Microstructural evolution and high-temperature oxidation resistance of YSZ/Crofer 22H brazed joints using Ag-based filler for solid-oxide fuel cell applications

Z.W. Yang, Z. Xiong, J.L. Wang, Y. Wang, D.P. Wang

Publisher page

Abstract

The YSZ/Crofer 22H vacuum brazed joints using a newly developed Ag-6.2Cu-1.6Al-2.1Ti (wt%) alloy, were systematically characterized from the aspects of the interfacial microstructure and mechanical properties with the variation in operating parameters. Resultantly, the representative interfacial microstructure of the YSZ ceramic/Crofer 22H stainless steel brazed joints at 960 °C/10 min was YSZ/TiO + Ti 3(Cu, Al) 3O/block Cu 3Al + Ag(s, s) + needle-shaped Cu(s, s)/Ti(Al, Cu) 2 + β-Ti + Fe 2Ti + Fe-Cr/Crofer 22H. The operating parameters were found to have a prominent impact on the microstructure, which is mainly reflected in the progress of transformation between TiO and Ti 3(Cu, Al) 3 O, the aggregation of β-Ti, and the thickness of the Ag-based brazing seam. The mountain peak of shear strength attained 178 MPa, and the shear failure first occurred from the YSZ ceramic substrate close to the brazing seam to the metallic reaction layers neighboring the Crofer 22H with increasing the operating parameters. Furthermore, the high-temperature oxidation resistance of the YSZ/Crofer 22H brazed joints was evaluated at 800 °C in the air over 200 h. Even though an increase in the O content of the interfacial products could be detected, the joint still kept structural integrity and remained at 50 MPa, and 32 MPa in the shear test for oxidation times of 50 h and 100 h separately. Ag-riched Delimination was found neighboring Crofer 22H due to a large difference in affinity between different elements (Ag, Cr, Al, Ti, Cu, and Fe) and O, and constantly kept the metallurgical bonding between Corfer 22H and brazing seam even the reaction layer continually diffused toward brazing seam for oxidation, indicating an excellent high-temperature oxidation resistance of this vacuum brazed joint.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Advanced ceramic materials synthesis · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (45)

Show source-provided references
1. Non-crystallising glass sealants for SOFC: Effect of Y2O3 addition10.1016/j.ceramint.2019.10.266 ↗
2. Study of sealants for SOFC10.1016/j.ijhydene.2016.07.156 ↗
3. Interfacial characterization and mechanical properties of reactive air brazed ZrO2 ceramic joints with Ag-CuO-Al2TiO5 composite filler metal10.1016/j.ceramint.2021.07.076 ↗
4. Novel glass-ceramic SOFC sealants from glass powders and a reactive silicone binder10.1016/j.jeurceramsoc.2018.05.024 ↗
5. Characteristics of a SiO2-B2O3-Al2O3-BaCO3-PbO2-ZnO glass-ceramic sealant for SOFCs10.1016/j.jallcom.2006.05.105 ↗
6. Aluminosilicate-based sealants for SOFCs and other electrochemical applications - A brief review10.1016/j.jpowsour.2013.05.099 ↗
7. Oxygen vacancy stabilized zirconia (OVSZ); a joint experimental and theoretical study10.1016/j.scriptamat.2016.06.025 ↗
8. Oxygen-ion conductivity and mechanical properties of Lu2O3-doped ZrO2 as a solid electrolyte10.1016/j.ceramint.2021.03.158 ↗
9. Three-dimensional and time-dependent simulation of a planar solid oxide fuel cell stack[J]10.1016/0378-7753(93)01833-4 ↗
10. Braze oxidation behavior and joint microstructure in YSZ/steel joints made using palladium brazes for SOFC applications10.1016/j.msea.2007.08.032 ↗
11. Effect of short-term aging on interfacial and mechanical properties of yttria stabilized zirconia (YSZ)/stainless steel joints10.1016/j.jeurceramsoc.2014.10.001 ↗
12. Interfacial and mechanical characterization of yttria-stabilized zirconia (YSZ) to stainless steel joints fabricated using Ag-Cu-Ti interlayers10.1016/j.ceramint.2013.07.119 ↗
13. Interfacial microstructure and mechanical properties of zirconia ceramic and niobium joints vacuum brazed with two Ag-based active filler metals10.1016/j.ceramint.2016.05.045 ↗
14. Experimental and theoretical study on air reaction wetting and brazing of Si3N4 ceramic by Ag-CuO filler metal: performance and interfacial behavior10.1016/j.jeurceramsoc.2021.10.039 ↗
15. Diffusion bonding of (Hf(0.2)Zr(0.2)Ti(0.2)Ta(0.2)Nb0.2)C high-entropy ceramic with metallic Ni foil10.1016/j.jeurceramsoc.2021.08.048 ↗
16. Wettability of Ti3SiC2 by Ag-Cu and Ag-Cu-Ti melts10.1007/s10853-009-3941-6 ↗
17. Microstructure and mechanical properties of 17-4 PH stainless steel and Al2O3 ceramic joints brazed with graphene reinforced Ag-Cu-Ti brazing alloy10.1016/j.vacuum.2020.109604 ↗
18. Mechanism of interfacial reaction between Ti and Al-ceramic10.1016/j.matdes.2016.05.073 ↗
19. Interfacial reactions and matrix microstructure evolution in SiCf/Ti composites dominated by primary structure of Ti matrix10.1016/j.ceramint.2019.05.347 ↗
20. Microstructure evolution and mechanical properties of ZrO2/ ZrO2 joints brazed with Ni-Ti filler metal10.1088/2053-1591/ab574b ↗
21. Brazing ZrO2 ceramic to Ti-6Al-4V alloy using NiCrSiB amorphous filler foil: Interfacial microstructure and joint properties10.1016/j.matchar.2013.04.009 ↗
22. Effects of fabrication parameters on Interface of zirconia and Ti-6Al-4V joints using Zr55Cu30Al10Ni5 amorphous filler10.1007/s11665-013-0534-y ↗
23. Zirconia ceramic and Nb joints brazed with Mo-particle-reinforced Ag-Cu-Ti composite fillers: Interfacial microstructure and formation mechanism10.1016/j.ceramint.2017.04.133 ↗
24. Microstructural evolution and characterisation of interfacial phases in Al2O3/Ag-Cu-Ti/Al2O3 braze joints10.1016/j.actamat.2015.05.048 ↗
25. Microstructural evolution and bonding mechanisms of the brazed Ti/ ZrO2 joint using an Ag68.8Cu26.7Ti4.5 interlayer at 900 °C10.1557/jmr.2014.30 ↗
26. Interfacial characterization of alumina-to-alumina joints fabricated using silver-copper-titanium interlayers10.1016/j.matchar.2014.01.009 ↗
27. Characterization of yttria-stabilized-zirconiaistainless steel joint interfaces with gold-based interlayers for solid oxide fuel cell applications10.1016/j.jeurceramsoc.2013.08.036 ↗
28. Microstructure and mechanical properties of Ti6Al4V alloy and sapphire joint brazed with graphene-AgCuTi
29. Joining of Zirconia and Ti-6A1-4V Using a Ti-based Amorphous Filler
30. Microstructural characterization of interfacial reaction products between alumina and braze alloy10.1007/BF00351596 ↗
31. Interface evolution of SiO2 glass ceramic and Ti-6Al-4V alloy joint brazed with Ag-Cu-Ti alloy10.1179/026708309X12506933873026 ↗
32. Interfacial microstructure and mechanical properties of ZTA/ZTA joints brazed with Ni-Ti filler metal10.1016/j.jeurceramsoc.2020.10.073 ↗
33. Brazing TC4 titanium alloy/316L stainless steel joint with Ti50-xZrxCu39Ni11 amorphous filler metals10.1016/j.jallcom.2020.156650 ↗
34. Interfacial microstructure and shear strength of Ti6Al4V alloy/316 L stainless steel joint brazed with Ti33.3Zr16.7Cu50-xNix amorphous filler metals10.1016/j.matdes.2019.108380 ↗
35. Brazing of porous Si3N4 ceramic to Invar alloy with a novel Cu-Ti filler alloy: Microstructure and mechanical properties10.1016/j.ceramint.2020.09.039 ↗
36. Reaction-composite diffusion brazing of C-SiC composite and Ni-based superalloy using mixed (Cu-Ti) plus C powder as an interlayer10.1016/j.jmatprotec.2021.117419 ↗
37. Brazing of yttria-stabilized zirconia (YSZ) to stainless steel using Cu, Ag, and Ti-based brazes10.1007/s10853-007-1985-z ↗
38. Microstructure evolution and mechanical properties of Co coated AISI 441 ferritic stainless steel/YSZ reactive air brazed joint10.1016/j.ijhydene.2020.12.059 ↗
39. Microstructural evolution during reactive brazing of alumina to Inconel 600 using Ag-based alloy10.1016/j.actamat.2012.09.040 ↗
40. Microstructural stability and mechanical properties of Al2O3/Kovar 4 J34 joint vacuum brazed using Ag-5Cu-1Al-1.25Ti (wt %) filler metal10.1016/j.jmapro.2021.10.057 ↗
41. Application of a simple subregular solution model to the computation of phase boundaries and free dendritic growth in the Ag-Cu system10.1016/j.actamat.2016.04.049 ↗
42. Microstructural evolution and thermal stress relaxation of Al2O3/1Cr18Ni9Ti brazed joints with nickel foam10.1016/j.vacuum.2017.10.030 ↗
43. The thermodynamic reassessment of the binary Al-Cu system10.1007/s10853-020-05423-7 ↗
44. Interfacial reactions between sapphire and Ag-Cu-Ti-based active braze alloy10.1016/j.actamat.2015.11.019 ↗
45. An Ag based brazing system with a tunable thermal expansion for the use as sealant for solid oxide cells10.1016/j.jpowsour.2016.03.030 ↗