Modulation of microstructure and improvement in the mechanical properties of TiBw/Ti65 composites by rolling at different temperatures
Source abstract
Abstract
The effect of rolling temperature on microstructure evolution and mechanical properties of as-sintered TiBw/Ti65 composites was systematically investigated. The results showed that at 900 °C (in the low α + β phase region), the matrix microstructure primarily exhibited a deformation structure. At 1000 °C (in the high α + β phase region), a bimodal structure was observed, and at 1100 °C (in the β phase region), a basket-weave structure emerged. Additionally, silicides precipitated at 900 °C were fine but grew and coarsened at 1000 °C, eventually dissolving almost completely into the matrix at 1100 °C. This behavior is attributed to the varying solubility of silicides in the α and β phases. With increasing rolling temperature, the dynamic recrystallization (DRX) mechanism within the TiBw/Ti65 composites transitioned from continuous dynamic recrystallization (CDRX) to discontinuous dynamic recrystallization (DDRX). Rolling significantly enhanced the mechanical properties of the composites. The HR-900 composite exhibited the optimal strength-plasticity combination at room temperature, achieving an ultimate tensile strength (UTS) of 1415 ± 21 MPa and elongation (EL) of 6.2 ± 2.7%, mainly due to grain refinement and work hardening. Conversely, the HR-1100 composite demonstrated superior high-temperature mechanical performance, showing improvements of 37.18%, 27.05%, and 9.59% at 963 MPa (650 °C), 789 MPa (700 °C), and 560 MPa (750 °C), respectively, compared to those of the as-sintered materials. The strengthening mechanisms were fine-grain strengthening, dislocation strengthening, and load transfer strengthening of the as-rolled composites, and the primary strengthening mechanism shifts from dislocation to fine-grain strengthening as the rolling temperature increases.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Intermetallics and Advanced Alloy Properties · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (57)
Show source-provided references
1. Perspectives on titanium science and technology10.1016/j.actamat.2012.10.043 ↗
2. In-situ manipulation of TiB whisker orientation and investigation of its high-temperature mechanical properties in titanium matrix composites10.1016/j.compositesb.2023.111165 ↗
3. Influence of thermomechanical processing and heat treatment on microstructure, tensile properties and fracture toughness of Ti-1100-0.1B alloy10.1016/j.jallcom.2013.11.014 ↗
4. Tensile and creep properties of thermomechanically processed boron modified Timetal 834 titanium alloy10.1016/j.msea.2011.05.069 ↗
5. Recent advances in silicon containing high temperature titanium alloys10.1016/j.jmrt.2021.08.117 ↗
6. TiB whiskers reinforced high temperature titanium Ti60 alloy composites with novel network microstructure10.1016/j.matdes.2013.04.048 ↗
7. Microstructure and texture variations in high temperature titanium alloy Ti65 sheets with different rolling modes and heat treatments10.3390/ma13112466 ↗
8. Effects of extrusion on microstructure and tensile properties of 3D network structured TiBw/Ti60 composites fabricated by reaction hot pressing10.1016/j.jallcom.2013.08.095 ↗
9. Strain induced additional growth and high integrity of TiB-whiskers in titanium matrix composite: intrinsic mechanisms and superior strengthening effects10.1088/2053-1591/ab406d ↗
10. The effects of sintering temperature on mechanical and electrical properties of Al2O3/Ti composites
11. Direct energy deposition of SiC reinforced Ti–6Al–4V metal matrix composites: structure and mechanical properties10.1016/j.ceramint.2022.08.097 ↗
12. Aligned TiB whiskers in TiB/Ti6Al4V composites manipulated by spark plasma sintering and hot extrusion: in-situ rotation and strengthening mechanism10.1016/j.msea.2022.144264 ↗
13. Evolution of microstructural characteristic and tensile properties during preparation of TiB/Ti composite sheet
14. Fabrication of TiB-reinforced titanium matrix composite via spark plasma sintering and vertical bidirectional reactive hot rolling10.1016/j.matchar.2023.113450 ↗
15. Effect of heat treatment on microstructure evolution and mechanical properties of selective laser melted Ti–6Al–4V and TiB/Ti–6Al–4V composite: a comparative study10.1016/j.msea.2020.140415 ↗
16. Microstructure evolution during hot-packed rolling and mechanical properties anisotropy of as-rolled network-structured TiBw/TA15 composites10.1016/j.msea.2022.143518 ↗
17. Superior superplasticity and multiple accommodation mechanisms in TiB reinforced near-α titanium matrix composites10.1016/j.compositesb.2022.109940 ↗
18. Microstructures and mechanical properties of hot indirect extruded in situ (TiB + TiC)/Ti6Al4V composites: effect of extrusion temperature10.1016/j.msea.2021.140988 ↗
19. Effect of multi-directional forging on the microstructure and mechanical properties of TiBw/TA15 composite with network architecture10.1016/j.matdes.2017.08.055 ↗
20. Microstructure characteristics and enhanced properties of network-structured TiB/(TA15-Si) composites via rolling deformation at different temperatures10.1016/j.msea.2021.142176 ↗
21. Effects of direct rolling deformation on the microstructure and tensile properties of the 2.5vol% (TiBw+TiCp)/Ti composites10.1016/j.msea.2016.12.113 ↗
22. A review of dynamic recrystallization phenomena in metallic materials10.1016/j.matdes.2016.09.012 ↗
23. Dynamic and post-dynamic recrystallization under hot, cold and severe plastic deformation conditions10.1016/j.pmatsci.2013.09.002 ↗
24. Microstructure evolution and properties of powder metallurgy Ti43Al9V0.3Y alloy sheets at different rolling temperatures10.1016/j.msea.2023.144685 ↗
25. The α phase recrystallization mechanism and mechanical properties of a near-α titanium matrix composite10.1016/j.intermet.2022.107597 ↗
26. Texture evolution and the recrystallization behavior in a near β titanium alloy Ti-7333 during the hot-rolling process10.1016/j.matchar.2019.109999 ↗
27. The impact of matrix texture and whisker orientation on property anisotropy in titanium matrix composites: experimental and computational evaluation10.1016/j.compositesb.2021.108682 ↗
28. Improved tensile properties of a novel near-α titanium alloy via tailoring microstructure by hot-rolling10.1016/j.msea.2020.139588 ↗
29. Orientation dependent behavior of tensile-creep deformation of hot rolled Ti65 titanium alloy sheet10.1016/j.jmst.2020.10.021 ↗
30. Li · 2020
31. Effect of boron on microstructure and mechanical properties of thermomechanically processed near alpha titanium alloy Ti-110010.1016/j.jallcom.2011.02.114 ↗
32. Effect of volume fraction of reinforcement on room temperature tensile property of in situ (TiB+TiC)/Ti matrix composites10.1016/j.matdes.2004.11.030 ↗
33. Creep rupture property of in situ synthesized (TiB+La2O3)/Ti composite10.1016/j.msea.2007.11.028 ↗
34. The effect of rolling temperature on the microstructure and mechanical properties of 5 vol.% (TiBw+TiCp)/Ti composites10.1007/s11837-019-03972-0 ↗
35. Towards high strengthening efficiency by in-situ planting nano-TiB networks into titanium matrix composites10.1016/j.compositesb.2022.110169 ↗
36. Insight into the formation mechanism and interaction of matrix/TiB whisker textures and their synergistic effect on property anisotropy in titanium matrix composites10.1016/j.jmst.2021.08.033 ↗
37. Synergistic strengthening behavior and microstructural optimization of hybrid reinforced titanium matrix composites during thermomechanical processing10.1016/j.matchar.2020.110527 ↗
38. Effect of TiB, TiC and Y2O3 on tensile properties and creep behavior at 650 °C of titanium matrix composites10.1016/j.jallcom.2022.164699 ↗
39. Constructing tri-modal microstructure via new three-step heat treatments for improved tensile strength and creep resistance in (TiB+TiC+Y2O3)/α-Ti composite10.1016/j.msea.2023.145808 ↗
40. Printability, microstructures and mechanical properties of a novel co-based superalloy fabricated via laser powder bed fusion10.1016/j.jmst.2023.10.062 ↗
41. Effects of yttrium content on solidification, microstructure, and mechanical properties of laser powder bed fused IN718 superalloy10.1016/j.jallcom.2023.173404 ↗
42. High-temperature tensile properties and strengthening mechanism of cryo-rolled MP159 superalloy strengthened by deformation nano-twins10.1016/j.matchar.2024.113692 ↗
43. Comparison study of microstructure and mechanical properties of standard and direct-aging heat treated superalloy Inconel 70610.1016/j.msea.2022.142836 ↗
44. Precipitation behavior of silicide and synergetic strengthening mechanisms in TiB-reinforced high-temperature titanium matrix composites during multi-directional forging[J]10.1016/j.jallcom.2021.159051 ↗
45. Microstructure evolution and deformation mechanisms of β phase in TiBw/Ti60 composites studied by reconstructing grain during the hot deformation10.1016/j.jallcom.2020.153872 ↗
46. Dynamic recrystallization mechanism and improved mechanical properties of a near α high temperature titanium alloy processed by severe plastic deformation10.1016/j.matchar.2020.110281 ↗
47. The hyperbolic constitutive equations and modified dynamic material model of TiBw/Ti-6.5Al-2.5Zr-1Mo-1V-0.5Si composites10.1016/j.msea.2019.138329 ↗
48. The double-edge effect of second-phase particles on the recrystallization behaviour and associated mechanical properties of metallic materials10.1016/j.pmatsci.2017.10.004 ↗
49. Particulate induced dynamic globularization/recrystallization and unique superplasticity in TiB/near-α Ti matrix composites10.1016/j.matchar.2020.110458 ↗
50. Enhancing microstructure refinement and strengthening efficiency of TiBw/near α-Ti composites by combining solid-solution treatment with hot processing10.1016/j.compositesb.2023.110696 ↗
51. Enhanced strength-ductility synergy in fiber-like structural titanium matrix composites by controlling TiB content10.1016/j.jallcom.2022.165399 ↗
52. Effects of degree of deformation on the microstructure, mechanical properties and texture of hybrid-reinforced titanium matrix composites10.1016/j.actamat.2012.01.032 ↗
53. Strengthening mechanisms in an Al-Fe-Cr-Ti nano-quasicrystalline alloy and composites10.1016/j.msea.2016.07.007 ↗
54. Chapter 7 - strengthening mechanisms and super-strength of severely deformed titanium10.1016/B978-0-12-814599-9.00007-9 ↗
55. A TiB whisker-reinforced titanium matrix composite with controllable orientation: a novel method and superior strengthening effect10.1016/j.msea.2021.142309 ↗
56. Properties and deformation behaviour of mg–Y2O3 nanocomposites10.1016/j.actamat.2007.05.032 ↗
57. Investigation on the microstructure, room and high temperature mechanical behaviors and strengthening mechanisms of the (TiB+TiC)/TC4 composites10.1016/j.jallcom.2017.08.017 ↗