Thermal fatigue behavior of two commercial Hot Work Tool Steels (PHTS-1, 2) (PHTS: Premium grade Hot Work Tool Steel) under cyclic heating (25 °C ∼ 700 °C, 3000 cycles) was investigated. Precipitation behavior of MC, M 23C 6, and M 6C carbides was characterized (initial stage of precipitation, site (PAG, packet, block, lath), size, fraction) in relation to thermal fatigue behavior. Especially, it focused on coarse V-rich MC carbide at grain boundaries. For suppressing coarse MC, it is suggested to modify contents of carbide former (decreasing MC former) and forging conditions (dissolution of MC and removing of macro-segregation band of V, C). And then thermal fatigue resistance was improved with suppressing coarse MC by modifying forging condition (SeAH-VD steel).
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Metal Alloys Wear and Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (66)
Show source-provided references
1. 2016
2. Tool steels
3. Methodology of high-speed steels design using the artificial intelligence tools
4. Materials design: the key to modern steel products
5. Simulation and evaluation of thermal fatigue cracking of hot work tool steels10.1016/j.ijfatigue.2004.03.005 ↗
6. Computer modeling and prediction of thermal fatigue cracking in die-casting tooling10.1016/S0043-1648(03)00281-3 ↗
7. Intermetallic formation and its relation to interface mass loss and tribology in die casting dies10.1016/j.wear.2003.08.001 ↗
8. Intermetallic compound layer growth between solid iron and molten aluminium10.1016/S0921-5093(98)00573-5 ↗
9. An evaluation of metallic coatings for erosive wear resistance in die casting applications10.1016/0043-1648(95)06749-3 ↗
10. Bhushan · 1991
11. 1995
12. Thermal fatigue testing of chromium martensitic hot-work tool steel after different austenitizing treatments10.1016/j.jmatprotec.2004.04.158 ↗
13. The influence of austenitizing and tempering temperature on the hardness and fracture toughness of hot-worked H11 tool steel10.1016/j.jmatprotec.2006.04.016 ↗
14. The effect of the addition of alloying elements on carbide precipitation and mechanical properties in 5% chromium martensitic steels10.1016/j.actamat.2007.05.004 ↗
15. Effect of substructure on mechanical properties and fracture behavior of lath martensite in 0.1 C–1.1 Si–1.7 Mn steel10.1016/j.jallcom.2016.03.100 ↗
16. The effects of alloying elements on thermal fatigue and thermal shock resistance of the HSLA cast steels10.2355/isijinternational.40.1164 ↗
17. Bone-like crack resistance in hierarchical metastable nanolaminate steels10.1126/science.aal2766 ↗
18. Thermal fatigue cracking of surface engineered hot work tool steels10.1016/j.surfcoat.2004.04.053 ↗
19. Thermal fatigue behavior of nitrocarburized and low pressure nitrided modified JIS SKD61 hot work mold steel10.2320/matertrans.M2013035 ↗
20. Enhancement of thermal cracking and mechanical properties of H13 tool steel by shot peening treatment10.1179/026708409X12490360425882 ↗
21. Overview of heat treatment and surface engineering, influences of surface finishing on hot–work tool steel
22. Correlation of yield strength and tensile strength with hardness for steels10.1007/s11665-008-9225-5 ↗
23. Development of a method for extracting fracture toughness from instrumented Charpy impact tests in the ductile and transition regimes10.1016/j.tafmec.2021.103080 ↗
24. Tempering of steel, metallurgical
25. The behavior of structural steels at elevated temperatures and the design of fire resistant steels10.2320/matertrans.42.1913 ↗
26. Hardness of tempered martensite in carbon and low-alloy steels10.1007/BF02646882 ↗
27. IG fracture at elevated temperature10.1016/0001-6160(75)90047-4 ↗
28. Creep cavitation in metals10.1016/S0749-6419(02)00111-0 ↗
29. The mechanism of stress-relief cracking in a ferritic alloy steel
30. Stress-relief cracking of a copper-containing HSLA steel
31. Bailey · 1994
32. Effects of strain and grain size on carbide precipitation and corrosion sensitization behavior in 304 stainless steel10.1016/S1359-6454(97)00106-7 ↗
33. Predicting IGSCC/IGA susceptibility of Ni-Cr-Fe alloys by modeling of GB chromium depletion10.1016/S0921-5093(97)00110-X ↗
34. Issues concerning the effects of applied tensile stress on intergranular segregation in a low alloy steel10.1016/1359-6454(95)00249-9 ↗
35. A study of stress relief cracking in 214Cr 1 Mo steel—I. The effects of P segregation10.1016/0001-6160(80)90104-2 ↗
36. Study on grain boundary character and strain distribution of intergranular cracking in the CGHAZ of T23 steel10.1016/j.matchar.2013.08.004 ↗
37. Dependence of intergranular fatigue cracking on the interactions of persistent slip bands with grain boundaries10.1016/S1359-6454(02)00399-3 ↗
38. Elevated temperature intergranular cracking in heat-resistant steels10.1016/j.msea.2012.09.007 ↗
39. Corrosion and stress corrosion cracking in supercritical water10.1016/j.jnucmat.2007.05.017 ↗
40. Stress criterion for fatigue fracture of steels10.1016/0022-5096(60)90011-9 ↗
41. Inclusion initiated fracture under cyclic torsion very high cycle fatigue at different load ratios10.1016/j.ijfatigue.2019.01.015 ↗
42. Changes in morphology and composition of carbides during cyclic deformation at room and elevated temperature and their effect on mechanical properties of Cr Mo V steel10.1016/0001-6160(85)90174-9 ↗
43. Tool steels
44. Effects of vanadium content on the carbides transformation and strengthening mechanism of MPS700V hot-work die steel at room and elevated temperatures10.1016/j.msea.2021.141091 ↗
45. The tempering of 2.25 Cr%-1% Mo steel after quenching and normalizing
46. Coherent to incoherent transition of precipitates during rupture test in TP347H austenitic stainless steels10.1016/j.matchar.2016.03.018 ↗
47. Effects of vanadium content on the carbides transformation and strengthening mechanism of MPS700V hot-work die steel at room and elevated temperatures10.1016/j.msea.2021.141091 ↗
48. Tensile behavior of ferrite-martensite dual phase steels with nano-precipitation of vanadium carbides10.2355/isijinternational.ISIJINT-2015-106 ↗
49. Effect of solid solution elements on solubility products of carbides and nitrides in austenite: thermodynamic calculations10.1007/s11661-019-05295-w ↗
50. Creep properties of 16Cr-14Ni stainless steel bearing carbon and vanadium10.2355/tetsutohagane1955.64.3_469 ↗
51. Cutting performance and microstructure of high speed steels: contributions of matrix strengthening and undissolved carbides10.1007/s11661-998-0173-3 ↗
52. Solution treatment effects in AF1410 steel
53. Controlling the MC and M2C carbide precipitation in Ferrium M54 steel to achieve optimum ultimate tensile strength/fracture toughness balance10.1016/j.matchar.2018.03.041 ↗
54. Relationship between microstructure and mechanical properties of a 5% Cr tempered martensitic tool steel10.1016/j.msea.2004.02.073 ↗
55. Influence of silicon content on the precipitation of secondary carbides and fatigue properties of a 5% Cr tempered martensitic steel10.1016/j.msea.2004.11.050 ↗
56. Effect of silicon on carbide precipitation after tempering of H11 hot work steels10.1007/s11661-010-0430-0 ↗
57. Determination of carbide and matrix compositions in high-speed steels by analytical electron microscopy10.1007/BF02670163 ↗
58. An atom probe study of secondary hardening in high speed steels10.1016/0001-6160(88)90136-8 ↗
59. Influence of thermal homogenization treatment on structure and impact toughness of H13 ESR steel10.1016/S1006-706X(10)60011-8 ↗
60. AP-FIM study on the effect of Mo addition on microstructure in Ti-Nb steel10.1016/0169-4332(94)90351-4 ↗
61. The effect of molybdenum on interphase precipitation and microstructures in microalloyed steels containing titanium and vanadium10.1016/j.actamat.2018.09.008 ↗
62. Improved the microstructures and properties of M3: 2 high-speed steel by spray forming and niobium alloying10.1016/j.matchar.2016.04.010 ↗
63. The structure and properties of W–Mo–V high-speed steels with increased contents of Si and Nb after heat treatment10.1016/S0924-0136(97)00416-0 ↗
64. Carbide precipitation and high-temperature strength of hot-rolled high-strength, low-alloy steels containing Nb and Mo10.1007/s11661-002-0178-2 ↗
65. Fractography survey on high cycle fatigue failure: crack origin characterisation and correlations between mechanical tests and microstructure in Fe–C–Cr–Mo–X alloys10.1016/j.ijfatigue.2006.06.012 ↗
66. Improved red hardness and toughness of hot work die steel through tungsten alloying10.1007/s11665-021-05793-2 ↗