The effect of nanometre-scale kinetic competition on the phase selection in Zr/Si superstructure
Source abstract
Abstract
Nano structured coating system demonstrates outstanding performance stemming from unique structure evolution. Zr/Si coating was proposed as an ideal candidate for the protection of Zr alloy cladding. However, the phase selection remains a challenge to coordinate the complex requirement under the service and accident conditions of reactor core. In this work, a phase selection mechanism for amorphous Zr-Si-O (abbr. ZSO) was elucidated by the competitive consumption of Zr layer by silicidation and oxidation, which was also scale-dependent. The energy-loss near-edge fine structure and nanoindentation were also employed to characterize the unique scale effect in the two processes. Both the oxides kinetics and elastic modulus gain indicated an immediate passivation process under the subcritical condition after the in situ phase selection of the amorphous ZSO. Ab initio molecular dynamics (AIMD) was performed to disclose the origination of depressed O migration in ZSO. The multilayer structure also shows accident tolerance potential. The interfacial phase selection provided a strategy to regulate mesoscale structure originating from nanomter interface and meets the diversified requirement for “structure-performance relationship” under the service and accident conditions.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Nuclear Materials and Properties · Nuclear materials and radiation effects · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Life extension strategy and research Progress of zirconium alloy cladding applied to light water reactors
2. Progress in preparation of zirconium alloy cladding surface coatings
3. Influence of a Mo interlayer on the oxidation behavior of a Cr coating on a Zr alloy substrate10.1016/j.corsci.2023.111192 ↗
4. Effect of Al content on high-temperature oxidation behavior and failure mechanism of CrAl-coated Zircaloy
5. High-temperature and interfacial oxidation of MAX phase-reinforced composite coatings deposited by laser cladding on Zr alloy substrates10.1016/j.ceramint.2023.09.200 ↗
6. Deposition, characterization and high-temperature steam oxidation behavior of single-phase Ti2AlC-coated Zircaloy-410.1016/j.corsci.2018.02.035 ↗
7. Magnetron sputter deposition of zirconium-silicide coating for mitigating high temperature oxidation of zirconium-alloy10.1016/j.surfcoat.2017.03.018 ↗
8. Blister formation in ZrN/SiN multilayers after He irradiation10.1016/j.surfcoat.2018.02.095 ↗
9. Size-dependent radiation tolerance in ion irradiated TiN/AlN nanolayer films10.1016/j.jnucmat.2013.05.035 ↗
10. Atomic scale investigations of thermally treated nano-structured Ti-Al-N/Mo-Si-B multilayers10.1016/j.surfcoat.2018.06.026 ↗
11. Effects of ion irradiation on structural and mechanical properties of crystalline Fe/amorphous SiOC nanolaminates10.1016/j.actamat.2017.08.031 ↗
12. Radiation tolerance of Cu/W multilayered nanocomposites10.1016/j.jnucmat.2011.03.030 ↗
13. Microstructure, high-temperature corrosion and steam oxidation properties of Cr/CrN multilayer coatings prepared by magnetron sputtering10.1016/j.corsci.2021.109755 ↗
14. Oxidation behavior and chemical evolution of architecturally arranged Zr/Si multilayer at high temperature10.1016/j.surfcoat.2020.126205 ↗
15. Multilayer (TiN, TiAlN) ceramic coatings for nuclear fuel cladding10.1016/j.jnucmat.2016.05.021 ↗
16. Early oxidation behavior of Si-coated titanium10.1016/j.corsci.2018.05.035 ↗
17. The oxidation of silicon in dry oxygen, wet oxygen, and steam10.1149/1.2425807 ↗
18. Self-consistent assessment of Li+ ion cathodes: theory vs. experiments10.1016/j.jechem.2020.11.008 ↗
19. Lithium ion conductivity in double Antiperovskite Li6.5OS1.5I1.5: alloying and boundary effects10.1021/acsaem.9b00861 ↗
20. First principles modeling and simulation of Zr-Si-B-C-N ceramics: developing hard and oxidation resistant coatings10.1016/j.actamat.2016.11.061 ↗
21. Displacements, mean-squared displacements, and Codisplacennents for the calculation of nonequilibrium properties10.1021/jp5012523 ↗
22. Qualitative interpretation of electron energy-loss near-edge structure in natural zircon10.1088/0953-8984/4/43/011 ↗
23. Electron energy-loss near-edge structure of zircon
24. Interpretation of O K-edge EELS in zircon using a structural variation approach10.1016/j.ultramic.2009.09.012 ↗
25. Thermal decomposition mechanisms of hafnium and zirconium silicates at the atomic scale10.1063/1.1926399 ↗
26. Diffusion of oxygen in amorphous Al2O3, Ta2O5, and Nb2O510.1063/1.4889800 ↗
27. C, diffusion in doped and undoped amorphous zirconia10.1016/j.jnucmat.2021.153108 ↗
28. Oxygen diffusion in zircon10.1016/S0012-821X(97)00057-5 ↗
29. Reactions and diffusion of water and oxygen molecules in amorphous SiO210.1103/PhysRevLett.88.055508 ↗
30. Diffusion of oxygen in fused silica
31. Slow oxygen diffusion rates in igneous zircons from metamorphic rocks10.2138/am-2003-0708 ↗
32. The diffusion of oxygen in silicon and germanium10.1016/0022-3697(60)90106-2 ↗
33. ZrO2 thin films on Si substrate10.1007/s10854-010-0144-5 ↗
34. ZrO2 film interfaces with Si and SiO210.1063/1.1994938 ↗
35. The diffusion of oxygen in alpha-zirconium10.1016/0022-3115(77)90097-6 ↗
36. Barin · 1995
37. Formation of amorphous and crystalline phases, and phase transition by solid-state reaction in Zr/Si multilayer thin films10.1016/0040-6090(95)06744-2 ↗
38. High-κ dielectric materials for microelectronics10.1080/714037708 ↗
39. Steam oxidation of Cr-coated Sn-containing Zircaloy solid rod at 1000 °C10.1016/j.corsci.2021.109682 ↗
40. Ultrastrong translucent glass ceramic with Nanocrystalline, biomimetic structure10.1021/acs.nanolett.8b03220 ↗
41. Spinodal decomposition in amorphous metal-silicate thin films: phase diagram analysis and interface effects on kinetics10.1063/1.1510590 ↗