Low-cost Ti-6Al-4V containing low content nano-carbon solid solution for achieving high strength and good ductility
Source abstract
Abstract
With the rapid advancement of the aerospace industry, in addition to higher requirements for material properties, the cost-effective of its production have also attracted more attention. In this work, titanium matrix composite with high performance and low cost was designed using ball milling, spark plasma sintering and hot rolling process, i.e. hydrogenated dehydrogenated Ti and Al V powders as the precursor of Ti-6Al-4 V matrix, and a low content (0.15 wt%) reduced graphene oxide (rGO) with high-activity was selected to reinforce the matrix alloy. The as-rolled composite shows obvious texture orientation along the rolling direction without pores and microcracks. The incorporation of rGO led to the activation of the as-rolled composites along the {0001}[11 2 ¯ 0] type base slip. The as-rolled composite containing only 0.15 wt% rGO exhibits superior yield strength (1308.1 MPa) and ultimate tensile strength (1444.3 MPa), which are 11% and 9.3% higher than those of the matrix alloy, respectively, and the elongation remains at ∼5.6%. The strengthening mechanisms are mainly attributed to the solid solution strengthening effect of interstitial carbon in the matrix after the incorporation of rGO. This work highlights the development potential of low-cost and high-strength titanium matrix composites
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Titanium Alloys Microstructure and Properties · Boron and Carbon Nanomaterials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (47)
Show source-provided references
1. Structural modelling and mechanical behaviors of graphene/carbon nanotubes reinforced metal matrix composites via atomic-scale simulations: a review
2. Breaking through the strength-ductility trade-off in graphene nanoplatelets reinforced titanium matrix composites via two-scale laminated architecture design10.1016/j.matchar.2023.113290 ↗
3. Carbonaceous nanomaterial reinforced Ti-6Al-4V matrix composites: properties, interfacial structures and strengthening mechanisms10.1016/j.carbon.2020.04.009 ↗
4. Improved mechanical properties in titanium matrix composites: controllable TiBw distribution by thermal deformation process
5. Rapid in-situ synthesis, microstructure and mechanical properties of titanium matrix composites with micro/nano-sized TiB/TiC hybrid structures10.1016/j.vacuum.2022.111635 ↗
6. Sintering effect on microstructural evolution and mechanical properties of spark plasma sintered Ti matrix composites reinforced by reduced graphene oxides10.1016/j.ceramint.2018.06.252 ↗
7. Interface microstructure and strengthening mechanisms of multilayer graphene reinforced titanium alloy matrix nanocomposites with network architectures10.1016/j.matdes.2020.109119 ↗
8. Effect of C addition on microstructure and mechanical properties of Nb–Si–Ti based alloys10.1016/j.msea.2021.140789 ↗
9. Microstructure evolution and superior tensile properties of low content graphene nanoplatelets reinforced pure Ti matrix composites10.1016/j.msea.2017.01.072 ↗
10. The effects of heat treatment and carbon content on the microstructure and mechanical properties of laser powder bed fusion Ti-6Al-4V with dissolved TiC particles10.1016/j.jallcom.2022.165930 ↗
11. Tensile properties improvement by homogenized nitrogen solid solution strengthening of commercially pure titanium through powder metallurgy process10.1016/j.matchar.2020.110700 ↗
12. First-principles study and its experimental verification on the strength and ductility of O/Si solid solution strengthened Ti alloys10.1016/j.jmrt.2023.11.221 ↗
13. Dual-phase nanostructure of amorphous carbon and TaCB solid solution: robust high-performance protective coating for marine equipment10.1016/j.ceramint.2023.04.143 ↗
14. Effects of carbon nanomaterials on interfacial structure and mechanical properties of high temperature Ti matrix composites10.1016/j.jallcom.2023.172360 ↗
15. Strengthening and deformation mechanism of selective laser-melted high-concentration nitrogen solute α-Ti materials with heterogeneous microstructures via heat treatment10.1016/j.msea.2021.141935 ↗
16. The effect of interstitial carbon on the mechanical properties and dislocation substructure evolution in Fe40.4Ni11.3Mn34.8Al7.5Cr6 high entropy alloys10.1016/j.actamat.2016.08.072 ↗
17. Novel insights on the near atomic scale spatial distributions of substitutional alloying and interstitial impurity elements in Ti-6Al-4V alloy10.1016/j.jallcom.2022.164511 ↗
18. Influence of simple metals on the stability of basal screw dislocations in hexagonal titanium alloys10.1016/j.actamat.2019.08.039 ↗
19. Interstitial carbon induced FCC-Ti exhibiting ultrahigh strength in a Ti37Nb28Mo28-C7 complex concentrated alloy10.1016/j.actamat.2020.10.075 ↗
20. Enhanced strength and ductility in a high-entropy alloy via ordered oxygen complexes10.1038/s41586-018-0685-y ↗
21. In-situ high-temperature EBSD characterization during a solution heat treatment of hot-rolled Ti-6Al-4V10.1016/j.matchar.2022.112207 ↗
22. Evolution of the α phase and microhardness for hot isostatic pressed Ti-6Al-4V alloy during multi-pass deformation10.1016/j.matchar.2021.111263 ↗
23. Microstructure evolution and corrosion mechanism of in situ synthesized TiC/TC4 alloy nanocomposites fabricated by laser powder bed fusion10.1016/j.ceramint.2022.09.257 ↗
24. Mechanisms of tensile strengthening and oxygen solid solution in single β-phase Ti-35 at.%ta+O alloys10.1016/j.msea.2020.140677 ↗
25. Microstructure evolution and mechanical properties of graphene reinforced Ti-6Al-4V matrix composites: defective vs high-quality graphene10.1016/j.jallcom.2023.172346 ↗
26. Effects of mixing methods on the interface and microstructure evolution of graphene platelets/Ti-6Al-4V powder composites fabricated by powder metallurgy and extrusion10.1016/j.surfin.2022.102553 ↗
27. Microstructure and mechanical properties of GNPs and in-situ TiB hybrid reinforced Ti–6Al–4V matrix composites with 3D network architecture10.1016/j.msea.2022.143536 ↗
28. Microstructure and mechanical properties of in-situ Ti5Si3/TC4 composites via spark plasma sintering and hot rolling10.1016/j.jallcom.2023.172404 ↗
29. Effect of ball milling time on microstructure and mechanical properties of graphene nanoplates and TiBw reinforced Ti–6Al–4V alloy composites10.1016/j.msea.2022.144240 ↗
30. Evolution mechanism of grain orientation and texture distribution of Ti-6.5Al-3.5Mo-1.5Zr-0.3Si alloy under electroshocking treatment10.1016/j.jmrt.2023.07.028 ↗
31. Molecular dynamics simulations of TC4 titanium alloy with mechanical property calculations after various heat treatments10.1039/D2CP03739D ↗
32. Quasi-continuous GNS network induced local dynamic recrystallization along interfaces in titanium MMCs under high strain rate loading10.1016/j.msea.2022.143723 ↗
33. Uniformly dispersing GNPs for fabricating graphene-reinforced pure Ti matrix composites with enhanced strength and ductility10.1016/j.jallcom.2021.161527 ↗
34. Achieving high strength and ductility in graphene/magnesium composite via an in-situ reaction wetting process10.1016/j.carbon.2018.08.009 ↗
35. Enhanced adiabatic shear band susceptibility in Ti composites reinforced with quasi-continuous network of graphene nanosheets10.1016/j.compositesa.2022.107055 ↗
36. Interface structure and strengthening behavior of graphene/CuCr composites10.1016/j.carbon.2018.03.018 ↗
37. A modified Hall–Petch relationship in ultrafine-grained titanium recycled from chips by equal channel angular pressing10.1016/j.scriptamat.2012.02.008 ↗
38. The effects of carbon, oxygen and nitrogen on the mechanical properties of titanium and titanium alloys
39. Investigation on the microstructure, room and high temperature mechanical behaviors and strengthening mechanisms of the (TiB+TiC)/TC4 composites10.1016/j.jallcom.2017.08.017 ↗
40. Microstructure, mechanical properties and strengthening mechanisms of in-situ prepared (Ti5Si3 + TiC0.67)/TC4 composites10.1016/j.jallcom.2019.04.056 ↗
41. CNTs/cu-Ti composites fabrication through the synergistic reinforcement of CNTs and in situ generated nano-TiC particles10.1016/j.jallcom.2018.08.116 ↗
42. Strengthening and plasticity improvement mechanisms of titanium matrix composites with two-scale network microstructure10.1016/j.powtec.2019.09.008 ↗
43. Strengthening effects of in-situ synthetic nano-TiC particles on Ti64 based nanocomposites through adding graphene nanoplatelets10.1016/j.vacuum.2020.109431 ↗
44. Microstructure characterization of a high strength Ti–6Al–4V alloy prepared from a powder mixture of TiH2 and 60Al40V masteralloy powders10.1016/j.jallcom.2019.152815 ↗
45. Dislocation generation due to differences between the coefficients of thermal expansion10.1016/0025-5416(86)90261-2 ↗
46. Influence of oxygen content on microstructure and mechanical properties of Ti–Nb–ta–Zr alloy10.1016/j.matdes.2010.11.049 ↗
47. Massive interstitial solid solution alloys achieve near-theoretical strength10.1038/s41467-022-28706-w ↗