Effect of 800 °C/10,000 h aging-induced μ phase on plasticity in Ni-Co-Cr based superalloys
Source abstract
Abstract
Since the concentration of refractory elements, such as W and Mo, increases in superalloys , the brittle μ phases, specifically (Co, Cr) 7 (W, Mo) 6 , tend to precipitate readily. These μ phases frequently serve as crack initiation sites, leading to a significant reduction in the lifetime of alloys. The present study focuses on the effect of μ phases on room-temperature tensile plasticity of a Ni-Co-Cr-based superalloy containing 4.0 wt% W and 4.0 wt% Mo during long-term aging. The objective is to analyze the precipitation behavior of μ phases and their influence on the elongation. With the precipitation of μ phases, W and Mo diffuse from the γ matrix into the μ phase, and meanwhile, the size and area fraction of μ phases initially increase before stabilizing. Notably, at an aging temperature of 800 °C, Mo exhibits a stronger diffusion ability compared to W. The depletion of solute atoms in the γ matrix, results the weakening of solid solution strength . Therefore, during tensile tests , more intergranular cracks propagate along the γ matrix interface near μ phases and γ' precipitates. Regarding the fracture characteristics , as the size and area fraction of μ phase increase, a greater number of dislocations pile-up near grain boundaries, leading to the formation of numerous creaks through shearing and bypassing. Moreover, the elongation significantly decreases from 17 to 19 % to 8–12 % after aging for more than 1000 h. This work enhances our understanding of μ precipitation and its effect on the material's plasticity.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: High Temperature Alloys and Creep · Advanced Materials Characterization Techniques · Metallurgical and Alloy Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Effects of solidification rate and heat treatment on microstructure characterization and hot tensile strength of single crystal CMSX-4 superalloy10.1016/j.matchar.2022.112449 ↗
2. Effect of μ precipitation and γ’ evolution on intra−/intergranular strength of Ni-Co-Cr-based superalloys after 800 °C thermal exposure10.1016/j.jallcom.2024.175073 ↗
3. A novel strategy for ingot cogging without homogenization: Dynamical recrystallization and nucleation mechanisms associated with as-cast dendrites of nickel-based superalloys10.1016/j.jmst.2024.08.061 ↗
4. Influence of scandium addition on microstructure and mechanical properties in nickel-based superalloys: an integrated multiscale modeling and experimental approach10.1016/j.ijplas.2023.103703 ↗
5. High-temperature tensile properties and strengthening mechanism of cryo-rolled MP159 superalloy strengthened by deformation nano-twins10.1016/j.matchar.2024.113692 ↗
6. Evolutionary mechanisms in the plastic deformation of γ'-Ni3(Al, Ti)-strengthened additively manufactured nickel-based 939 superalloys at intermediate temperatures10.1016/j.matdes.2024.112795 ↗
7. PPB structure elimination, DRX nucleation mechanisms and grain growth behavior of the 3rd-generation PM superalloy for manufacturing aviation components10.1016/j.cja.2023.10.016 ↗
8. Microstructure and mechanical behaviour of an advanced powder metallurgy nickel base superalloy processed through hot isostatic pressing route for aerospace applications10.1016/j.msea.2020.140254 ↗
9. A review on cracking mechanism and suppression strategy of nickel-based superalloys during laser cladding10.1016/j.jallcom.2024.175164 ↗
10. Microstructural evolution and coarsening in Ni-Al-Cr-Co model superalloys with nano γ’-precipitates: an experimental and thermodynamic investigation
11. Effect of cobalt on γ’ coarsening behavior of Ni-base powder metallurgy superalloy10.1016/j.jallcom.2022.166057 ↗
12. Morphological development, coarsening, and oxidation behavior of Ni-Al-Nb Superalloys10.1007/s11665-020-04926-3 ↗
13. Temporal evolution, coarsening behavior and oxidation resistance of Ni–15Al superalloy10.1016/j.jallcom.2019.151784 ↗
14. Role of alloy composition on micro-cracking mechanisms in additively manufactured Ni-based superalloys10.1016/j.actamat.2023.119089 ↗
15. Interface microstructural evolution, microhardness variation mechanism and 750 °C tensile behavior of the HIPed/FGed PM superalloy plastic bonded joints10.1016/j.jmrt.2024.05.259 ↗
16. Understanding the fracture mechanisms of Ni-Co-Cr-type superalloys: Role of precipitate evolution and strength degradation10.1016/j.msea.2024.146623 ↗
17. Effects of cerium addition on the microstructure and stress rupture properties of a new nickel-based cast superalloy10.1016/j.jmst.2023.01.060 ↗
18. High-temperature structural stabilities of Ni-based single-crystal superalloys Ni-Co-Cr-Mo-W-Al-Ti-Ta with varying Co contents10.1007/s40195-017-0678-0 ↗
19. Structural properties and cyclic oxidation behavior of Ni-Al-Y superalloys
20. Development of a low-density Co-Ni-Al-Ta-Cr superalloy with high mechanical performance and superior oxidation resistance10.1016/j.matdes.2024.112673 ↗
21. The improved physically-mechanism constitutive model for a Ni-Mo-Cr-based superalloy with the pre-precipitation of μ phase in hot forming10.1016/j.jallcom.2024.174934 ↗
22. Atomic configurations of planar defects in μ phase in Ni-based superalloys10.1016/j.scriptamat.2020.09.045 ↗
23. Nucleation and transition sequences of TCP phases during heat-exposure in a re-containing Ni-based single crystal superalloy10.1016/j.jmst.2024.02.081 ↗
24. In site TEM investigation on the precipitation behavior of μ phase in Ni-base single crystal superalloys10.1016/j.actamat.2016.03.046 ↗
25. The precipitation and effect of topologically close-packed phases in Ni-based single crystal superalloys10.1016/j.jmst.2023.05.074 ↗
26. Precipitation behavior of μ phase and creep rupture in single crystal superalloy CMSX-410.1016/j.jallcom.2011.04.001 ↗
27. The effects of tensile stress on the microsturcture evolution and elemental interdiffusion behavior of (Ni, Pt)Al coating and nickel-based superalloy at 1100 °C for 200 h10.1016/j.jallcom.2023.169422 ↗
28. Nanoindentation studies of the mechanical properties of the μ phase in a creep deformed Re containing nickel-based superalloy10.1016/j.msea.2015.03.045 ↗
29. Effect of solid solution elements on cracking susceptibility of Ni-based superalloys during additive manufacturing10.1016/j.jmst.2023.11.073 ↗
30. Precipitation behavior and mechanical property evolution in a solid solution strengthened Ni-Cr-W superalloy during short-term aging10.1016/j.jallcom.2024.173678 ↗
31. The element occupation preference of μ phase in ternary Ni-Cr-Mo model superalloy10.1016/j.matdes.2022.111569 ↗
32. Interface of chemistry and deformation-induced defects on facilitating topologically-close-packed phase precipitation in nickel-base superalloys10.1016/j.actamat.2022.118109 ↗
33. Investigation of microstructural stability and tensile deformation behavior of a novel PM Ni-based superalloy during long-term thermal exposure10.1016/j.msea.2024.146457 ↗
34. Correlations between microstucture evolution and mechanical behavior of a nickel-based single crystal superalloy with long-term aging effects10.1016/j.matchar.2020.110652 ↗
35. Microstructure-sensitive creep models for nickel-base superalloy single crystals10.1016/j.msea.2013.04.072 ↗
36. Interdiffusion in the face-centred cubic phase of the Ni-Re, Ni-Ta and Ni-W systems between 900 and 1300 °C10.1016/S0921-5093(99)00705-4 ↗
37. Interdiffusion of the platinum-group metals in nickel at elevated temperatures10.1016/S1359-6454(03)00105-8 ↗
38. Interdiffusion and its size effect in nickel solid solution of Ni-Co, Ni-Cr and Ni-Ti systems10.1007/BF00729354 ↗
39. Effect of aging temperature on the secondary γ’ precipitation in a model Ni based single crystal superalloy10.1016/j.jallcom.2020.155486 ↗
40. Microstructural evolution and stress rupture behaviour of a Ni-based wrought superalloy during thermal exposure10.1016/j.msea.2021.141659 ↗
41. Alloys by design: modelling next generation superalloys10.1179/174328408X372056 ↗
42. First-principles theoretical and experimental studies of effects of ruthenium on precipitation behavior of μ phase and μ/matrix interface stability in Ni-based single crystal superalloys10.1016/j.intermet.2019.106556 ↗