journal article·2023-08

Correlating microstructural features with improved wear and corrosion resistance of laser surface remelted A356 alloy at different scanning speeds

Chengquan Zhang, Linjiang Chai, Yuanzhuo Liu, Zhihao Li, Fangli Zhang, Xinyi Li, Zhongtao Fu

Publisher page

Abstract

In this work, two scanning speeds (2 mm/s and 8 mm/s) were employed to remelt the surface of an A356 cast Al alloy by a pulsed laser at 300 W, with microstructural features of the laser-remelted surface layers well characterized and correlated with their wear/corrosion resistance. Through high-quality microstructure characterizations, it is found that the as-received A356 alloy is comprised of coarse α-Al dendrites and interdendritic Al-Si eutectics. After laser surface remelting (LSR) at both speeds, microstructure homogeneity is greatly improved due to the remarkable refinement of the dendrites and interdendrites. Hardness and wear tests show that surface hardness and wear rate of the 2 mm/s specimen are 71.6 ± 0.6 HV and 1.1 × 10 −3 mm 3·N −1·m −1, while those of the 8 mm/s specimen are 67.2 ± 1.1 HV and 1.7 × 10 −3 mm 3·N −1·m −1, respectively, markedly improved compared to the substrate (55.3 ± 0.5 HV and 2.8 × 10 −3 mm 3·N −1·m −1). Electrochemical test results reveal that self-corrosion potential (E corr) and current (I corr) of the 2 mm/s specimen are −0.82 V and 9.5 × 10 −7 μA, while those of the 8 mm/s specimen are −0.89 V and 1.8 × 10 −6 μA, respectively. After comparing with the substrate (−0.95 V and 4.3 × 10 −6 μA), the corrosion resistance of both the LSRed specimens is confirmed to be significantly enhanced. Comprehensive analyses reveal that after the LSR the simultaneously increased wear/corrosion resistance can be related to the largely homogenized microstructure, the enhanced supersaturation of Si in α-Al, and the refinement and redistribution of Al-Si eutectics in the remelted layer.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. Quasi-continuous-wave laser surface melting of aluminium alloy: precipitate morphology, solute segregation and corrosion resistance10.1016/j.corsci.2019.01.035 ↗
2. A review of selective laser melting of aluminum alloys: processing, microstructure, property and developing trends10.1016/j.jmst.2018.09.004 ↗
3. Laser surface alloying on aluminum and its alloys: a review10.1016/j.optlaseng.2017.07.006 ↗
4. A review on selective laser sintering/melting (SLS/SLM) of aluminium alloy powders: processing, microstructure, and properties10.1016/j.pmatsci.2015.03.002 ↗
5. The comfort of the soft-safety driver alerts: measurements and evaluation
6. Laser-based surface modifications of aluminum and its alloys10.1080/10408436.2015.1076716 ↗
7. Selective laser melting of aluminium and aluminium metal substrate composites: review
8. Comparison of corrosion behaviour of friction stir processed and laser melted AA 2219 aluminium alloy10.1016/j.matdes.2011.03.033 ↗
9. Fundamental understanding of the corrosion performance of laser-melted metallic alloys10.1016/j.surfcoat.2005.07.108 ↗
10. Nd:YAG laser surface melting of aluminium alloy 6013 for improving pitting corrosion fatigue resistance10.1016/j.surfcoat.2005.05.034 ↗
11. Influence of laser surface remelting on Al-Si alloy properties10.5545/sv-jme.2012.696 ↗
12. Effects of laser energies on wear and tensile properties of biomimetic 7075 aluminum alloy10.1007/s11665-018-3162-8 ↗
13. Laser surface treatment and modification of aluminum alloy substrate composites10.1007/s40516-018-0054-6 ↗
14. Improvement in wear resistance of hyper-eutectic Al-Si cast alloy by laser surface remelting10.1016/S0257-8972(03)00100-2 ↗
15. Investigation of the influence of laser treatment parameters on the properties of the surface layer of aluminum alloys10.1016/j.phpro.2010.08.167 ↗
16. Influence of diode laser surface melting on microstructure and corrosion resistance of 7075 aluminium alloy
17. Morphology and corrosion characteristics of laser surface remelted Al-Si alloy at cryogenic conditions10.1002/1521-4176(200205)53:5<335::AID-MACO335>3.0.CO;2-O ↗
18. Dry sliding wear behavior of laser clad TiVCrAlSi high entropy alloy coatings on Ti–6Al–4V substrate10.1016/j.matdes.2012.04.049 ↗
19. Achieving parallelly-arranged Ti3C2Tx in epoxy coating for anti-corrosive/wear high-efficiency protection10.1016/j.compositesb.2021.109581 ↗
20. Corrosion performance of high pressure die-cast Al-Si-Mg-Zn alloys in 3.5 wt% NaCl solution10.1016/j.jallcom.2018.12.313 ↗
21. New technique for preparing A356 alloy semisolid slurry and its rheo-diecast microstructure and properties10.1016/S1003-6326(21)65623-6 ↗
22. A comparison of selective laser melting with bulk rapid solidification of AlSi10Mg alloy10.1016/j.jallcom.2018.01.309 ↗
23. Wear performance of A356 substrate composites reinforced with different types of reinforcing particles10.1007/s11665-017-2901-6 ↗
24. Tribological characteristics of an A356 aluminium alloy laser surface alloyed with nickel and Ni–Ti–C10.1016/j.apsusc.2014.06.061 ↗
25. Microstructural characteristics, hardness and wear resistance of a typical ferritic/martensitic steel surface-treated by pulsed laser10.1016/j.surfcoat.2021.127261 ↗
26. Limitations of linear energy density for laser powder bed fusion of Mg-15Gd-1Zn-0.4Zr alloy10.1016/j.matchar.2022.112071 ↗
27. A novel crack-free Ti-modified Al-Cu-Mg alloy designed for selective laser melting
28. A review on grain refinement of aluminum alloys: progresses, challenges and prospects10.1007/s40195-017-0565-8 ↗
29. Columnar to equiaxed transition in directional solidification of inoculated melts10.1016/j.actamat.2012.12.002 ↗
30. Strength-hardness correlations of thermal-exposed oxide dispersion strengthened nickel-based superalloy with different grain size distributions10.1016/j.matchar.2021.111178 ↗
31. Hall–Petch relation and boundary strengthening10.1016/j.scriptamat.2004.06.002 ↗
32. The strain and grain size dependence of the flow stress of copper10.1016/0001-6160(82)90221-8 ↗
33. Solid solution strengthening mechanism in high pressure die casting Al–Ce–Mg alloys10.1016/j.msea.2021.141109 ↗
34. Solid solution strengthening in Ti-Al alloys10.1007/BF02644529 ↗
35. Novel gradient alloy steel with quasi-continuous ratios fabricated by SLM: material microstructure and wear mechanism10.1016/j.matchar.2021.111020 ↗
36. Ultrahigh strength and plasticity in laser rapid solidified Al–Si nanoscale eutectics10.1080/21663831.2020.1755380 ↗
37. Microstructure evolution and high density of nanotwinned ultrafine Si in hypereutectic Al-Si alloy by laser surface remelting10.1016/j.matchar.2020.110147 ↗
38. Effect of hardness on three very different forms of wear10.1016/S0043-1648(96)07414-5 ↗
39. Laser-clad Nb(Ta)TiZr medium-entropy alloy coatings on pure Zr sheet: microstructural characteristics, hardness and wear resistance10.1016/j.intermet.2022.107498 ↗
40. Investigation of microstructure and wear resistance of laser-clad CoCrNiTi and CrFeNiTi medium-entropy alloy coatings on Ti sheet10.1016/j.optlastec.2021.107518 ↗
41. On enhancing surface wear resistance via rotating grains during selective laser melting
42. Influence of orientations biomimetic units processed by laser on wear resistance of 6082 aluminium alloy10.1016/j.optlastec.2020.106196 ↗
43. The pitting corrosion behavior of rapidly solidified aluminum alloys10.1016/0010-938X(86)90064-8 ↗
44. Influence of heat treatments on the corrosion mechanism of additive manufactured AlSi10Mg10.1016/j.corsci.2018.11.038 ↗
45. Abnormal corrosion behavior of selective laser melted AlSi10Mg alloy induced by heat treatment at 300 °C10.1016/j.jallcom.2019.06.274 ↗
46. Corrosion mechanism associated with Mg2Si and Si particles in Al–Mg–Si alloys10.1016/S1003-6326(11)61092-3 ↗
47. Localized corrosion in AA2099-T83 aluminum–lithium alloy: the role of intermetallic particles10.1016/j.matchemphys.2015.05.037 ↗
48. Microhardness and corrosion properties of hypoeutectic Al–7Si alloy processed by high-pressure torsion10.1016/j.matdes.2015.06.018 ↗
49. Stress corrosion cracking behavior of Nd:YAG laser-treated aluminum alloy 707510.1016/j.apsusc.2005.07.052 ↗
50. High-throughput computing for screening the potential alloying elements of a 7xxx aluminum alloy for increasing the alloy resistance to stress corrosion cracking10.1016/j.corsci.2021.109304 ↗
51. Identification of the metallurgical parameters explaining the corrosion susceptibility in a 2050 aluminium alloy10.1016/j.corsci.2015.10.020 ↗