Zn additions modifying microstructure, thermal parameters and cytotoxicity of Sn-0.7Cu eutectic solder alloys

Jeverton Laureano Paixão, Raí Batista de Sousa, Bruno Silva Sobral, Rubiamara Mauricio de Sousa, Jefferson Romáryo Duarte da Luz, José Eduardo Spinelli, Bismarck Luiz Silva

Publisher page

Abstract

Alloys from the Sn Cu systems have superior properties as compared to the Sn Pb alloys, such as mechanical and corrosion resistance. However, Sn Cu alloys still exhibit low oxidation resistance, poor wettability and low reliability. One way to optimize such properties is by adding alloying elements, such as zinc. Zn is generally used in Pb-free solder alloys to minimize intermetallic compound growth in soldered joints, refine the microstructure and increase mechanical strength, in addition to reducing the final cost. The addition of Zn is motivated by the effects it promotes such as microstructural refining, suppression of intermetallics in the substrate/alloy reaction layer, increase in fluidity and mechanical properties. Therefore, this study aims to understand the effects of Zn additions (0.2 and 0.5 in wt%) on solidification thermal parameters (growth rate-V and cooling rate-Ṫ), macrostructure, microstructure, phase transformation, macrosegregation and cytotoxicity in directionally solidified eutectic Sn-0.7wt.%Cu alloy under transient heat flow regime of solidification in copper sheet. Thus, the samples have been characterized by Optical Microscopy (OM), Scanning Electron Microscopy (SEM), X-Ray Fluorescence (XRF) and X-Ray Diffraction (XRD). The CALPHAD (CALculation of PHAse Diagrams) method by Thermo-calc software was used to generate property diagrams and isopleths. Cytotoxicity analysis was performed based on cell viability with incubation periods of 15 and 30 days for the alloys, with subsequent exposures of the extracts for 24 and 48 h. The Zn additions caused slight changes in the phase transformation temperatures of the Sn-Cu-Zn alloys. Macrostructures exhibiting columnar-to-equiaxed transition (CET) were observed for the Sn-Cu-Zn alloys. The microstructures of the Sn-Cu-Zn alloys were predominantly dendritic with a matrix rich in tin (β-Sn) surrounded by a eutectic mixture of the β-Sn + Cu 6Sn 5 + CuZn phases. After CET on Sn-Cu-Zn castings, low velocity eutectic cells have been observed. Moreover, Zn additions refined and did not change the dendritic arrangement of the Sn-Cu-Zn alloys, when compared to the Sn-0.7wt.%Cu alloy. However, increasing the Zn content did not affect the microstructural scale in the ternary alloys when compared to each other. The variations in the microstructural scale did not influence the toxicity of the examined alloys, but factors such as incubation time and chemical composition did. In general, Zn improved the cell viability of the Sn-Cu-Zn alloys, but still with moderate cytotoxic levels.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (55)

Show source-provided references
1. A review of lead-free solders for electronics applications10.1016/j.microrel.2017.06.016 ↗
2. Lead-free solders in microelectronics10.1016/S0927-796X(00)00010-3 ↗
3. Sn–0.7 wt% Cu–(xNi) alloys: microstructure–mechanical properties correlations with solder/substrate interfacial heat transfer coefficient10.1016/j.jallcom.2015.01.140 ↗
4. Thermal parameters, microstructure, and mechanical properties of directionally solidified Sn-0.7 wt.%cu solder alloys containing 0 ppm to 1000 ppm Ni10.1007/s11664-012-2263-7 ↗
5. Stabilisation of Cu6Sn5 by Ni in Sn-0.7 Cu-0.05 Ni lead-free solder alloys10.1016/j.intermet.2009.07.005 ↗
6. Cellular to dendritic transition during transient solidification of a eutectic Sn–0.7 wt% Cu solder alloy10.1016/j.matchemphys.2011.11.033 ↗
7. Microstructure control in Sn–0.7 mass% cu alloys10.2320/matertrans.46.2419 ↗
8. Effect of Ni addition to Sn0. 7Cu solder alloy on thermal behavior, microstructure, and mechanical properties10.1007/s11665-018-3734-7 ↗
9. Developments of high strength Bi-containing Sn0. 7Cu lead-free solder alloys prepared by directional solidification10.1016/j.jallcom.2014.10.205 ↗
10. Enhancement of creep resistance and thermal behavior of eutectic Sn–Cu lead-free solder alloy by Ag and In-additions10.1016/j.matdes.2012.04.007 ↗
11. The influence of Ni and Zn additions on microstructure and phase transformations in Sn–0.7 Cu/Cu solder joints10.1016/j.actamat.2014.10.003 ↗
12. Effects of minor additions of Zn on interfacial reactions of Sn-Ag-Cu and Sn-Cu solders with various Cu substrates during thermal aging10.1007/s11664-007-0254-x ↗
13. Reactive wetting of Sn0. 7Cu–xZn lead-free solders on Cu substrate10.1016/j.jallcom.2006.06.076 ↗
14. Improvement of microstructure and interface structure of eutectic Sn–0.7 Cu solder with small amount of Zn addition10.1016/j.scriptamat.2005.05.013 ↗
15. Role of zinc on shear property evolution between Sn-0.7 Cu solder and joints10.1016/j.proeng.2011.08.1158 ↗
16. Improvement of Ga and Zn alloyed Sn–0.7 Cu solder alloys and joints10.1007/s10854-015-2873-y ↗
17. Rogero · 2006
18. Cytotoxicity testing: measuring viable cells, dead cells, and detecting mechanism of cell death10.1007/978-1-61779-108-6_12 ↗
19. In vitro cytotoxicity of metallic ions released from dental alloys10.1007/s10266-014-0192-z ↗
20. In vitro cytotoxicity evaluation of elemental ions released from different prosthodontic materials10.1016/j.dental.2009.07.008 ↗
21. Zinc-based alloys for degradable vascular stent applications10.1016/j.actbio.2018.03.005 ↗
22. Research on a Zn-cu alloy as a biodegradable material for potential vascular stents application10.1016/j.msec.2016.06.082 ↗
23. Biodegradable metals for cardiovascular stents: from clinical concerns to recent Zn-alloys10.1002/adhm.201501019 ↗
24. A. International · 2017
25. Directional solidification of aluminium–copper alloys10.1016/S0921-5093(01)01649-5 ↗
26. Chemical characterization of flowers and leaf extracts obtained from Turnera subulata and their immunomodulatory effect on LPS-activated RAW 264.7 macrophages10.3390/molecules27031084 ↗
27. Thermodynamic assessment of the Al–Cu–Zn system, part I: Cu–Zn binary system10.1016/j.calphad.2015.09.010 ↗
28. Insights into the atomic scale structure, bond characteristics and wetting behavior of Cu (001)/Cu6Sn5 (110) interface: a first-principles investigation10.1016/j.vacuum.2021.110103 ↗
29. Critical properties of Cu6Sn5 in electronic devices: recent progress and a review10.1016/j.cossms.2015.08.001 ↗
30. A novel antioxidant and low-temperature Sn-Zn solder paste based on Zn@ Sn core-shell structure10.1016/j.mtcomm.2022.103356 ↗
31. On the columnar to equiaxed transition in small ingots10.1007/BF02661748 ↗
32. Assessment of tertiary dendritic growth and its effects on mechanical properties of directionally solidified Sn-0.7 Cu-x Ag solder alloys10.1007/s11664-014-3087-4 ↗
33. Influence of melt convection on the columnar to equiaxed transition and microstructure of downward unsteady-state directionally solidified Sn-Pb alloys10.1016/j.jallcom.2004.04.098 ↗
34. The columnar to equiaxed transition during the horizontal directional solidification of Sn–Pb alloys10.1016/j.jallcom.2008.11.026 ↗
35. Influence of solidification thermal parameters on the columnar-to-equiaxed transition of aluminum-zinc and zinc-aluminum alloys10.1007/s11661-007-9111-z ↗
36. The columnar to equiaxed transition in tin-lead alloys10.1007/BF02656163 ↗
37. The columnar to equiaxed transition during solidification of Sn–Pb alloys10.1016/S0925-8388(02)01026-5 ↗
38. Cellular/dendritic transition and microstructure evolution during transient directional solidification of Pb-Sb alloys10.1007/s11661-008-9542-1 ↗
39. Evolution of thermal property and creep resistance of Ni and Zn-doped Sn–2.0 Ag–0.5 Cu lead-free solders10.1016/j.matdes.2013.04.081 ↗
40. Cooling thermal parameters and microstructure features of directionally solidified ternary Sn–Bi–(Cu, Ag) solder alloys10.1016/j.matchar.2016.02.002 ↗
41. Microstructural development and mechanical properties of a near-eutectic directionally solidified Sn–bi solder alloy10.1016/j.matchar.2015.06.026 ↗
42. Effects of Zn addition on dendritic/cellular growth, phase formation, and hardness of a Sn–3.5 wt% Ag solder alloy10.1002/adem.202201270 ↗
43. Microstructural development of hypoeutectic Zn–(10–40) wt% Sn solder alloys and impacts of interphase spacing and macrosegregation pattern on hardness10.1016/j.jallcom.2015.05.195 ↗
44. Interfacial reactions of Sn-8wt.% Zn-3wt.% Bi solder with Cu, Ag, and Ni substrates10.1007/s11664-007-0255-9 ↗
45. Effects of Cu and in trace elements on microstructure and thermal and mechanical properties of Sn-Zn eutectic alloy10.1007/s11664-018-06869-x ↗
46. Macrosegregation and channel segregation formation of faceted mushy zone in solidification of Sn–Ni hypereutectic alloy in a temperature gradient10.1016/j.matchemphys.2021.124447 ↗
47. Retarding the Cu5Zn8 phase fracture at the Sn–9 wt.% Zn/Cu interface10.1016/j.scriptamat.2010.12.006 ↗
48. Interfacial reaction and die attach properties of Zn-Sn high-temperature solders10.1007/s11664-008-0550-0 ↗
49. Microstructure of the Sn—Cu6Sn5 fibrous eutectic and its modification by segregation10.1016/S1359-6454(96)00060-2 ↗
50. Scanning electron microscopy: physics of image formation and microanalysis10.1088/0957-0233/11/12/703 ↗
51. Solidification of Sn-0.7 cu-0.15 Zn solder: in situ observation10.1007/s11661-013-2008-0 ↗
52. Effect of adding 0.3 wt% Ni into the Sn–0.7 wt% Cu solder: Part II. Growth of intermetallic layer with Cu during wetting and aging10.1016/j.jallcom.2006.08.071 ↗
53. Restriction of the use of certain hazardous substances in electrical and electronic equipment (RoHS)
54. Critical role of zinc as either an antioxidant or a prooxidant in cellular systems10.1155/2018/9156285 ↗
55. Biocompatibility of dental casting alloys: a review10.1016/S0022-3913(00)80016-5 ↗