Short-time creep behavior of (TiB + TiC + Y2O3) reinforced titanium matrix composite in the range of 600 °C to 700 °C
Source abstract
Abstract
A titanium matrix composite reinforced by TiB, TiC and Y 2O 3 was prepared by induction skull melting. The creep behavior of the composite was tested at the temperature range from 600 °C to 700 °C in short time to investigate the deformation mechanism and microstructure involution. The as-cast composite shows a typical basket-weave microstructure. At the stress of 150 MPa, the stress exponents of the composite are 3.48 at 600 °C and 5.33 at 700 °C, corresponding to the deformation mechanism mainly controlled by solute-dragging and dislocation climbing respectively. Reinforcements added hinder dislocations movement effectively, which improves the creep resistance of the composite. As the creep temperature rises, the solubility of β-Ti increases, accompanied by the precipitation of silicides with different morphologies. Silicides play a role in pinning dislocations and hindering interface from migration. The dislocation movement and rearrangement during creep lead to the formation of sub-grains.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Advanced materials and composites · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. Perspectives on titanium science and technology10.1016/j.actamat.2012.10.043 ↗
2. Microstructural and mechanical characteristics of in situ metal matrix composites10.1016/S0927-796X(00)00024-3 ↗
3. On the characteristics of titanium alloys for the aircraft applications
4. Interface microstructure and strengthening mechanisms of multilayer graphene reinforced titanium alloy matrix nanocomposites with network architectures10.1016/j.matdes.2020.109119 ↗
5. Effect of the laser-wire relative position on the wire-based laser-directed energy deposition of in-situ synthesis Ti/TiB/TiC composite coatings10.1016/j.matchar.2023.113408 ↗
6. Effects of degree of deformation on the microstructure, mechanical properties and texture of hybrid-reinforced titanium matrix composites10.1016/j.actamat.2012.01.032 ↗
7. Deformation behavior and microstructure evolution mechanism of 5vol.% (TiBw+TiCp)/Ti composites during isothermal compression10.1016/j.matchar.2019.06.002 ↗
8. Titanium metal matrix composites: An overview10.1016/j.compositesa.2019.04.005 ↗
9. Progress on discontinuously reinforced titanium matrix composites10.1016/j.jallcom.2018.07.100 ↗
10. Fabrication of TiB-reinforced titanium matrix composite via spark plasma sintering and vertical bidirectional reactive hot rolling10.1016/j.matchar.2023.113450 ↗
11. Microstructural evolution and wear properties of in-situ (TiB+TiC)-reinforced Ti6Al4V matrix composite coating by laser melting deposition10.1016/j.matchar.2023.113192 ↗
12. Microstructure growth behavior and its evolution mechanism during laser additive manufacture of in-situ reinforced (TiB+TiC)/Ti composite10.1016/j.jallcom.2017.09.033 ↗
13. Characterization of triplet Ti-TiB-TiC composites: comparison of in-situ formation and ex-situ addition of TiC10.1016/j.ceramint.2020.01.204 ↗
14. In-situ (TiB+TiC) particulate reinforced titanium matrix composites: effect of B4C size and content10.1007/s12540-013-6024-9 ↗
15. Oxidation behavior of the Y2O3-modified aluminide coating on Ti-6Al-4V alloy10.1016/j.msea.2007.01.111 ↗
16. Microstructure and mechanical properties of Y2O3 reinforced Ti6Al4V composites fabricated by spark plasma sintering10.1016/j.jallcom.2018.07.229 ↗
17. Creep behaviour of Ti-6Al-2Sn-4Zr-2Mo: II. Mechanisms of deformation10.1016/S1359-6454(02)00280-X ↗
18. Effect of TiB, TiC and Y2O3 on tensile properties and creep behavior at 650 °C of titanium matrix composites10.1016/j.jallcom.2022.164699 ↗
19. Effect of nanoparticles on creep behaviour of metals: a review10.1016/j.jmrt.2023.08.068 ↗
20. Creep behaviour and creep microstructures of a high-temperature titanium alloy Ti-5.8Al-4.0Sn-3.5Zr-0.7Nb-0.35Si-0.06C (Timetal 834): part I. Primary and steady-state creep10.1016/S1044-5803(01)00136-X ↗
21. Dynamic recrystallization and silicide precipitation behavior of titanium matrix composites under different strains10.1016/S1003-6326(21)65739-4 ↗
22. Effect of stress and temperature on creep behavior of a (TiB+TiC+Y2O3)/α-Ti composite10.1016/j.matchar.2021.111495 ↗
23. Enhancement in creep resistance of Ti-6Al-4V alloy due to boron addition10.1016/j.msea.2013.12.078 ↗
24. Creep behavior of in situ dual-scale particles-TiB whisker and TiC particulate-reinforced titanium composites10.1557/JMR.2002.0338 ↗
25. Tensile and creep properties under different temperature conditions of titanium matrix composites reinforced by TiB and TiC10.1016/j.msea.2022.144279 ↗
26. Microstructural evolution and mechanical properties of near α-Ti matrix composites reinforced by hybrid (TiB+Y2O3) with bimodal size10.1016/j.vacuum.2017.08.001 ↗
27. Effects of hybrid reinforcements to the high temperature tensile and creep properties of a (TiB+TiC+Y2O3)/α-Ti composite10.1016/j.matchar.2022.112067 ↗
28. Microstructural effects on the mechanical behavior of B-modified Ti-6Al-4V alloys10.1016/j.actamat.2007.05.009 ↗
29. Achieving near equiaxed α-Ti grains and significantly improved plasticity via heat treatment of TiB reinforced titanium matrix composite manufactured by selective laser melting10.1016/j.jallcom.2020.155344 ↗
30. Creep behavior of Ti-6Al-4V and a comparison with titanium matrix composites10.1016/j.msea.2006.05.089 ↗
31. Tensile creep behavior of heat-treated TC11 titanium alloy at 450-550 °C10.1016/j.msea.2013.03.038 ↗
32. Five-power-law creep in single phase metals and alloys10.1016/S0079-6425(99)00006-7 ↗
33. Creep of zirconium and Zirc onium alloy10.1007/BF02586213 ↗
34. A critical analysis of the conventionally employed creep lifing methods10.3390/ma7053371 ↗
35. Creep mechanisms in Ti-3Al-2.5V alloy tubing deformed under closed-end internal gas pressurization10.1016/j.actamat.2008.01.052 ↗
36. Evolution of microstructural characteristic and tensile properties during preparation of TiB/Ti composite sheet10.1016/j.matdes.2011.11.060 ↗
37. Experimental and first-principles study on TiB/TiC interface in hybrid (TiB+TiC)/Ti6Al4V composite10.1016/j.ceramint.2022.04.249 ↗
38. Effect of Zr and Si addition on high temperature mechanical properties of near-α Ti-Al-Zr-Sn based alloys10.1016/j.msea.2014.06.078 ↗
39. Review on the creep resistance of high-temperature titanium alloy10.1007/s12666-020-02137-x ↗
40. Enhanced mechanical properties and structure stability induced by Si in Ti-8.5Al-1.5Mo alloys10.1016/j.msea.2016.09.009 ↗
41. Cooperative effect of silicon and other alloying elements on creep resistance of titanium alloys: insight from first-principles calculations10.1038/srep30611 ↗
42. Solidification paths and reinforcement morphologies in melt-processed (TiB+TiC)/Ti in situ composites10.1007/s11661-002-0290-3 ↗
43. Microstructural characterization of in situ synthesized TiB in cast Ti-1100-0.10B alloy10.1016/S1003-6326(15)63833-X ↗
44. Effects of dislocations on the early stageof TiC precipitation kinetics in ferritic steel: a comparative study with and without a pre-deformation10.1016/j.actamat.2019.06.055 ↗
45. Effects of hot-deformation on grain boundary precipitation and segregation in Ti-Mo microalloyed steels10.1016/j.matdes.2017.12.023 ↗
46. Reinforcements stimulated dynamic recrystallization behavior and tensile properties of extruded (TiB+TiC+La2O3)/Ti6Al4V composites10.1016/j.jallcom.2016.12.418 ↗
47. Enhanced creep properties of Y2O3-bearing Ti-48Al-2Cr-2Nb alloys10.1016/j.msea.2021.140952 ↗
48. Effects of microstructure and C and Si additions on elevated temperature creep and fatigue of gamma TiAl alloys10.1016/j.intermet.2014.04.006 ↗
49. Constructing two-scale network microstructure with nano-Ti5Si3 for superhigh creep resistance10.1016/j.jmst.2019.04.001 ↗