journal article·2023-12

Importance of cold rolling and tempering on the microstructure evolution, precipitation behavior and mechanical responses of 9Cr3Co3W1Cu ferritic/martensitic steel

Linxi Liu, Liyuan Zhao, Meng Sun, Xiaolin Li, Yingjie Ren, Senhao Hou, Hongbo Yang, Xiangtao Deng, Haifeng Wang

Publisher page

Abstract

The effects of thermomechanical treatment (cold rolling + tempering) on the microstructure evolution, precipitation behavior, and mechanical properties of the 9Cr3Co3W1Cu martensitic steel (G115) were investigated, by adjusting the cold rolling reduction (0, 20% and 40%), tempering temperature (750 °C and 800 °C) and time (30 min and 120 min). The results indicate that the G115 steel with 20% cold-rolling reduction rate followed by tempering at 800 °C for 30 min exhibits the optimum mechanical response (yield strength ( σ s) 899 MPa, elongation ( δ) 26%), compared with that of 40% cold-rolled ( σ s 812 MPa, δ 17%) and undeformed steels ( σ s 670 MPa, δ 15%). The optimum yield strength in 20%-800 °C-30 min steel is attributed to the dislocation strengthening and precipitation strengthening, for the relatively low recrystallization rate and high density Cr 23C 6 and NbC precipitates, and the good ductility is attributed to the low recrystallization ratio and the uniform microstructure. As a comparison, in 40%-800 °C-30 min steel, a ferrite martensite dual phase structure formed. Due to the hardness difference between the two phases, there may be significant inharmony during the deformation process, leading to premature fracture.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Hydrogen embrittlement and corrosion behaviors in metals · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (60)

Show source-provided references
1. Nano-sized MX carbonitrides contribute to the stability of mechanical properties of martensite ferritic steel in the later stages of long-term aging10.1016/j.actamat.2019.06.012 ↗
2. The effect of microstructure evolution on the mechanical properties of martensite ferritic steel during long-term aging10.1016/j.actamat.2017.03.045 ↗
3. Solute-dislocation interactions and creep-enhanced cu precipitation in a novel ferritic-martensitic steel10.1016/j.actamat.2020.05.054 ↗
4. Phase transformation behavior and microstructural control of high-Cr martensitic/ferritic heat-resistant steels for power and nuclear plants: a review10.1016/j.jmst.2014.12.001 ↗
5. Materials for ultra-supercritical coal-fired power plant boilers10.1016/j.ijpvp.2006.08.006 ↗
6. Materials for ultrasupercritical coal power plants-boiler materials: part 110.1361/105994901770345394 ↗
7. Effect of microstructural evolution on high-temperature strength of 9Cr-3W-3Co martensitic heat resistant steel under different aging conditions10.1016/j.msea.2013.09.033 ↗
8. Effect of normalizing temperature on the strength of 9Cr-3W-3Co martensitic heat resistant steel10.1016/j.msea.2013.12.068 ↗
9. Nanoindentation investigation on the creep behavior of P92 steel weld joint after creep-fatigue loading10.1016/j.ijfatigue.2020.105506 ↗
10. High-temperature oxidation behavior of modified 4Al alumina-forming austenitic steel: effect of cold rolling10.1016/j.jmst.2020.08.013 ↗
11. Evolution of the microstructure in aged G115 steels with the different concentration of tungsten10.1016/j.msea.2018.05.068 ↗
12. Effect of boron on G115 martensitic heat resistant steel during aging at 650 °C10.1016/j.msea.2020.139529 ↗
13. Effect of normalizing temperature on microstructural stability and mechanical properties of creep strength enhanced ferritic P91 steel10.1016/j.msea.2016.01.066 ↗
14. Microstructure evolution and fracture mechanism of a novel 9Cr tempered martensite ferritic steel during short-term creep10.1016/j.msea.2017.09.086 ↗
15. On the contribution of carbides and micrograin boundaries to the creep strength of tempered martensite ferritic steels10.1016/j.actamat.2006.08.046 ↗
16. On laves phase in a 9Cr3W3CoB martensitic heat resistant steel when aged at high temperatures10.1016/j.jmst.2020.12.062 ↗
17. Creep behavior and stability of MX precipitates at high temperature in 9Cr–0.5Mo–1.8W–VNb steel10.1016/S0921-5093(01)00973-X ↗
18. Creep-strengthening of steel at high temperatures using nano-sized carbonitride dispersions10.1038/nature01740 ↗
19. Effect of W addition on the low cycle fatigue behavior of high Cr ferritic steels10.1016/S0921-5093(00)01291-0 ↗
20. Importance of austenitization temperature and ausforming on creep strength in 9Cr ferritic/martensitic steel10.1016/j.scriptamat.2018.04.038 ↗
21. A physically-based high temperature yield strength model for 9Cr steels10.1016/j.msea.2018.05.086 ↗
22. Effects of cu-rich phases on microstructure evolution and creep deformation behavior of a novel martensitic heat-resistant steel G11510.1016/j.msea.2022.143937 ↗
23. Mapping the parent austenite orientation reconstructed from the orientation of martensite by EBSD and its application to ausformed martensite10.1016/j.actamat.2010.08.001 ↗
24. Variant selection of lenticular martensite by ausforming10.1016/j.scriptamat.2012.05.007 ↗
25. Creep behavior, microstructure evolution and fracture mechanism of a novel martensite heat resistance steel G115 affected by prior cold deformation10.1016/j.msea.2022.143564 ↗
26. Diffusion of tungsten in α-iron10.1080/14786430600732093 ↗
27. The estimation of dislocation densities in metals from X-ray data10.1016/0001-6160(53)90106-0 ↗
28. Improving mechanical properties of laminate heterogeneous GW103K/AZ31 alloys10.1016/j.jallcom.2023.169156 ↗
29. Orientation gradients and geometrically necessary dislocations in ultrafine grained dual-phase steels studied by 2D and 3D EBSD10.1016/j.msea.2010.01.004 ↗
30. Effect of reduction in area per pass on strain distribution and microstructure during caliber rolling in twinning-induced plasticity steel10.1007/s42243-019-00260-8 ↗
31. Geometrically necessary dislocations and strain gradient plasticity––a dislocation dynamics point of view10.1016/S1359-6462(02)00341-X ↗
32. Indentation size effects in crystalline materials: a law for strain gradient plasticity10.1016/S0022-5096(97)00086-0 ↗
33. On the nucleation of laves phase particles during high-temperature exposure and creep of tempered martensite ferritic steels10.1016/j.actamat.2014.08.008 ↗
34. Precipitate design for creep strengthening of 9% Cr tempered martensitic steel for ultra-supercritical power plants10.1088/1468-6996/9/1/013002 ↗
35. Study on the creep deformation behavior and characterization of 9Cr-1Mo-V-Nb steel at elevated temperatures10.1016/j.matchar.2018.10.011 ↗
36. High temperature strengthening in 12Cr-W-Mo steels by controlling the formation of Delta ferrite10.1007/s11661-014-2411-1 ↗
37. Microstructure evolution in a 3%co modified P911 heat resistant steel under tempering and creep conditions10.1016/j.msea.2010.10.006 ↗
38. Orientation relationships in precipitation systems10.1016/0001-6160(82)90045-1 ↗
39. New orientation relationship with low interfacial energy in MC/ferrite system observed in Nb-Ti bearing steel during isothermal quenching process10.1016/j.scriptamat.2019.01.008 ↗
40. Über den Mechanismus der Stahlhärtung10.1007/BF01397346 ↗
41. Krauss · 2005
42. Bhadeshia · 2006
43. Defect tolerant fatigue assessment of AM materials: size effect and probabilistic prospects10.1016/j.ijfatigue.2022.106884 ↗
44. Strengthening mechanisms of creep resistant tempered martensitic steel10.2355/isijinternational.41.641 ↗
45. 9 - development of creep-resistant steels and alloys for use in power plants
46. Courtney · 1990
47. Hydrogen embrittlement behavior of SUS301L-MT stainless steel laser-arc hybrid welded joint localized zones10.1016/j.corsci.2019.108337 ↗
48. Discontinuous dynamic recrystallization and nucleation mechanisms associated with 2-, 3- and 4-grain junctions of polycrystalline nickel-based superalloys10.1016/j.matdes.2023.112041 ↗
49. Martensite in steel: strength and structure10.1016/S0921-5093(99)00288-9 ↗
50. Substitutional solution hardening10.1016/0001-6160(63)90213-X ↗
51. A statistical theory of solid solution hardening10.1002/pssb.19700410221 ↗
52. Modelling solid solution hardening in high entropy alloys10.1016/j.actamat.2014.11.014 ↗
53. Multi-component solid solution hardening10.1007/BF00540988 ↗
54. Solid solution hardening of copper crystals10.1007/BF00552938 ↗
55. Gladman · 1997
56. Precipitation hardening in metals10.1179/026708399773002782 ↗
57. Carbide precipitation in ferrite in Nb–V-bearing low-carbon steel during isothermal quenching process10.1007/s40195-017-0632-1 ↗
58. Structure–property optimization of ultrafine-grained dual-phase steels using a microstructure-based strain hardening model10.1016/j.actamat.2006.11.029 ↗
59. Probabilistic framework for fatigue life assessment of notched components under size effects10.1016/j.ijmecsci.2020.105685 ↗
60. Size effect in fatigue modelling of defective materials: application of the calibrated weakest-link theory10.1016/j.ijfatigue.2022.107213 ↗