The study of Ni-Sn transient liquid phase bonded joints under high temperatures
Source abstract
Abstract
To develop new electronic packaging techniques for harsh environments, the microstructure and associated mechanical properties of Ni-Sn transient liquid phase (TLP) bonded joints at high temperatures have been investigated in this work. The effect of bonding temperature (from 400 °C to 700 °C) on the microstructure and mechanical properties of joints has been studied. In addition, the growth kinetics of Ni3Sn2 and Ni3Sn intermetallic compounds (IMCs) have been studied to analyse the phase transformation mechanisms and microstructure evolution of joints bonded at 500 °C for different times. Also, the long-term (up to 100 h) high-temperature (500 °C) thermal reliability of the joints has been investigated. The results showed that the average shear strength increased as the bonding temperature increased from 400 °C to 500 °C, but continuously dropped as the bonding temperature further increased from 500 °C to 700 °C. It was found that volume diffusion dominated the growth mechanisms of both Ni3Sn2 and Ni3Sn IMCs during bonding at 500 °C for different times. Furthermore, as the aging (at 500 °C) time increased from 0 h to 100 h, the average shear strength of joints continuously decreased. The joints aged for 50 h shear fractured mainly within the Ni3Sn2 IMCs, while the joints after aging for 100 h fractured mainly through the Ni3Sn IMCs.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Advanced Welding Techniques Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. Microstructure and mechanical properties of electroplated Ni-Sn TLP bonded joints with different bonding and aging times10.1016/j.matchar.2022.112452 ↗
2. Transient liquid phase Ag-based solder technology for high-temperature packaging applications10.1016/j.jallcom.2013.10.204 ↗
3. Ag@Sn core-shell powder preform with a high re-melting temperature for high-temperature power devices packaging10.1002/adem.201700524 ↗
4. Transient liquid phase bonding (TLPB) of Cu to Cu using Sn interconnect solder reinforced by submicron Al particles10.1016/j.jmatprotec.2022.117686 ↗
5. Microstructure evolution and grain orientation of IMC in Cu-Sn TLP bonding solder joints10.1016/j.jallcom.2019.01.384 ↗
6. Microstructural evolution and performance of high-tin-content Cu40Sn60 (wt.%) core/shell powder TLPS bonding joints10.1016/j.jmapro.2022.01.045 ↗
7. Ag-Sn transient liquid phase bonding for high temperature electronic packaging: effect of Ag content10.1109/TCPMT.2020.3009515 ↗
8. Microstructure characterization and mechanical behavior for Ag3Sn joint produced by foil-based TLP bonding in air atmosphere10.1016/j.msea.2016.10.092 ↗
9. A comparative study on the microstructure and mechanical properties of Cu6Sn5 and Cu3Sn joints formed by TLP soldering with/without the assistance of ultrasonic waves10.1007/s11661-018-4664-6 ↗
10. Reliability modeling of Sn-Ag transient liquid phase die-bonds for high-power SiC devices10.1016/j.microrel.2016.02.016 ↗
11. Ni3Sn4-composed die bonded interface rapidly formed by ultrasonic-assisted soldering of Sn/Ni solder paste for high-temperature power device packaging
12. Suppression effect of Ni grain size on the Ni3Sn4 growth at the Sn/Ni interface10.1016/j.matchar.2017.04.013 ↗
13. Microstructural evolution of Ni-Sn transient liquid phase sintering bond during high-temperature aging10.1007/s11664-018-6336-0 ↗
14. Elimination of voids in reactions between Ni and Sn: a novel effect of silver10.1016/j.scriptamat.2011.10.032 ↗
15. An interconnection method based on Sn-coated Ni core-shell powder preforms for high-temperature applications10.1016/j.jallcom.2018.10.267 ↗
16. 2023
17. Intermediate temperature embrittlement of one new Ni-26W-6Cr based superalloy for molten salt reactors10.1016/j.msea.2016.04.032 ↗
18. Interface reaction between electroless Ni-Sn-P metallization and lead-free Sn-3.5Ag solder with suppressed Ni3P formation10.1007/s11664-014-3306-z ↗
19. Structure refinement of Ni3Sn410.1107/S056774088200346X ↗