Abstract

The existing form of Sc in Si-containing 6xxx-series Al alloys and its role in strength has always been controversial. In this study, isothermal section phase diagram of the Al-0.60 wt%Mg-Si-Sc system at 350 °C was calculated by CALPHAD method and Pandat software, and the results show that Sc exists in Al 3Sc or V (AlSc 2Si 2 ) phases, depending on the contents of Si and Sc. Subsequently, we designed a Al-0.60 Mg-0.75Si-0.05Sc (wt%) Melt Inert Gas (MIG) welded alloy, and investigated its microstructure and mechanical property by tensile tests and electron microscopy. HRTEM and STEM-EDS results show that, Sc exists in the form of core(Sc)-shell (Si) structured (Al, Si) 3 Sc transition phases with the size range of 60–80 nm in the fractured zone (heat affected zone, HAZ) of the welded joints, deriving from equilibrium phase diagram, V (AlSc 2Si 2 ) theoretically. The HAZ of the Al-Mg-Si-Sc joint consists of partly recrystallized grains and strong rolling texture, different from the completely recrystallized and coarsened grains in the Al-Mg-Si joint. In addition, the (Al, Si) 3Sc phases increase the density of β`′ aging strengthening phases and prevent them from coarsening under welding heat cycle. The above positive effects of (Al, Si) 3 Sc particles increase the yield strength, ultimate tensile strength and elongation of Al-Mg-Si welded joints by 31 MPa (20.6%), 41 MPa (21.2%) and 0.8% (12.9%), respectively.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (58)

Show source-provided references
1. Atomic model for GP-zones in a 6082 Al–Mg–Si system10.1016/S1359-6454(00)00302-5 ↗
2. Scandium in aluminium alloys10.1179/174328005X14311 ↗
3. Processing and characterization of continuous-cast AlMgSc(Zr) sheets for improved strength10.1016/j.msea.2017.05.038 ↗
4. Mechanical properties and microstructure evolution in incremental forming of AA5754 and AA6061 aluminum alloys10.1016/S1003-6326(19)65179-4 ↗
5. Fatigue life improvement of mig welded aluminium T-joints by friction stir processing10.1016/j.ijfatigue.2013.11.004 ↗
6. Local corrosion behaviour of hybrid laser-MIG welded Al-Zn-Mg alloy joints10.1016/j.matdes.2015.08.140 ↗
7. Microstructures and fatigue behavior of metal-inert-gas-welded joints for extruded Al-Mg-Si alloy10.1016/j.msea.2018.12.080 ↗
8. Structure-property correlation of sub-zero treated AISI D2 steel10.1016/j.msea.2012.01.130 ↗
9. Influences of pulsed current welding and post weld aging treatment on fatigue crack growth behaviour of AA7075 aluminium alloy joints10.1016/j.ijfatigue.2007.04.012 ↗
10. Cryogenic properties of Al-Mg-Sc-Zr friction-stir welds10.1016/j.msea.2014.01.060 ↗
11. Ambient- and high-temperature mechanical properties of isochronally aged Al-0.06Sc, Al-0.06Zr and Al-0.06Sc-0.06Zr (at.%) alloys10.1016/j.actamat.2010.10.017 ↗
12. Highly monodisperse core-shell particles created by solid-state reactions10.1038/nmat3077 ↗
13. Homogeneous nucleation kinetics of Al3Sc in a dilute Al-Sc alloy10.1007/BF02647542 ↗
14. Atom probe tomographic study of a friction-stir-processed Al-Mg-Sc alloy10.1016/j.actamat.2012.09.015 ↗
15. The influence of Sc solute partitioning on the microalloying effect and mechanical properties of Al-Cu alloys with minor Sc addition10.1016/j.actamat.2016.08.013 ↗
16. Effect of minor Sc on microstructure and mechanical properties of Al-Zn-Mg-Zr alloy metal–inert gas welds10.1016/j.jallcom.2014.11.227 ↗
17. Effect of scandium content on the hot extrusion of Al-Zn-Mg-(Sc) alloy10.1016/j.jmatprotec.2006.11.047 ↗
18. Toropova · 2017
19. Construction of Al-based solid-solution range boundaries in the Al-Sc-Si system at 550 and 500°C10.1134/S0036029511110097 ↗
20. Scientific principles of making an alloying addition of scandium to aluminium alloys10.1016/S0921-5093(99)00652-8 ↗
21. Improving aging and creep resistance in a dilute Al-Sc alloy by microalloying with Si, Zr and Er10.1016/j.actamat.2013.10.008 ↗
22. Role of silicon in accelerating the nucleation of Al3(Sc, Zr) precipitates in dilute Al-Sc-Zr alloys10.1016/j.actamat.2012.05.036 ↗
23. Precipitation sequence in Al-Mg-Si-Sc-Zr alloys during isochronal aging10.1016/j.mtla.2019.100437 ↗
24. Micro-segregation and precipitates in as-solidified Al-Sc-Zr-(Mg)-(Si)-(Cu) alloys10.1016/j.matchar.2019.06.021 ↗
25. Thermodynamic description of the Al-Mg-Si system using a new formulation for the temperature dependence of the excess Gibbs energy10.1016/j.tca.2011.10.017 ↗
26. Formation of β″-related composite precipitates in relation to enhanced thermal stability of Sc-alloyed Al-Mg-Si alloys10.1016/j.jallcom.2021.160942 ↗
27. Understanding the formation of (Al, Si)3Sc and V-phase (AlSc2Si2) in Al-Si-Sc alloys via ex situ heat treatments and in situ transmission electron microscopy studies10.1016/j.jallcom.2020.158511 ↗
28. Materials · 2004
29. Steel · 2011
30. Experimental investigation and thermodynamic optimization of the Al-Ni-Sc ternary system10.1016/j.calphad.2022.102397 ↗
31. Experimental investigations and thermodynamic calculation in the Al-Mg-Sc system
32. Thermodynamic description of the quaternary Al-Si-Mg-Sc system and its application to the design of novel Sc-additional A356 alloys10.1016/j.matdes.2016.12.034 ↗
33. Precipitation of (Al, Si)3Sc in an Al-Sc-Si alloy10.1016/j.scriptamat.2009.05.014 ↗
34. Effects of Sc and Zr on mechanical property and microstructure of tungsten inert gas and friction stir welded aerospace high strength Al-Zn-Mg alloys10.1016/j.msea.2015.05.052 ↗
35. Microstructure and mechanical properties of laser beam-welded AA2060 Al-Li alloy10.1016/j.jmatprotec.2016.06.021 ↗
36. Effects of Sc(Zr) on the microstructure and mechanical properties of as-cast Al-Mg alloys10.1080/02670836.2016.1270573 ↗
37. Effects of Sc and Zr microalloying additions on the recrystallization texture and mechanism of Al-Zn-Mg alloys10.1016/j.jallcom.2013.06.020 ↗
38. The effect of TIG welding techniques on microstructure, properties and porosity of the welded joint of 2219 aluminum alloy10.1016/j.jallcom.2017.08.157 ↗
39. Effect of cooling rate on the grain refinement of Mg-3Nd alloys by aluminum
40. Study of the fusion zone and heat-affected zone microstructures in tungsten inert gas-welded INCONEL 738LC superalloy10.1007/s11661-006-0013-2 ↗
41. Rapid prototyping of 4043 Al-alloy parts by VP-GTAW10.1016/j.jmatprotec.2004.01.058 ↗
42. Uneven hardness mechanism and related fracture characteristics in laser-MIG hybrid welded Al-Mg-Si alloy butt10.2351/7.0000431 ↗
43. Softening behavior of Al-Zn-Mg alloys with different strengthening mechanisms in a coupled field10.1016/j.msea.2019.138582 ↗
44. Al3(Sc, Zr) precipitation in deformed Al-Mg-Mn-Sc-Zr alloy: effect of annealing temperature and dislocation density10.1016/j.jallcom.2020.154856 ↗
45. Characterization of TIG and MIG welded aluminium 6063 alloys
46. Influence of welding speed on the fatigue of friction stir welds, and comparison with MIG and TIG10.1016/S0142-1123(03)00059-8 ↗
47. Mechanical properties and microstructures of 6082-T6 joint welded by twin wire metal inert gas arc welding with the SiO2 flux10.1016/j.matdes.2011.09.002 ↗
48. Modifying microstructures and mechanical properties of laser-arc welded joints of dissimilar advanced aluminum alloys10.1016/j.matchar.2020.110331 ↗
49. Effect of TIG current on microstructural and mechanical properties of 6061-T6 aluminium alloy joints by TIG-CMT hybrid welding10.1016/j.jmatprotec.2017.12.006 ↗
50. Effects of base metal state on the microstructure and mechanical properties of Al-Mg-Si alloy friction stir-welded joints10.1016/j.jmapro.2020.04.084 ↗
51. Experimental study on microstructure and mechanical properties of AA6061/Ti-6Al-4V joints made by bypass-current MIG welding-brazing10.1016/j.jmatprotec.2018.05.019 ↗
52. Behavior and stability of droplet transfer under laser-MIG hybrid welding with synchronized pulse modulations10.1016/j.jmapro.2020.02.017 ↗
53. Effect of platform temperature on the porosity, microstructure and mechanical properties of an Al-Mg-Sc-Zr alloy fabricated by selective laser melting10.1016/j.msea.2018.06.049 ↗
54. Role of additive manufacturing applications towards environmental sustainability
55. Effects of homogenization treatment on recrystallization behavior and dispersoid distribution in an Al-Zn-Mg-Sc-Zr alloy10.1016/j.jallcom.2007.02.054 ↗
56. Improving aging and creep resistance in a dilute Al-Sc alloy by microalloying with Si, Zr and Er10.1016/j.actamat.2013.10.008 ↗
57. Strengthening mechanisms of an Al-Mg-Sc-Zr alloy10.1016/S1359-6454(02)00258-6 ↗
58. Chemistry and structure of core/double-shell nanoscale precipitates in Al-6.5Li-0.07Sc-0.02Yb (at.%)10.1016/j.actamat.2011.02.015 ↗