journal article·2022-12

Segregation-modified interfacial strength and deformation mechanism at SiCp/2009Al composite interface

Xiaolei Guo, Wenfu Liu, Junhui Nie, Jun Song, Shule Xing, Peng Shi

Publisher page

Abstract

The reinforcement/matrix interface is a crucial factor affecting the mechanical performance of metal matrix composites (MMCs). However, it is difficult to quantitatively characterize the correlation between interfacial microstructure and mechanical properties, especially between interfacial segregation and interfacial strength. In this study, composite micro-pillars containing a single slanted interface with Mg segregation were fabricated in engineering SiCp/2009Al composites produced by the powder metallurgy technique (PMT). Upon uniaxial compression, changes in interfacial deformation behavior depended on the Mg segregation amount. Specifically, as the segregation amount increased, the interfacial shear strength increased from 174.5 MPa to 230 MPa, and the misorientation angles of the interfacial micro-region increased from 1.2 ± 0.5° to 8.8 ± 5.6°. It was demonstrated that the Mg segregation in the SiC/Al interface can considerably enhance interfacial adhesion by improving interfacial wettability, and the interfacial micro-region with stronger interfacial adhesion can endure more external strain through grain fragmentation.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (63)

Show source-provided references
1. A study of advancement in application opportunities of aluminum metal matrix composites10.1016/j.matpr.2020.02.516 ↗
2. Characterization of Al-7075 metal matrix composites: a review10.1016/j.jmrt.2017.10.012 ↗
3. Fabrication and the mechanical and physical properties of nanocarbon-reinforced light metal matrix composites: a review and future directions10.1016/j.msea.2021.141542 ↗
4. Interface interaction and synergistic strengthening behavior in pure copper matrix composites reinforced with functionalized carbon nanotube-graphene hybrids10.1016/j.carbon.2019.02.048 ↗
5. Finite element modeling and simulation of the fiber–matrix interface in fiber reinforced metal matrix composites10.1016/j.matpr.2020.06.160 ↗
7. Interfacial superstructures and chemical bonding transitions at metal-ceramic interfaces10.1126/sciadv.abf6667 ↗
8. Metal matrix composites reinforced by nano-particles-a review10.3390/met4010065 ↗
9. Influence of spark plasma sintering temperature on the microstructure and strengthening mechanisms of discontinuous three-dimensional graphene-like network reinforced Cu matrix composites10.1016/j.msea.2019.04.032 ↗
10. Molecular-dynamics simulation of Al/SiC interface structures10.1103/PhysRevB.59.10125 ↗
11. Carbon nanotube-reinforced aluminum matrix composites10.1002/adem.201901176 ↗
12. Particle size effect on the interfacial properties of SiC particle-reinforced Al-Cu-Mg composites10.1016/j.msea.2017.11.068 ↗
13. Tensile and fracture properties of 15 vol% SiCp/2009Al composites fabricated by hot isostatic pressing and hot extrusion processes10.1007/s40195-014-0127-2 ↗
14. Interfacial segregation and precipitates behavior in the ultrafine grained Al-based metal matrix composites10.1016/j.jallcom.2018.08.183 ↗
15. Influence of interfaces on the mechanical behavior of SiC particulate-reinforced Al–Zn–Mg–Cu composites10.1016/j.msea.2015.07.050 ↗
16. Metal-ceramic interfaces studied with high-resolution transmission electron microscopy10.1016/S1359-6454(99)00268-2 ↗
17. Effects of SiC particle size on mechanical properties of SiC particle reinforced aluminum metal matrix composite10.1016/j.msea.2019.03.037 ↗
18. Interface coupling and energy storage of inorganic–organic nanocomposites10.1039/D2TA02900F ↗
19. Plasticity in small-sized metallic systems: intrinsic versus extrinsic size effect10.1016/j.pmatsci.2011.01.005 ↗
20. Size dependence of mechanical properties of gold at the micron scale in the absence of strain gradients10.1016/j.actamat.2004.12.031 ↗
21. Nanoscale gold pillars strengthened through dislocation starvation10.1103/PhysRevB.73.245410 ↗
22. Micro-compression studies of face-centered cubic and body-centered cubic high-entropy alloys: size-dependent strength, strain rate sensitivity, and activation volumes10.1016/j.msea.2020.139429 ↗
23. Microstructure versus size: nano/microscale deformation of solute-strengthening Al alloys via pillar compression tests10.1080/21663831.2018.1553802 ↗
24. Grain boundary sliding in aluminum nano-bi-crystals deformed at room temperature10.1002/smll.201301060 ↗
25. In situ TEM tensile testing of bicrystals with tailored misorientation angles10.1016/j.actamat.2021.117505 ↗
26. Micropillar compression of Al/SiC nanolaminates10.1016/j.actamat.2010.08.025 ↗
27. High temperature micropillar compression of Al/SiC nanolaminates10.1016/j.actamat.2013.04.013 ↗
28. Anisotropy, size, and aspect ratio effects on micropillar compression of AlSiC nanolaminate composites10.1016/j.actamat.2016.05.018 ↗
29. Deformation and strengthening of SiC reinforced Al-MMCs during in-situ micro-pillar compression10.1016/j.msea.2019.138141 ↗
30. Interfacial strength and deformation mechanism of SiC–Al composite micro-pillars10.1016/j.scriptamat.2015.11.018 ↗
31. Effect of hot pressing temperature on microstructure and tensile properties of SiC/Al-Zn-Mg-Cu composites
32. An enhanced continuum model for size-dependent strengthening and failure of particle-reinforced composites10.1016/j.actamat.2009.08.010 ↗
33. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
34. Sample dimensions influence strength and crystal plasticity10.1126/science.1098993 ↗
35. Strengthening and toughening mechanisms in graphene-Al nanolaminated composite micro-pillars10.1016/j.actamat.2016.11.043 ↗
36. Compressive properties of interface-containing Cu–Fe nano-pillars10.1016/j.scriptamat.2011.11.008 ↗
37. Structural phase transformations in metallic grain boundaries10.1038/ncomms2919 ↗
38. Helium implantation effects on the compressive response of Cu nanopillars10.1002/smll.201201614 ↗
39. Stochastic nature of plasticity of aluminum micro-pillars10.1016/j.actamat.2007.12.016 ↗
40. Dislocation avalanches, strain bursts, and the problem of plastic forming at the micrometer scale10.1126/science.1143719 ↗
41. Interface-dominated mechanical behavior in advanced metal matrix composites10.1016/j.nanoms.2020.03.007 ↗
42. Two-dimensional misorientation mapping by rocking dark-field transmission electron microscopy10.1016/j.ultramic.2015.07.003 ↗
43. Misorientation-angle-dependent electrical transport across molybdenum disulfide grain boundaries10.1038/ncomms10426 ↗
44. In-situ synthesis, microstructure and mechanism of SiC/Al–Mg–Si composites: effects of Mg addition10.1016/j.ceramint.2020.04.070 ↗
45. Orús · 2020
46. Effect of heat treatment on microstructure and mechanical properties of Al 2024 matrix composites reinforced with Ni60Nb40 metallic glass particles10.1016/j.jallcom.2019.151732 ↗
47. Identification of σ and Ω phases in AA2009/SiC composites10.1016/j.jallcom.2009.03.154 ↗
48. A model for precipitation kinetics and strengthening in Al–Cu–Mg alloys10.1016/j.msea.2007.03.033 ↗
49. Precipitation processes in Al–Mg–Cu alloys10.1016/S0921-5093(01)01049-8 ↗
50. Precipitation processes in Al-Cu-Mg alloys microalloyed with Si10.1007/BF02830331 ↗
51. Influence of predeformation and agEing of an Al–Zn–Mg alloy—II. Modeling of precipitation kinetics and yield stress10.1016/S1359-6454(98)00296-1 ↗
52. Microstructural evolution and mechanical behavior of powder metallurgy based SiC/Al–Mg-Sc-Zr nanocomposite subjected to multi-pass friction stir processing10.1016/j.msea.2021.140831 ↗
53. Influence of silicon on the corrosion behaviour of Al–Zn–In–Mg–Ti sacrificial anode10.1016/j.corsci.2011.07.039 ↗
54. Structure and mechanical behavior of in situ developed Mg 2 Si phase in magnesium and aluminum alloys–a review10.1039/D0RA02744H ↗
55. Processing and properties of magnesium containing a dense uniform dispersion of nanoparticles10.1038/nature16445 ↗
56. The wettability of SiC particles by molten aluminium alloy10.1016/S0924-0136(01)00975-X ↗
57. The wettability of silicon carbide by liquid aluminium: the effect of free silicon in the carbide and of magnesium, silicon and copper alloy additions to the aluminium10.1007/BF00356199 ↗
58. Unified tensile fracture criterion10.1103/PhysRevLett.94.094301 ↗
59. An enhanced FEM model for particle size dependent flow strengthening and interface damage in particle reinforced metal matrix composites10.1016/j.compscitech.2010.09.014 ↗
60. Interfacial structure of a SiC/Al composite10.1016/0921-5093(96)10168-4 ↗
61. A comparison of interfacial arrangements of sical composites10.1016/0956-716X(95)00008-J ↗
62. Microstructure of α-Al base matrix and SiC particulate composites10.1016/0921-5093(91)90373-U ↗
63. Structure and mechanism of bonding at a diffusion-bonded Al/SiC interface10.1016/0956-7151(94)90276-3 ↗