The formation of three phases containing Fe and Mn in 5182 aluminum alloy
Source abstract
Abstract
The categories, crystal types, morphology, dimension, distribution and selectivity of precipitation positions of alloy phases containing Fe and Mn in the DC casting ingot of 5182 aluminum alloy under industrial production conditions after being treated with different homogenization processes were studied through TEM and EPMA with FIB sample preparation. The formation process of three phases containing Fe and Mn was clarified as well. The results showed that there was only one category of alloy phase containing Fe and Mn in the as-cast 5182 aluminum alloy, which was one category of skeletal nonequilibrium constituent Al 19(Fe,Mn) 4 ′ with orthorhombic structure formed by the eutectic reaction L → α(Al)′ + Al 19(Fe,Mn) 4′. After the ingot was homogenized at a high temperature above 460 °C, there were three categories of alloy phases containing Fe and Mn, which were skeletal equilibrium phase Al 19(Fe,Mn) 4 with orthorhombic structure, short rod-like intermetallic phase Al 3 (Fe,Mn) with monoclinic structure and acicular alloy phase Al 6(Fe,Mn) with orthorhombic structure, respectively. The metastable constituent Al 19(Fe,Mn) 4′ transformed into the equilibrium phase Al 19(Fe,Mn) 4 with orthorhombic structure and the alloy phase Al 3(Fe,Mn) with monoclinic structure by desolation transformation Al 19(Fe,Mn) 4′ → Al 19(Fe,Mn) 4 + Al 3(Fe,Mn). In addition, acicular alloy phase particles Al 6(Fe,Mn) with orthorhombic structure were precipitated from the alloy matrix with supersaturated solute Fe and Mn atoms through the desolation reaction α(Al)′ → α(Al) + Al 6(Fe,Mn). With increasing homogenization temperature, the skeletal constituent Al 19(Fe,Mn) 4 particles with orthorhombic structure were almost the same, and the short rod-like alloy phase Al 3(Fe,Mn) particles, with monoclinic structure changed unobviously in morphology and size, but its number increased significantly. At the same time, the number and the size of acicular Al 6(Fe,Mn) alloy phase particles with orthorhombic structure precipitated from the alloy matrix increased.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Bauxite Residue and Utilization
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. Characterization of wear and friction between tool steel and aluminum alloys in sheet forming at room temperature10.1016/j.jmapro.2021.02.007 ↗
2. Mechanism of low temperature deformation in aluminium alloys10.1016/j.msea.2020.139935 ↗
3. Enhanced mechanical property and corrosion resistance of alloy 5182 FSW joints by Sc and Zr alloying10.1016/j.matchar.2022.112412 ↗
4. Microstructural, porosity and mechanical properties of lap joint laser welding for 5182 and 6061 dissimilar aluminum alloys under different place configurations10.1016/j.matdes.2020.108625 ↗
5. Ultrasonic spot welding of 5182 aluminum alloy: evolution of microstructure and mechanical properties10.1016/j.msea.2019.04.059 ↗
6. The influence of Sc and Zr additions on microstructure and corrosion behavior of AA5182 alloy sheet10.1016/j.corsci.2022.110181 ↗
7. Influence of pre-straining and heating on strain-rate sensitivity of AA5182-O10.1016/j.ijimpeng.2021.104106 ↗
8. Weld zone porosity elimination process in remote laser welding of AA5182-O aluminum alloy lap-joints10.1016/j.jmatprotec.2020.116826 ↗
9. Mechanism and numerical simulation analysis of laser welding 5182 aluminum alloy/PA66 based on surface texture treatment10.1016/j.optlastec.2022.108273 ↗
10. The effects of reduction and thermal treatment on the recrystallization and crystallographic texture evolution of 5182 aluminum alloy10.3390/met10101380 ↗
11. Strain rate sensitivity of the commercial aluminum alloy AA5182-O10.1016/j.msea.2004.08.029 ↗
12. Effect of initial grain size on the recrystallization and recrystallization texture of cold-rolled AA5182 aluminum alloy10.1016/j.msea.2017.03.015 ↗
13. Microstructure evolution of annealed 7075 aluminum alloy and its influence on room-temperature plasticity10.1016/j.matdes.2020.109192 ↗
14. The mechanistic contribution of nanosized Al3Fe phase on the mechanical properties of Al-Fe alloy10.1016/j.msea.2018.04.002 ↗
15. Formation of θ-Al13Fe4 and the multi-step phase transformations to α-Al8Fe2Si, β-Al5FeSi and δ-Al4FeSi2 in Al-20Si-0.7Fe alloy10.1016/j.intermet.2020.106960 ↗
16. Transformation of the metastable Al6Fe intermetallic phase during homogenization of a binary Al-Fe alloy10.3390/ma14237208 ↗
17. Formation of multiple intermetallic phases in a hypereutectic Al-Fe binary alloy additively manufactured by laser powder bed fusion10.1016/j.intermet.2020.106892 ↗
18. Effect of Mn addition on Fe-rich intermetallics morphology and dry sliding wear investigation of hypereutectic Al-17.5%Si alloys10.1016/j.jmrt.2015.11.008 ↗
19. The formation mechanism of Al6(Fe,Mn) in die-cast Al-Mg alloys10.1039/C8CE00675J ↗
20. A eutectoid phase transformation for the primary intermetallic particle from Alm(Fe,Mn) to Al3(Fe,Mn) in AA5182 alloy10.1016/j.actamat.2004.02.041 ↗
21. Effect of preheat temperature on the orientation relationship of (Mn,Fe)Al6 precipitates in an AA5182 Aluminium-Magnesium alloy10.1016/0956-7151(94)00261-F ↗
22. Evolution of micro-chemistry during solidification and homogenisation of AA3xxx aluminium-manganese alloys10.1080/02670836.2021.1963540 ↗
23. Precipitation crystallography of plate-shaped Al6(Mn,Fe) dispersoids in AA5182 alloy10.1016/j.actamat.2012.06.022 ↗
24. Effect of corrosion product films on the in vitro degradation behavior of Mg-3%Al-1%Zn (in wt%) alloy in Hank’s solution10.1016/j.jmst.2018.02.013 ↗
25. A thermodynamic evaluation of the Al-Mn system10.1007/BF02646113 ↗
26. In situ measurement of the precipitate volume fraction and interfacial crystal misfit during non-isothermal creep in the superalloy CMSX-410.1016/j.msea.2018.10.033 ↗
27. Deformation behavior and dynamic recrystallization during hot compression in homogenized Al-6Mg-0.8Mn alloys10.1016/j.msea.2022.142953 ↗