1016/j.actamat.2018.09.064 ↗
17. On the thermodynamics and kinetics of electropulsing induced dissolution of β-Mg17Al12 phase in an aged mg–9Al–1Zn alloy10.1016/j.actamat.2009.06.044 ↗
18. Effects of electropulsing on the microstructure and microhardness of a selective laser melted Ti6Al4V alloy10.1016/j.jallcom.2021.160044 ↗
19. Electropulse-induced laminated structures in a ferritic-pearlitic 35CrMo steel10.1016/j.scriptamat.2019.02.008 ↗
20. A novel strategy for preparation of α’ + β dual-phase microstructure through heating massive-like transformation induced by Electropulsing in Ti-6Al-4V alloy10.1016/j.scriptamat.2022.115156 ↗
21. Potential of rapid heat treatment of titanium alloys and steels10.1016/S0921-5093(98)01173-3 ↗
22. Microstructure and mechanical properties of TA15 alloy after thermo-mechanical processing10.1016/j.msea.2018.03.109 ↗
23. Variant selection in additively manufactured alpha-beta titanium alloys10.1016/j.jmst.2021.10.021 ↗
24. Rapid thermokinetics driven nanoscale vanadium clustering within martensite laths in laser powder bed fused additively manufactured Ti6Al4V10.1080/21663831.2020.1772396 ↗
25. Additive manufacturing of strong and ductile Ti–6Al–4V by selective laser melting via in situ martensite decomposition10.1016/j.actamat.2014.11.028 ↗
26. Instability mechanisms in lamellar microstructures10.1016/S1359-6454(99)00378-X ↗
27. Shape instabilities of plate-like structures—I. Experimental observations in heavily cold worked in situ composites10.1016/0001-6160(89)90059-X ↗
28. Formation and evolution of new α grain boundary and its influence on globularization of α lamellae in TC17 alloy10.1016/j.jallcom.2020.156141 ↗
29. Microstructure characterization of hot isostatic pressed Ti–6Al–4V alloy under uniaxial compression and post heat treatment10.1016/j.jmrt.2021.11.132 ↗
30. Effect of electropulsing treatment on static recrystallization behavior of cold-rolled magnesium alloy ZK60 with different reductions10.1016/j.jmst.2018.11.008 ↗
31. Microstructural stability at elevated temperatures10.1016/S0955-2219(99)00094-1 ↗
32. Livingston · 2013
33. Formation of a transition V-rich structure during the α’ to α + β phase transformation process in additively manufactured Ti-6Al-4 V10.1016/j.actamat.2022.118104 ↗
34. A study of the mechanism of α to β phase transformation by tracking texture evolution with temperature in Ti–6Al–4V using neutron diffraction10.1016/j.scriptamat.2005.09.026 ↗
35. In situ observation of texture evolution during α→β and β→α phase transformations in titanium alloys investigated by neutron diffraction10.1016/j.actamat.2007.06.017 ↗
36. Decoupling microlattice metamaterial properties through a structural design strategy inspired by the Hall–Petch relation10.1016/j.actamat.2022.118214 ↗
37. Mechanical properties of fully martensite microstructure in Ti-6Al-4V alloy transformed from refined beta grains obtained by rapid heat treatment (RHT)10.1016/j.scriptamat.2017.05.038 ↗
38. Fatigue crack tip plastic zone of α + β titanium alloy with Widmanstatten microstructure10.1016/j.jmst.2018.03.012 ↗
39. Achieving superior ductility for laser solid formed extra low interstitial Ti-6Al-4V titanium alloy through equiaxial alpha microstructure10.1016/j.scriptamat.2017.11.021 ↗