Al-Ce alloys are promising for high-temperature applications due to their thermally stable Al₁₁Ce₃ eutectic phase, yet their strength-ductility trade-off remains a critical challenge. This study introduces Zr to Al-5wt.%Ce hypoeutectic alloys to address this limitation. Combining thermodynamic calculations , microstructure characterization , and in-situ synchrotron X-ray imaging and diffraction, we elucidate the mechanisms of Zr-induced grain refinement and strengthening. Increasing Zr content promotes the formation of primary Al₃Zr phases, which act as heterogeneous nucleation sites , refining the average grain size from 576 ± 182 μm (Zr-free) to 452 ± 148 μm (0.5 wt% Zr). The Al-5Ce-0.5Zr alloy achieves optimized mechanical properties, with ultimate tensile strength increasing from 126 MPa to 137 MPa and elongation improving from 32 % to 37 %. In-situ experiments reveal that load transfer to the Al₁₁Ce₃ phase and enhanced strain hardening in both α-Al and Al₁₁Ce₃ contribute synergistically to strength and ductility. A quantitative model confirms that stress partitioning to Al₁₁Ce₃ rises from 170 MPa to 210 MPa with Zr addition. These findings provide critical insights for designing high-performance Al-Ce alloys via grain refinement and eutectic phase strengthening, advancing their potential in casting and additive manufacturing .
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Microstructure and mechanical properties · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Design and development of an experimental wrought aluminum alloy for use at elevated temperatures10.1007/BF02628387 ↗
2. A novel heat-resistant Al–Si–Cu–Ni–Mg base material synergistically strengthened by Ni-rich intermetallics and nano-AlNp microskeletons10.1016/j.jmst.2018.09.051 ↗
3. Simulation of the concomitant process of nucleation-growth-coarsening of Al 2 Cu particles in a 319 foundry aluminum alloy10.1088/0965-0393/23/4/045012 ↗
4. Microstructural evolution and strengthening mechanisms of additively-manufactured Al-Mg-Sc-Zr alloys: laser directed energy deposition versus laser powder bed fusion10.1016/j.jallcom.2024.173946 ↗
5. Research on microstructure and mechanical properties at elevated temperature of Al-Mg-Si-Sc-Zr alloy strengthened by Al3(Sc, Zr) nanoprecipitates10.1016/j.jallcom.2024.174050 ↗
6. High performance aluminum–cerium alloys for high-temperature applications10.1039/C7MH00391A ↗
7. Thermal stability of aluminum–cerium binary alloys containing the Al–Al11Ce3 eutectic10.1016/j.msea.2021.140973 ↗
8. Microstructure and properties of a high temperature Al–Ce–Mn alloy produced by additive manufacturing10.1016/j.actamat.2020.07.014 ↗
9. Microstructure and creep properties of cast near-eutectic Al–Ce–Ni alloys10.1016/j.msea.2021.142551 ↗
10. Microstructure and strengthening of Al-6Ce-3Ni-0.7Fe (wt%) alloy manufactured by laser powder-bed fusion
11. Additively manufactured Al-Ce-Ni-Mn alloy with improved elevated-temperature fatigue resistance
12. Phase stability in cast and additively manufactured Al-rich Al-Cu-Ce alloys10.1016/j.jallcom.2022.166984 ↗
13. Strength mechanisms and tunability in Al-Ce-Mg ternary alloys enabled by additive manufacturing10.1016/j.matdes.2023.112009 ↗
14. Aging and wear characteristics of A356 alloy with Er and Zr addition[J]10.1080/02670836.2023.2196474 ↗
15. Microstructure and impression creep behavior of Al–7Si–0.3 Mg alloy with Zr addition[J]10.1007/s12540-020-00628-6 ↗
16. Tensile and creep properties of Al–7Si–0.3 Mg alloy with Zr and Er addition[J]10.1080/02670836.2020.1809144 ↗
17. Chankitmunkong · 2024
18. On the origin of a remarkable increase in the strength and stability of an Al rich Al-Ni eutectic alloy by Zr addition10.1016/j.actamat.2019.03.025 ↗
19. Combining solution-, precipitation- and load-transfer strengthening in a cast Al-Ce-Mn-Sc-Zr alloy10.1016/j.actamat.2024.119683 ↗
20. Enhancing ambient and elevated temperature performance of hypoeutectic Al–Ce cast alloys by Al3(Sc,Zr) precipitate10.1016/j.jmrt.2023.12.021 ↗
21. A criterion for cracking during solidification10.1016/j.actamat.2015.01.034 ↗
22. Grain refinement in aluminum-zirconium and aluminum-titanium alloys by metastable phases
23. Metastable phase and grain refinement in rapidly solidified Al-Zr alloys10.2464/jilm.27.129 ↗
24. Deformation mechanism of a strong and ductile maraging steel investigated using in-situ X-ray synchrotron diffraction10.1016/j.ijplas.2023.103612 ↗
25. Reveling the orientation preference along with localized Lüders-type deformation in polycrystalline NiTi SMA by in-situ synchrotron-based high energy X-ray diffraction10.1016/j.vacuum.2023.112921 ↗
26. Microstructural origins of high strength of Al–Si alloy manufactured by laser powder bed fusion: in-situ synchrotron radiation X-ray diffraction approach10.1016/j.jmst.2023.08.050 ↗
27. Evolution of microstructure and deformation mechanisms in a metastable Fe42Mn28Co10Cr15Si5 high entropy alloy: a combined in-situ synchrotron X-ray diffraction and EBSD analysis
28. Outstanding thermal stability of cold-rolled Al–Y alloy revealed using in-situ synchrotron X-ray diffraction and ex-situ microscopy10.1016/j.jmrt.2023.12.195 ↗
29. Processing of an as-cast Al-7.5 wt%Y eutectic alloy by rolling and annealing to improve the tradeoff between strength and electrical conductivity10.1016/j.msea.2023.145950 ↗
30. Mechanical properties and electrical conductivity of cold rolled Al-7.5 wt% Y alloy with heterogeneous lamella structure and stacking faults[J]10.1016/j.jallcom.2021.160692 ↗
31. GSAS-II: the genesis of a modern open-source all purpose crystallography software package10.1107/S0021889813003531 ↗