journal article·2024-08Open access

In-situ observation of solidification behaviors of Fe-Mn-Cr-Ni-Si alloy during TIG melt-run welding using synchrotron radiation X-ray

Tomoya Nagira, Houichi Kitano, Takashi Kimura, Fumiyoshi Yoshinaka, Susumu Takamori, Takahiro Sawaguchi, Takayuki Yamashita, Yasuhiro Aoki, Hidetoshi Fujii, Akihisa Takeuchi, Masayuki Uesugi

Abstract

The solidification behaviors, including the solidification cracking and solidification mode of the Fe-Mn-Cr-Ni-Si alloys at the weld bead during tungsten inert gas (TIG) melt-run welding, were examined by time-resolved in-situ observations using synchrotron radiation X-ray imaging and X-ray diffraction. The dynamics of initiation and propagation of solidification cracking at the weld bead could be observed at the dendrite scale. For the specimen solidified in the austenite mode at a welding speed of 10 mm/s, solidification cracking with a zigzag interface developed via the coalescence of many small pores at the centerline, where the columnar dendrite tips impinged. Quantitative image analysis indicated that the local tensile strain was highly localized at the centerline, and the critical local tensile strain for the initiation of solidification cracking was approximately 0.04. For the specimen solidifying in the ferrite-austenite mode at the welding speed of 10 mm/s, the centerline solidification cracking was suppressed by the formation of many equiaxed γ-Fe dendrites ahead of the growing columnar δ-Fe dendrites. Grain refinement at the centerline can be achieved at a welding speed of more than 7 mm/s without requiring inoculants.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Welding Techniques and Residual Stresses · High Entropy Alloys Studies · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (45)

Show source-provided references
1. Designing Fe-Mn-Si alloys with improved low-cycle fatigue lives10.1016/j.scriptamat.2014.11.024 ↗
2. Effect of strain amplitude on the low-cycle fatigue behavior of a new Fe-15Mn-10Cr-8Ni-4Si seismic damping alloy10.1016/j.ijfatigue.2016.03.021 ↗
3. Fatigue-resistant Fe-Mn-Si-based alloy seismic dampers to counteract long-period ground motion10.1002/2475-8876.12193 ↗
4. Development of ferrous-based weldable seismic damping alloy with prolonged plastic fatigue life10.1016/j.scriptamat.2021.113815 ↗
5. Austenitic solidification mode in austenitic stainless steel welds10.1007/BF02811663 ↗
6. Microstructure evolution and solidification cracking in austenitic stainless steel welds10.29391/2018.97.026 ↗
7. Solidification crack susceptibility in weld metals of duplex stainless steels
8. In-situ observations of phase transformations during solidification and cooling of austenitic stainless steel welds using time-resolved x-ray diffraction10.1016/S1359-6462(00)00481-4 ↗
9. Time-resolved X-ray diffraction investigation of primary weld solidification in Fe-C-Al-Mn steel welds10.1016/S1359-6454(02)00317-8 ↗
10. Time-resolved in-situ analysis of phase evolution for the directional solidification of carbon steel weld metal10.1007/s11661-006-1077-8 ↗
11. Time-resolved X-ray diffraction studies of solidification microstructure evolution in welding10.1016/j.actamat.2014.01.040 ↗
12. Effect of alloy element on weld pool dynamics in laser welding of aluminum alloys10.1038/s41598-018-31350-4 ↗
13. Initiation and growth kinetics of solidification cracking during welding of steel10.1038/srep40255 ↗
14. Development of evaluation method for solidification cracking susceptibility of Inconel/SUS347 dissimilar laser weld metal by in-situ observation10.4028/www.scientific.net/MSF.580-582.49 ↗
15. Observation of the initiation and propagation of solidification cracks by means of in situ synchrotron X-ray radiography
16. The effect of welding conditions on solidification cracking susceptibility of type 310S stainless steel during laser welding using an in-situ observation technique
17. Investigation of solidification cracking susceptibility during laser beam welding using an in-situ observation technique10.1080/13621718.2017.1367550 ↗
18. Time-resolved X-ray imaging of solidification cracking for Al-cu alloy at the weld crater10.1016/j.matchar.2020.110469 ↗
19. In situ observation of solidification crack propagation for type 310S and 316L stainless steels during TIG welding using synchrotron X-ray imaging10.1007/s10853-021-05969-0 ↗
20. Direct observation of solidification behaviors of Fe-Mn-Si alloys during arc spot welding using synchrotron X-ray10.1016/j.scriptamat.2022.114743 ↗
21. Elucidation of solidification mode of Fe-Mn-Si alloy during TIG spot welding using synchrotron X-ray10.2207/qjjws.41.1s ↗
22. Construction and commissioning of a 215-m-long beamline at SPring-810.1016/S0168-9002(01)00445-4 ↗
23. Tomasi · 1998 · 839
24. Contrast limited adaptive histogram equalization, graphics gems
25. TV-L1 optical flow estimation, image process
26. Implementation and evolution of optical flow methods for two-dimensional deformation measurement in comparison to digital image correlation10.1016/j.optlaseng.2018.03.021 ↗
27. Welding parameters and the grain structure of weld metal – a thermodynamic consideration10.1007/BF02628392 ↗
28. Behavior of metal alloys in the semisolid state10.1007/BF02661090 ↗
29. Mathers · 2002 · 10
30. Time-resolved and in-situ observation of δ-γ transformation during unidirectional solidification in Fe-C alloys10.2355/isijinternational.ISIJINT-2019-636 ↗
31. Solidification mechanism of austenitic stainless steels solidified with primary ferrite10.1016/j.actamat.2016.11.030 ↗
32. Mechanisms of equiaxed grain formation in ferritic stainless steel gas tungsten arc welds10.1016/0921-5093(94)09656-2 ↗
33. Use of inoculants to refine weld solidification structure and improve weldability in type 2090 Al-li alloy10.1016/S0921-5093(99)00515-8 ↗
34. Effect of scandium and titanium-boron on grain refinement and hot cracking of aluminium alloy 710810.1179/136217199101538030 ↗
35. Influence of superheat and grain structure on hot-tearing susceptibilities of Al-cu alloy casting10.1179/030716983803291226 ↗
36. Kou · 2021
37. Lippold · 2015
38. Nucleation mechanisms and grain refining of weld metal
39. Solidification and solidification structure control of solid metals10.1080/09507110209549544 ↗
40. Grain refinement in magnetically stirred GTA welds of aluminum alloys10.1007/BF02654317 ↗
41. Use of inoculants to refine weld solidification structure and improve weldability in type 2090 Al-li alloy10.1016/S0921-5093(99)00515-8 ↗
42. Columnar to equiaxed grain transition in as solidified alloys10.1179/174328006X102493 ↗
43. Columnar to equiaxed transition in solidification processing10.1016/S1468-6996(01)00047-X ↗
44. Solidification of austenitic stainless steel weldments: part 2 - the effect of alloy composition on ferrite morphology
45. A new set of Creq and Nieq equations for predicting solidification modes of cast austenitic Fe-Mn-Si-Cr-Mo shape memory alloys10.1007/s11663-013-0005-8 ↗