journal article·2024-03

Microstructural evolution in laser-based directed energy deposition of 316 L stainless steel with interlayer deformation

Abeer Mithal, Niroj Maharjan, Sridhar Idapalapati

Publisher page

Abstract

There has been a significant industrial interest in additive manufacturing (AM) technologies such as directed energy deposition (DED) due to their ability to produce complex geometries with controlled microstructures. More recently, AM processes have been hybridized with plastic deformation technologies to achieve further benefits. In this experimental work, we systematically investigate the microstructural evolution in a DED process, selectively coupled with interlayer deformation using 316 L stainless steel. Our results revealed that the region below the interlayer deformed surface comprised of a recrystallized zone and a retained deformation zone with increased hardness in both zones. The region above the interlayer deformed surface experienced a refined solidification at both the grain and the sub-grain levels, which was attributed to the change in nucleation conditions due to the interlayer deformation. Moreover, microstructural evolution was found to vary significantly under different deformation levels and DED parameters. The extent of the recrystallized zone increased with increasing interlayer deformation level and decreased with faster scan speed. The findings provide comprehensive insights into the microstructural evolution in AM processes coupled with interlayer deformation and could pave the way for quick and cost-effective methods to engineer microstructures for different applications.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (76)

Show source-provided references
1. Directed energy deposition (DED) additive manufacturing: physical characteristics, defects, challenges and applications10.1016/j.mattod.2021.03.020 ↗
2. Metal Additive manufacturing: a review10.1007/s11665-014-0958-z ↗
3. Laser additive manufacturing of metallic components: materials, processes and mechanisms10.1179/1743280411Y.0000000014 ↗
4. Integration of interlayer surface enhancement technologies into metal additive manufacturing: a review10.1016/j.jmst.2023.03.064 ↗
5. Hybrid processes in Additive manufacturing10.1115/1.4038644 ↗
6. Mori
7. Glocal integrity in 420 stainless steel by asynchronous laser processing10.1016/j.cirp.2019.04.105 ↗
8. Compressive behavior of 420 stainless steel after asynchronous laser processing10.1016/j.cirp.2020.04.059 ↗
9. An approach to reduce stress and defects: a hybrid process of laser cladding deposition and shot peening10.1108/RPJ-06-2020-0129 ↗
10. The effect of inter-layer cold working and post-deposition heat treatment on porosity in additively manufactured aluminum alloys10.1016/j.jmatprotec.2015.11.006 ↗
11. Effect of in-situ layer-by-layer rolling on the microstructure, mechanical properties, and corrosion resistance of a directed energy deposited 316L stainless steel
12. In situ interlayer hot forging arc-based directed energy deposition of Inconel® 625: process development and microstructure effects
13. In-situ hot forging directed energy deposition-arc of CuAl8 alloy
14. Hot forging wire and arc additive manufacturing (HF-WAAM)
15. Synchronous-hammer-forging-assisted laser directed energy deposition additive manufacturing of high-performance 316L samples10.1016/j.jmatprotec.2022.117695 ↗
16. 3D laser shock peening as a way to improve geometrical accuracy in selective laser melting
17. Healing cracks in selective laser melting by 3D laser shock peening
18. 3D laser shock peening – a new method for improving fatigue properties of selective laser melted parts
19. Application of ultrasonic peening during DMLS production of 316L stainless steel and its effect on material behavior10.1108/RPJ-09-2016-0140 ↗
20. Reducing corrosion of additive manufactured magnesium alloys by interlayer ultrasonic peening10.1016/j.cirp.2021.04.052 ↗
21. Tailoring microstructure of additively manufactured Ti6Al4V titanium alloy using hybrid additive manufacturing technology
22. A hybrid directed energy deposition process to manipulate microstructure and properties of austenitic stainless steel10.1016/j.matdes.2021.110360 ↗
23. An approach to improve the microstructure and mechanical properties: a hybrid manufacturing of laser directed energy deposition and shot peening
24. Recrystallization behavior and tensile properties of laser metal deposited Inconel 718 upon in-situ ultrasonic impact peening and heat treatment10.1016/j.msea.2020.139434 ↗
25. Microstructure and properties of Inconel 718 fabricated by directed energy deposition with in-situ ultrasonic impact peening10.1007/s11663-019-01672-3 ↗
26. The effectiveness of grain refinement by machine hammer peening in high deposition rate wire-arc AM Ti-6Al-4V10.1007/s11661-020-05781-6 ↗
27. 2021
28. Steels in additive manufacturing: a review of their microstructure and properties10.1016/j.msea.2019.138633 ↗
29. Additive manufacturing of steels: a review of achievements and challenges10.1007/s10853-020-05109-0 ↗
30. Microstructure and mechanical properties of AISI 316L produced by directed energy deposition-based Additive manufacturing: a review10.3390/app10093310 ↗
31. Carpenter Additive
32. Enhanced cooling rates in laser directed energy deposition with interlayer peening10.1108/RPJ-11-2022-0395 ↗
33. A comparison on metallurgical behaviors of 316L stainless steel by selective laser melting and laser cladding deposition10.1016/j.msea.2016.12.112 ↗
34. Influence of processing parameters and heat treatment on the mechanical properties of 18Ni300 manufactured by laser based directed energy deposition10.1016/j.optlastec.2018.03.011 ↗
35. NIH image to ImageJ: 25 years of image analysis10.1038/nmeth.2089 ↗
36. Beausir
37. In-depth quantitative analysis of the microstructures produced by surface mechanical attrition treatment (SMAT)10.1016/j.matchar.2013.06.006 ↗
38. Microstructural characterization and mechanical behavior of ultrasonic impact peened and laser shock peened AISI 316L stainless steel10.1016/j.surfcoat.2020.125403 ↗
39. Study of the austenitic stainless steel with gradient structured surface fabricated via shot peening10.1016/j.matlet.2017.12.021 ↗
40. Nanoscale surface modification of AISI 316L stainless steel by severe shot peening10.1016/j.matdes.2016.03.162 ↗
41. Assessment of surface hardening effects from shot peening on a Ni-based alloy using electron backscatter diffraction techniques10.1016/j.actamat.2011.04.025 ↗
42. On the effectiveness of surface severe plastic deformation by shot peening at cryogenic temperature10.1016/j.apsusc.2016.08.009 ↗
43. Comparative study of additively manufactured and reference 316 L stainless steel samples – effect of severe shot peening on microstructure and residual stresses10.1016/j.matchar.2022.112162 ↗
44. Additive manufactured 316L stainless-steel samples: microstructure, residual stress and corrosion characteristics after post-processing10.3390/met11020182 ↗
45. Enhancement of surface characteristics of direct metal laser sintered stainless steel 316L by shot peening10.1016/j.surfin.2018.04.010 ↗
46. Strategy for surface post-processing of AISI 316L additively manufactured by powder bed fusion using ultrasonic nanocrystal surface modification10.3390/met11050843 ↗
47. The effects of laser peening on laser additive manufactured 316L steel10.1007/s00170-020-05167-3 ↗
48. Microstructural evolution and tensile property enhancement of remanufactured Ti6Al4V using hybrid manufacturing of laser directed energy deposition with laser shock peening
49. Annealing twin development during recrystallization and grain growth in pure nickel10.1016/j.msea.2014.01.018 ↗
50. Recrystallization-based grain boundary engineering of 316L stainless steel produced via selective laser melting10.1016/j.actamat.2020.09.015 ↗
51. 2021
52. Chapter 7 - recrystallization of single-phase alloys
53. Influence of process parameters and deposition strategy on laser metal deposition of 316L powder10.3390/met9111160 ↗
54. Adjusting microstructure and improving mechanical property of additive manufacturing 316L based on process optimization10.1016/j.msea.2023.144824 ↗
55. Effect of direct energy deposition process parameters on single-track deposits of alloy 71810.3390/met10010096 ↗
56. Controlling the solidification process parameters of direct energy deposition additive manufacturing considering laser and powder properties10.1016/j.commatsci.2020.109788 ↗
57. Laser shock peening: a promising tool for tailoring metallic microstructures in selective laser melting10.1016/j.jmatprotec.2018.11.024 ↗
58. Nucleation on dislocations10.1016/0001-6160(57)90021-4 ↗
59. Layer-wise engineering of grain orientation (LEGO) in laser powder bed fusion of stainless steel 316L
60. Solidification microstructure simulation of Ti-6Al-4V in metal additive manufacturing: a review
61. Selective laser melting of 316L stainless steel: influence of TiB2 addition on microstructure and mechanical properties
62. Crack elimination and mechanical properties enhancement in additive manufactured Hastelloy X via in-situ chemical doping of Y2O310.1016/j.msea.2021.141867 ↗
63. Additive manufacturing of a 316L steel matrix composite reinforced with CeO2 particles: process optimization by adjusting the laser scanning speed10.3390/technologies6010025 ↗
64. Kurz · 1989
65. Effect of SiCp content on cooling curve characteristics and solidification kinetics of Al-Si/SiCp cast composites10.1080/13640461.2003.11819631 ↗
66. Effects of solute content on grain refinement in an isothermal melt10.1016/j.actamat.2011.01.008 ↗
67. Thermal analysis of copper-tin alloys during rapid solidification10.1023/A:1004846812384 ↗
68. Correlation of recalescence with grain refinement of magnesium alloys10.1016/S1003-6326(10)60219-1 ↗
69. Additive manufacturing of Al-12Si alloy via pulsed selective laser melting10.1007/s11837-014-1272-9 ↗
70. Promoting the columnar to equiaxed transition and grain refinement of titanium alloys during additive manufacturing10.1016/j.actamat.2019.02.020 ↗
71. Effect of trace lanthanum hexaboride and boron additions on microstructure, tensile properties and anisotropy of Ti-6Al-4V produced by additive manufacturing10.1016/j.msea.2018.02.012 ↗
72. Modelling of recalescence effect on austenite decomposition10.1080/02670836.2017.1282693 ↗
73. Modelling of solidification for copper-base alloys during rapid solidification processing10.1016/S0921-5093(96)10582-7 ↗
74. Effect of scanning speed on the microstructure and mechanical behavior of 316L stainless steel fabricated by selective laser melting10.1016/j.matdes.2019.108355 ↗
75. Recrystallization and grain growth behavior in severe cold-rolling deformed SUS316L steel under Anisothermal annealing condition10.2355/isijinternational.48.475 ↗
76. An investigation of the effect of laser deposition parameters on characteristics of multilayered 316 L deposits10.1007/s00170-014-5951-z ↗